Title: Dislocation dynamics modeling of precipitation strengthening in Fe–Ni–Al–Cr ferritic superalloys

Abstract

Abstract

Authors:
;
Publication Date:
Research Org.:
Univ. of Tennessee, Knoxville, TN (United States)
Sponsoring Org.:
USDOE Office of Fossil Energy (FE)
OSTI Identifier:
1541929
DOE Contract Number:  
FE0005868
Resource Type:
Journal Article
Journal Name:
Journal of Materials Research
Additional Journal Information:
Journal Volume: 32; Journal Issue: 22; Journal ID: ISSN 0884-2914
Publisher:
Materials Research Society
Country of Publication:
United States
Language:
English
Subject:
Materials Science

Citation Formats

Rawlings, Michael J. S., and Dunand, David C. Dislocation dynamics modeling of precipitation strengthening in Fe–Ni–Al–Cr ferritic superalloys. United States: N. p., 2017. Web. doi:10.1557/jmr.2017.334.
Rawlings, Michael J. S., & Dunand, David C. Dislocation dynamics modeling of precipitation strengthening in Fe–Ni–Al–Cr ferritic superalloys. United States. doi:10.1557/jmr.2017.334.
Rawlings, Michael J. S., and Dunand, David C. Tue . "Dislocation dynamics modeling of precipitation strengthening in Fe–Ni–Al–Cr ferritic superalloys". United States. doi:10.1557/jmr.2017.334.
@article{osti_1541929,
title = {Dislocation dynamics modeling of precipitation strengthening in Fe–Ni–Al–Cr ferritic superalloys},
author = {Rawlings, Michael J. S. and Dunand, David C.},
abstractNote = {Abstract},
doi = {10.1557/jmr.2017.334},
journal = {Journal of Materials Research},
issn = {0884-2914},
number = 22,
volume = 32,
place = {United States},
year = {2017},
month = {9}
}

Works referenced in this record:

Precipitation hardening of Ni-Al alloys containing large volume fractions of γ′
journal, September 1976

  • Ardell, A. J.; Munjal, V.; Chellman, D. J.
  • Metallurgical Transactions A, Vol. 7, Issue 9
  • DOI: 10.1007/BF02658809

The kinetics of precipitation from supersaturated solid solutions
journal, April 1961


Trace element effects on precipitation processes and mechanical properties in an Al-Cu-Li alloy
journal, July 1997


Scaling of Dislocation Strengthening by Multiple Obstacle Types
journal, June 2010

  • Dong, Y.; Nogaret, T.; Curtin, W. A.
  • Metallurgical and Materials Transactions A, Vol. 41, Issue 8
  • DOI: 10.1007/s11661-010-0229-z

The Hardness of Solid Solutions
journal, June 1921

  • Rosenhain, W.
  • Proceedings of the Royal Society A: Mathematical, Physical and Engineering Sciences, Vol. 99, Issue 698
  • DOI: 10.1098/rspa.1921.0034

Creep behavior of a β′(NiAl) precipitation strengthened ferritic Fe–Cr–Ni–Al alloy
journal, May 1998


The peak- and overaged states of particle strengthened materials: computer simulations
journal, August 2001


Ferritic Alloys with Extreme Creep Resistance via Coherent Hierarchical Precipitates
journal, November 2015

  • Song, Gian; Sun, Zhiqian; Li, Lin
  • Scientific Reports, Vol. 5, Issue 1
  • DOI: 10.1038/srep16327

Multiphase intermetallic alloys for structural applications
journal, September 2000


Solid-solution hardening and softening by Fe additions to NiAl
journal, January 1997


Slip Modes in B2-Type Intermetallic Alloys
journal, January 1990


On the additivity of solid solution and dispersion strengthening
journal, December 2001


Duplex Precipitates and Their Effects on the Room-temperature Fracture Behaviour of a NiAl-Strengthened Ferritic Alloy
journal, March 2015


Simulation of dislocation glide in precipitation hardened materials
journal, December 1999


Computer simulations of the glide of dissociated dislocations in lattice mismatch strengthened materials
journal, February 2002


Improvement of Creep strength in a nickel-base single-crystal superalloy by heat treatment
journal, November 1983


Neutron-diffraction study and modeling of the lattice parameters of a NiAl-precipitate-strengthened Fe-based alloy
journal, August 2012


Advances in Physical Metallurgy and Processing of Steels. Design of Ferritic Creep-resistant Steels.
journal, January 2001


Quantitative investigation of precipitation and mechanical behaviour for AA2024 friction stir welds
journal, May 2005


Discrete dislocation modeling on interaction between type-I blunt crack and cylindrical void in single crystals
journal, March 2015


Active slip systems in bcc iron during nanoindentation: A molecular dynamics study
journal, September 2013


Enabling microstructural changes of FCC/BCC alloys in 2D dislocation dynamics
journal, March 2015


Effects of Al on the microstructure and ductility of NiAl-strengthened ferritic steels at room temperature
journal, August 2010


Calculation of the taylor factor and lattice rotations for bcc metals deforming by pencil glide
journal, December 1971

  • Rosenberg, J. M.; Piehler, H. R.
  • Metallurgical Transactions, Vol. 2, Issue 1
  • DOI: 10.1007/BF02662666

Incorporating three-dimensional mechanisms into two-dimensional dislocation dynamics
journal, April 2004

  • Benzerga, A. A.; chet, Y. Br; Needleman, A.
  • Modelling and Simulation in Materials Science and Engineering, Vol. 12, Issue 3
  • DOI: 10.1088/0965-0393/12/3/C01

A model for precipitation kinetics and strengthening in Al–Cu–Mg alloys
journal, January 2008

  • Khan, I. N.; Starink, M. J.; Yan, J. L.
  • Materials Science and Engineering: A, Vol. 472, Issue 1-2
  • DOI: 10.1016/j.msea.2007.03.033

Interfacial dislocation motion and interactions in single-crystal superalloys
journal, October 2014


Superposition of dispersion strengthening and size-mismatch strengthening: Computer simulations
journal, January 2003


Characterization of nanoscale NiAl-type precipitates in a ferritic steel by electron microscopy and atom probe tomography
journal, July 2010


Simulations of dislocation glide in overaged precipitation-hardened crystals
journal, April 2001


The critical resolved shear stress of γ′-strengthened nickel-based superalloys with γ′-volume fractions between 0.07 and 0.47
journal, April 1992


The operative slip system and general plasticity of NiAl-II
journal, November 1966


Formation and role of dislocation networks during high temperature creep of a single crystal nickel–base superalloy
journal, February 2000


Ferritic Fe–Al–Ni–Cr alloys with coherent precipitates for high-temperature applications
journal, December 2004


Synergetic effects in the superposition of strengthening mechanisms
journal, December 1992


Precipitation hardening
journal, December 1985


A non-singular continuum theory of dislocations
journal, March 2006

  • Cai, W.; Arsenlis, A.; Weinberger, C.
  • Journal of the Mechanics and Physics of Solids, Vol. 54, Issue 3
  • DOI: 10.1016/j.jmps.2005.09.005

The determination of the 1/2<lll> {110} antiphase boundary energy of NiAl
journal, July 1973


Comparison between dislocation dynamics model predictions and experiments in precipitation-strengthened Al–Li–Sc alloys
journal, October 2014


A two-dimensional dislocation dynamics model of the plastic deformation of polycrystalline metals
journal, December 2010

  • Ahmed, Naveed; Hartmaier, Alexander
  • Journal of the Mechanics and Physics of Solids, Vol. 58, Issue 12
  • DOI: 10.1016/j.jmps.2010.09.005

The physical meaning of indentation and scratch hardness
journal, May 1956


Precipitation hardening of superalloys by ordered γ′-particles
journal, January 1985


Dislocation dynamics simulations of precipitation hardening in Ni-based superalloys with high γ′ volume fraction
journal, December 2009


Characterization of interfacial dislocation networks in a creep-deformed nickel-base superalloy
journal, January 1993


Discrete dislocation dynamics simulation of cutting of γ′ precipitate and interfacial dislocation network in Ni-based superalloys
journal, April 2006


Creep properties and microstructure of a precipitation-strengthened ferritic Fe–Al–Ni–Cr alloy
journal, June 2014


Nano-sized precipitate stability and its controlling factors in a NiAl-strengthened ferritic alloy
journal, November 2015

  • Sun, Zhiqian; Song, Gian; Ilavsky, Jan
  • Scientific Reports, Vol. 5, Issue 1
  • DOI: 10.1038/srep16081