Title: Conductivity and touch-sensor application for atomic layer deposition ZnO and Al:ZnO on nylon nonwoven fiber mats

Abstract

Flexible electronics and wearable technology represent a novel and growing market for next generation devices. In this work, the authors deposit conductive zinc oxide films by atomic layer deposition onto nylon-6 nonwoven fiber mats and spun-cast films, and quantify the impact that deposition temperature, coating thickness, and aluminum doping have on the conductivity of the coated substrates. The authors produce aluminum doped zinc oxide (AZO) coated fibers with conductivity of 230 S/cm, which is ∼6× more conductive than ZnO coated fibers. Furthermore, the authors demonstrate AZO coated fibers maintain 62% of their conductivity after being bent around a 3 mm radius cylinder. As an example application, the authors fabricate an “all-fiber” pressure sensor using AZO coated nylon-6 electrodes. The sensor signal scales exponentially under small applied force (<50 g/cm{sup 2}), yielding a ∼10{sup 6}× current change under 200 g/cm{sup 2}. This lightweight, flexible, and breathable touch/force sensor could function, for example, as an electronically active nonwoven for personal or engineered system analysis and diagnostics.

Authors:
; ;  [1]
  1. Department of Chemical and Biomolecular Engineering, North Carolina State University, Raleigh, North Carolina 27695 (United States)
Publication Date:
OSTI Identifier:
22392092
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films; Journal Volume: 33; Journal Issue: 1; Other Information: (c) 2014 American Vacuum Society; Country of input: International Atomic Energy Agency (IAEA)
Country of Publication:
United States
Language:
English
Subject:
42 ENGINEERING; ALUMINIUM; CURRENTS; DEPOSITION; DOPED MATERIALS; FIBERS; FILMS; NYLON; SENSORS; SYSTEMS ANALYSIS; THICKNESS; ZINC OXIDES

Citation Formats

Sweet, William J., Oldham, Christopher J., and Parsons, Gregory N., E-mail: parsons@ncsu.edu. Conductivity and touch-sensor application for atomic layer deposition ZnO and Al:ZnO on nylon nonwoven fiber mats. United States: N. p., 2015. Web. doi:10.1116/1.4900718.
Sweet, William J., Oldham, Christopher J., & Parsons, Gregory N., E-mail: parsons@ncsu.edu. Conductivity and touch-sensor application for atomic layer deposition ZnO and Al:ZnO on nylon nonwoven fiber mats. United States. doi:10.1116/1.4900718.
Sweet, William J., Oldham, Christopher J., and Parsons, Gregory N., E-mail: parsons@ncsu.edu. Thu . "Conductivity and touch-sensor application for atomic layer deposition ZnO and Al:ZnO on nylon nonwoven fiber mats". United States. doi:10.1116/1.4900718.
@article{osti_22392092,
title = {Conductivity and touch-sensor application for atomic layer deposition ZnO and Al:ZnO on nylon nonwoven fiber mats},
author = {Sweet, William J. and Oldham, Christopher J. and Parsons, Gregory N., E-mail: parsons@ncsu.edu},
abstractNote = {Flexible electronics and wearable technology represent a novel and growing market for next generation devices. In this work, the authors deposit conductive zinc oxide films by atomic layer deposition onto nylon-6 nonwoven fiber mats and spun-cast films, and quantify the impact that deposition temperature, coating thickness, and aluminum doping have on the conductivity of the coated substrates. The authors produce aluminum doped zinc oxide (AZO) coated fibers with conductivity of 230 S/cm, which is ∼6× more conductive than ZnO coated fibers. Furthermore, the authors demonstrate AZO coated fibers maintain 62% of their conductivity after being bent around a 3 mm radius cylinder. As an example application, the authors fabricate an “all-fiber” pressure sensor using AZO coated nylon-6 electrodes. The sensor signal scales exponentially under small applied force (<50 g/cm{sup 2}), yielding a ∼10{sup 6}× current change under 200 g/cm{sup 2}. This lightweight, flexible, and breathable touch/force sensor could function, for example, as an electronically active nonwoven for personal or engineered system analysis and diagnostics.},
doi = {10.1116/1.4900718},
journal = {Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films},
number = 1,
volume = 33,
place = {United States},
year = {Thu Jan 15 00:00:00 EST 2015},
month = {Thu Jan 15 00:00:00 EST 2015}
}