Title: Galvanic corrosion of copper-coated carbon steel for used nuclear fuel containers

Authors:
ORCiD logo [1];  [1];  [2]; ORCiD logo [3];  [4];  [4]
  1. Department of Chemistry, The University of Western Ontario, London, Canada
  2. Surface Science Western, The University of Western Ontario, London, Canada
  3. Nuclear Waste Management Organization, Toronto, Canada
  4. Department of Chemistry, The University of Western Ontario, London, Canada; Surface Science Western, The University of Western Ontario, London, Canada
Publication Date:
Research Org.:
Argonne National Lab. (ANL), Argonne, IL (United States). Advanced Photon Source (APS)
Sponsoring Org.:
FOREIGN
OSTI Identifier:
1603172
Resource Type:
Journal Article
Journal Name:
Corrosion Engineering, Science and Technology
Additional Journal Information:
Journal Volume: 52; Journal Issue: sup1; Journal ID: ISSN 1478-422X
Publisher:
Taylor & Francis
Country of Publication:
United States
Language:
ENGLISH

Citation Formats

Standish, Thalia E., Zagidulin, Dmitrij, Ramamurthy, Sridhar, Keech, Peter G., Noël, James J., and Shoesmith, David W. Galvanic corrosion of copper-coated carbon steel for used nuclear fuel containers. United States: N. p., 2017. Web. doi:10.1080/1478422X.2017.1306972.
Standish, Thalia E., Zagidulin, Dmitrij, Ramamurthy, Sridhar, Keech, Peter G., Noël, James J., & Shoesmith, David W. Galvanic corrosion of copper-coated carbon steel for used nuclear fuel containers. United States. doi:10.1080/1478422X.2017.1306972.
Standish, Thalia E., Zagidulin, Dmitrij, Ramamurthy, Sridhar, Keech, Peter G., Noël, James J., and Shoesmith, David W. Fri . "Galvanic corrosion of copper-coated carbon steel for used nuclear fuel containers". United States. doi:10.1080/1478422X.2017.1306972.
@article{osti_1603172,
title = {Galvanic corrosion of copper-coated carbon steel for used nuclear fuel containers},
author = {Standish, Thalia E. and Zagidulin, Dmitrij and Ramamurthy, Sridhar and Keech, Peter G. and Noël, James J. and Shoesmith, David W.},
abstractNote = {},
doi = {10.1080/1478422X.2017.1306972},
journal = {Corrosion Engineering, Science and Technology},
issn = {1478-422X},
number = sup1,
volume = 52,
place = {United States},
year = {2017},
month = {4}
}