Iron-based amorphous alloys and methods of synthesizing iron-based amorphous alloys
Patent
·
OSTI ID:1568550
A method according to one embodiment includes combining an amorphous iron-based alloy and at least one metal selected from a group consisting of molybdenum, chromium, tungsten, boron, gadolinium, nickel phosphorous, yttrium, and alloys thereof to form a mixture, wherein the at least one metal is present in the mixture from about 5 atomic percent (at %) to about 55 at %; and ball milling the mixture at least until an amorphous alloy of the iron-based alloy and the at least one metal is formed. Several amorphous iron-based metal alloys are also presented, including corrosion-resistant amorphous iron-based metal alloys and radiation-shielding amorphous iron-based metal alloys.
- Research Organization:
- Lawrence Livermore National Laboratory (LLNL), Livermore, CA (United States)
- Sponsoring Organization:
- USDOE
- DOE Contract Number:
- AC52-07NA27344
- Assignee:
- Lawrence Livermore National Security, LLC (Livermore, CA)
- Patent Number(s):
- 10,337,088
- Application Number:
- 15/077,819
- OSTI ID:
- 1568550
- Country of Publication:
- United States
- Language:
- English
Similar Records
Iron-based amorphous alloys and methods of synthesizing iron-based amorphous alloys
Tungsten--nickel--iron--molybdenum alloys. [1 to 12 percent Ni, 0. 5 to 8 percent Fe, 0. 5 to 25 percent Mo, balance W, other additions]
Amorphous metal alloy
Patent
·
2016
·
OSTI ID:1250459
Tungsten--nickel--iron--molybdenum alloys. [1 to 12 percent Ni, 0. 5 to 8 percent Fe, 0. 5 to 25 percent Mo, balance W, other additions]
Patent
·
1976
·
OSTI ID:7116571
Amorphous metal alloy
Patent
·
1980
·
OSTI ID:6607778