Title: Local strain around hydrogen in amorphous Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50}

Abstract

The hydrogen-induced volume expansion, a change in the X-ray diffraction first peak due to hydrogen charging and the hydrogen Gorsky effects were measured for amorphous (a-) Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50} and discussed together with the hydrogen Snoek peak reported. In contrast, anisotropy of the elastic distortion around hydrogen appears to be much larger in a-Cu{sub 50}Zr{sub 50} than in a-Cu{sub 50}Ti{sub 50}. It is surmised that the local atomic structures are more deformable in a-Cu{sub 50}Zr{sub 50} than in a-Cu{sub 50}Ti{sub 50}.

Authors:
; ;
Publication Date:
Research Org.:
Univ. of Tsukuba, Ibaraki (JP)
OSTI Identifier:
20000476
Resource Type:
Journal Article
Journal Name:
Acta Materialia
Additional Journal Information:
Journal Volume: 47; Journal Issue: 12; Other Information: PBD: 29 Sep 1999; Journal ID: ISSN 1359-6454
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; INTERNAL FRICTION; COPPER ALLOYS; ZIRCONIUM ALLOYS; TITANIUM ALLOYS; METALLIC GLASSES; HYDROGEN; METALLURGICAL EFFECTS; X-RAY DIFFRACTION

Citation Formats

Mizubayashi, H, Shibasaki, M, and Murayama, S. Local strain around hydrogen in amorphous Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50}. United States: N. p., 1999. Web. doi:10.1016/S1359-6454(99)00224-4.
Mizubayashi, H, Shibasaki, M, & Murayama, S. Local strain around hydrogen in amorphous Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50}. United States. https://doi.org/10.1016/S1359-6454(99)00224-4
Mizubayashi, H, Shibasaki, M, and Murayama, S. 1999. "Local strain around hydrogen in amorphous Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50}". United States. https://doi.org/10.1016/S1359-6454(99)00224-4.
@article{osti_20000476,
title = {Local strain around hydrogen in amorphous Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50}},
author = {Mizubayashi, H and Shibasaki, M and Murayama, S},
abstractNote = {The hydrogen-induced volume expansion, a change in the X-ray diffraction first peak due to hydrogen charging and the hydrogen Gorsky effects were measured for amorphous (a-) Cu{sub 50}Zr{sub 50} and Cu{sub 50}Ti{sub 50} and discussed together with the hydrogen Snoek peak reported. In contrast, anisotropy of the elastic distortion around hydrogen appears to be much larger in a-Cu{sub 50}Zr{sub 50} than in a-Cu{sub 50}Ti{sub 50}. It is surmised that the local atomic structures are more deformable in a-Cu{sub 50}Zr{sub 50} than in a-Cu{sub 50}Ti{sub 50}.},
doi = {10.1016/S1359-6454(99)00224-4},
url = {https://www.osti.gov/biblio/20000476}, journal = {Acta Materialia},
issn = {1359-6454},
number = 12,
volume = 47,
place = {United States},
year = {Wed Sep 29 00:00:00 EDT 1999},
month = {Wed Sep 29 00:00:00 EDT 1999}
}