Title: Enabling Large Superalloy Parts Using Compact Coprecipitation of γ' and γ"

Abstract

Not provided.

Authors:
; ; ; ; ; ; ;
Publication Date:
Research Org.:
General Electric Company, Boston, MA (United States)
Sponsoring Org.:
USDOE Office of Fossil Energy (FE)
OSTI Identifier:
1537814
DOE Contract Number:  
FE0026299
Resource Type:
Journal Article
Journal Name:
Metallurgical and Materials Transactions. A, Physical Metallurgy and Materials Science
Additional Journal Information:
Journal Volume: 49; Journal Issue: 3; Journal ID: ISSN 1073-5623
Publisher:
ASM International
Country of Publication:
United States
Language:
English
Subject:
Materials Science; Metallurgy & Metallurgical Engineering

Citation Formats

Detor, Andrew J., DiDomizio, Richard, Sharghi-Moshtaghin, Reza, Zhou, Ning, Shi, Rongpei, Wang, Yunzhi, McAllister, Donald P., and Mills, Michael J. Enabling Large Superalloy Parts Using Compact Coprecipitation of γ' and γ". United States: N. p., 2017. Web. doi:10.1007/s11661-017-4356-7.
Detor, Andrew J., DiDomizio, Richard, Sharghi-Moshtaghin, Reza, Zhou, Ning, Shi, Rongpei, Wang, Yunzhi, McAllister, Donald P., & Mills, Michael J. Enabling Large Superalloy Parts Using Compact Coprecipitation of γ' and γ". United States. doi:10.1007/s11661-017-4356-7.
Detor, Andrew J., DiDomizio, Richard, Sharghi-Moshtaghin, Reza, Zhou, Ning, Shi, Rongpei, Wang, Yunzhi, McAllister, Donald P., and Mills, Michael J. Tue . "Enabling Large Superalloy Parts Using Compact Coprecipitation of γ' and γ"". United States. doi:10.1007/s11661-017-4356-7.
@article{osti_1537814,
title = {Enabling Large Superalloy Parts Using Compact Coprecipitation of γ' and γ"},
author = {Detor, Andrew J. and DiDomizio, Richard and Sharghi-Moshtaghin, Reza and Zhou, Ning and Shi, Rongpei and Wang, Yunzhi and McAllister, Donald P. and Mills, Michael J.},
abstractNote = {Not provided.},
doi = {10.1007/s11661-017-4356-7},
journal = {Metallurgical and Materials Transactions. A, Physical Metallurgy and Materials Science},
issn = {1073-5623},
number = 3,
volume = 49,
place = {United States},
year = {2017},
month = {10}
}

Works referenced in this record:

A generalized field method for multiphase transformations using interface fields
journal, December 1999


Multi phase field model for solid state transformation with elastic strain
journal, May 2006


Alloying behaviour of Ni3Al, Ni3Ga, Ni3Si and Ni3Ge
journal, February 1984


Morphology of y’ and y” precipitates and thermal stability of inconel 718 type alloys
journal, January 1973

  • Cozar, R.; Pineau, A.
  • Metallurgical Transactions, Vol. 4, Issue 1
  • DOI: 10.1007/BF02649604

Precipitation hardening of superalloys by ordered γ′-particles
journal, January 1985


Cooling precipitation and strengthening study in powder metallurgy superalloy U720LI
journal, October 2001

  • Mao, Jian; Chang, Keh-Minn; Yang, Wanhong
  • Metallurgical and Materials Transactions A, Vol. 32, Issue 10
  • DOI: 10.1007/s11661-001-0034-9

Effect of continuous cooling rate on the precipitation of gamma prime in nickel-based superalloys
journal, August 1995


Nanoscale Characterization of Elemental Partitioning between Gamma and Gamma Prime Phases in René 88 DT Nickel-Base Superalloy
journal, November 2008

  • Hwang, J. Y.; Banerjee, R.; Tiley, J.
  • Metallurgical and Materials Transactions A, Vol. 40, Issue 1
  • DOI: 10.1007/s11661-008-9691-2

Phase-field models in materials science
journal, July 2009


Nano γ′/γ ″ composite precipitates in Alloy 718
journal, May 2012

  • Phillips, P. J.; McAllister, D.; Gao, Y.
  • Applied Physics Letters, Vol. 100, Issue 21
  • DOI: 10.1063/1.4721456

Phase stability and yield stress of Ni-base superalloys containing high Co and Ti
journal, November 2006

  • Cui, C. Y.; Sato, A.; Gu, Y. F.
  • Metallurgical and Materials Transactions A, Vol. 37, Issue 11
  • DOI: 10.1007/BF02586152

Influence of cooling rate on the development of multiple generations of γ′ precipitates in a commercial nickel base superalloy
journal, September 2011


Interfaces in a modified Inconel 718 with compact precipitates
journal, December 1998