Stabilization of Polyoxometalate Water Oxidation Catalysts on Hematite by Atomic Layer Deposition
Journal Article
·
· ACS Applied Materials and Interfaces
- Department of Chemistry, Emory University, 1515 Dickey Drive, Atlanta, Georgia 30322, United States
- School of Materials Science and Engineering, Georgia Institute of Technology, Love Manufacturing Building, 771 Ferst Drive NW, Atlanta, Georgia 30332, United States
- Department of Chemistry, Merkert Chemistry Center, Boston College, 2609 Beacon Street, Chestnut Hill, Massachusetts 02467, United States
Not provided.
- Research Organization:
- Emory Univ., Atlanta, GA (United States)
- Sponsoring Organization:
- USDOE Office of Science (SC)
- DOE Contract Number:
- FG02-07ER15906
- OSTI ID:
- 1539454
- Journal Information:
- ACS Applied Materials and Interfaces, Vol. 9, Issue 40; ISSN 1944-8244
- Publisher:
- American Chemical Society (ACS)
- Country of Publication:
- United States
- Language:
- English
Similar Records
Atomic Layer Deposition of a Submonolayer Catalyst for the Enhanced Photoelectrochemical Performance of Water Oxidation with Hematite
Atomic Layer Deposition of a Submonolayer Catalyst for the Enhanced Photoelectrochemical Performance of Water Oxidation with Hematite
Atomic Layer Deposition of a Submonolayer Catalyst for the Enhanced Photoelectrochemical Performance of Water Oxidation with Hematite
Journal Article
·
Tue Jan 01 00:00:00 EST 2013
· ACS Nano
·
OSTI ID:1539454
+5 more
Atomic Layer Deposition of a Submonolayer Catalyst for the Enhanced Photoelectrochemical Performance of Water Oxidation with Hematite
Journal Article
·
Tue Mar 26 00:00:00 EDT 2013
· ACS Nano
·
OSTI ID:1539454
+5 more
Atomic Layer Deposition of a Submonolayer Catalyst for the Enhanced Photoelectrochemical Performance of Water Oxidation with Hematite
Journal Article
·
Thu Feb 28 00:00:00 EST 2013
· ACS Nano
·
OSTI ID:1539454
+5 more