skip to main content
OSTI.GOV title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Mechanical Property Evolution of Silicon Composite Electrodes Studied by Environmental Nanoindentation

Abstract

Not provided.

Authors:
 [1];  [2];  [3];  [1];  [4];  [1];  [2];  [1]
  1. Department of Chemical and Materials Engineering, University of Kentucky, Lexington KY 40506 USA
  2. Chemical and Materials Systems Lab, General Motors Research and Development Center, Warren MI 48090 USA
  3. Department of Chemical and Materials Engineering, University of Kentucky, Lexington KY 40506 USA; Shanghai Institute of Applied Mathematics and Mechanics, Shanghai University, Shanghai 200072 China
  4. Optimal, Inc., 47802 West Anchor Court Plymouth MI 48170 USA
Publication Date:
Research Org.:
General Motors LLC, Detroit, MI (United States)
Sponsoring Org.:
USDOE Office of Energy Efficiency and Renewable Energy (EERE)
OSTI Identifier:
1537414
DOE Contract Number:  
EE0007787
Resource Type:
Journal Article
Journal Name:
Advanced Energy Materials
Additional Journal Information:
Journal Volume: 8; Journal Issue: 10; Journal ID: ISSN 1614-6832
Publisher:
Wiley
Country of Publication:
United States
Language:
English
Subject:
Chemistry; Energy & Fuels; Materials Science; Physics

Citation Formats

Wang, Yikai, Zhang, Qinglin, Li, Dawei, Hu, Jiazhi, Xu, Jiagang, Dang, Dingying, Xiao, Xingcheng, and Cheng, Yang-Tse. Mechanical Property Evolution of Silicon Composite Electrodes Studied by Environmental Nanoindentation. United States: N. p., 2018. Web. doi:10.1002/aenm.201702578.
Wang, Yikai, Zhang, Qinglin, Li, Dawei, Hu, Jiazhi, Xu, Jiagang, Dang, Dingying, Xiao, Xingcheng, & Cheng, Yang-Tse. Mechanical Property Evolution of Silicon Composite Electrodes Studied by Environmental Nanoindentation. United States. doi:10.1002/aenm.201702578.
Wang, Yikai, Zhang, Qinglin, Li, Dawei, Hu, Jiazhi, Xu, Jiagang, Dang, Dingying, Xiao, Xingcheng, and Cheng, Yang-Tse. Tue . "Mechanical Property Evolution of Silicon Composite Electrodes Studied by Environmental Nanoindentation". United States. doi:10.1002/aenm.201702578.
@article{osti_1537414,
title = {Mechanical Property Evolution of Silicon Composite Electrodes Studied by Environmental Nanoindentation},
author = {Wang, Yikai and Zhang, Qinglin and Li, Dawei and Hu, Jiazhi and Xu, Jiagang and Dang, Dingying and Xiao, Xingcheng and Cheng, Yang-Tse},
abstractNote = {Not provided.},
doi = {10.1002/aenm.201702578},
journal = {Advanced Energy Materials},
issn = {1614-6832},
number = 10,
volume = 8,
place = {United States},
year = {2018},
month = {1}
}

Works referenced in this record:

Amorphous silicon as a possible anode material for Li-ion batteries
journal, September 1999


Structural Changes in Silicon Anodes during Lithium Insertion/Extraction
journal, January 2004

  • Obrovac, M. N.; Christensen, Leif
  • Electrochemical and Solid-State Letters, Vol. 7, Issue 5
  • DOI: 10.1149/1.1652421

Alloy Negative Electrodes for Li-Ion Batteries
journal, October 2014

  • Obrovac, M. N.; Chevrier, V. L.
  • Chemical Reviews, Vol. 114, Issue 23
  • DOI: 10.1021/cr500207g

Silicon based lithium-ion battery anodes: A chronicle perspective review
journal, January 2017


Best Practice: Performance and Cost Evaluation of Lithium Ion Battery Active Materials with Special Emphasis on Energy Efficiency
journal, October 2016


Size-Dependent Fracture of Silicon Nanoparticles During Lithiation
journal, January 2012

  • Liu, Xiao Hua; Zhong, Li; Huang, Shan
  • ACS Nano, Vol. 6, Issue 2
  • DOI: 10.1021/nn204476h

Anisotropic Swelling and Fracture of Silicon Nanowires during Lithiation
journal, August 2011

  • Liu, Xiao Hua; Zheng, He; Zhong, Li
  • Nano Letters, Vol. 11, Issue 8, p. 3312-3318
  • DOI: 10.1021/nl201684d

Crack Pattern Formation in Thin Film Lithium-Ion Battery Electrodes
journal, January 2011

  • Li, Juchuan; Dozier, Alan K.; Li, Yunchao
  • Journal of The Electrochemical Society, Vol. 158, Issue 6
  • DOI: 10.1149/1.3574027

Toward High Cycle Efficiency of Silicon-Based Negative Electrodes by Designing the Solid Electrolyte Interphase
journal, November 2014

  • Zhang, Qinglin; Xiao, Xingcheng; Zhou, Weidong
  • Advanced Energy Materials, Vol. 5, Issue 5
  • DOI: 10.1002/aenm.201401398

A Step toward High-Energy Silicon-Based Thin Film Lithium Ion Batteries
journal, April 2017


Running out of lithium? A route to differentiate between capacity losses and active lithium losses in lithium-ion batteries
journal, January 2017

  • Holtstiege, Florian; Wilken, Andrea; Winter, Martin
  • Physical Chemistry Chemical Physics, Vol. 19, Issue 38
  • DOI: 10.1039/C7CP05405J

Deformation and Chemomechanical Degradation at Solid Electrolyte–Electrode Interfaces
journal, July 2017


Unveiling the Critical Role of Polymeric Binders for Silicon Negative Electrodes in Lithium-Ion Full Cells
journal, January 2017

  • Xu, Jiagang; Zhang, Long; Wang, Yikai
  • ACS Applied Materials & Interfaces, Vol. 9, Issue 4
  • DOI: 10.1021/acsami.6b11121

Microstructural degradation of silicon electrodes during lithiation observed via operando X-ray tomographic imaging
journal, February 2017


Reversible High-Capacity Si Nanocomposite Anodes for Lithium-ion Batteries Enabled by Molecular Layer Deposition
journal, December 2013

  • Piper, Daniela Molina; Travis, Jonathan J.; Young, Matthias
  • Advanced Materials, Vol. 26, Issue 10
  • DOI: 10.1002/adma.201304714

Lithium-Assisted Plastic Deformation of Silicon Electrodes in Lithium-Ion Batteries: A First-Principles Theoretical Study
journal, July 2011

  • Zhao, Kejie; Wang, Wei L.; Gregoire, John
  • Nano Letters, Vol. 11, Issue 7
  • DOI: 10.1021/nl201501s

Voltage hysteresis of lithium ion batteries caused by mechanical stress
journal, January 2016

  • Lu, Bo; Song, Yicheng; Zhang, Qinglin
  • Physical Chemistry Chemical Physics, Vol. 18, Issue 6
  • DOI: 10.1039/C5CP06179B

Electrochemical stiffness in lithium-ion batteries
journal, August 2016

  • Tavassol, Hadi; Jones, Elizabeth M. C.; Sottos, Nancy R.
  • Nature Materials, Vol. 15, Issue 11
  • DOI: 10.1038/nmat4708

High damage tolerance of electrochemically lithiated silicon
journal, September 2015

  • Wang, Xueju; Fan, Feifei; Wang, Jiangwei
  • Nature Communications, Vol. 6, Issue 1
  • DOI: 10.1038/ncomms9417

In situ measurement of mechanical property and stress evolution in a composite silicon electrode
journal, October 2017


Elastic softening of amorphous and crystalline Li–Si Phases with increasing Li concentration: A first-principles study
journal, October 2010


Structure and Properties of Li−Si Alloys: A First-Principles Study
journal, December 2010

  • Kim, Hyunwoo; Chou, Chia-Yun; Ekerdt, John G.
  • The Journal of Physical Chemistry C, Vol. 115, Issue 5
  • DOI: 10.1021/jp1083899

Ex-situ depth-sensing indentation measurements of electrochemically produced Si–Li alloy films
journal, August 2011


In Situ Porous Structure Characterization of Electrodes for Energy Storage and Conversion by EQCM-D: a Review
journal, April 2017


Improved Mechanical Integrity of ALD-Coated Composite Electrodes for Li-Ion Batteries
journal, January 2011

  • Riley, Leah A.; Cavanagh, Andrew S.; George, Steven M.
  • Electrochemical and Solid-State Letters, Vol. 14, Issue 3
  • DOI: 10.1149/1.3529367

Effect of porosity on electrochemical and mechanical properties of composite Li-ion anodes
journal, January 2015

  • Antartis, Dimitrios; Dillon, Shen; Chasiotis, Ioannis
  • Journal of Composite Materials, Vol. 49, Issue 15
  • DOI: 10.1177/0021998314568653

Consequences of air exposure on the lithiated graphite SEI
journal, August 2013


Examining Solid Electrolyte Interphase Formation on Crystalline Silicon Electrodes: Influence of Electrochemical Preparation and Ambient Exposure Conditions
journal, September 2012

  • Schroder, Kjell W.; Celio, Hugo; Webb, Lauren J.
  • The Journal of Physical Chemistry C, Vol. 116, Issue 37
  • DOI: 10.1021/jp307372m

Electronic Origin for the Phase Transition from Amorphous Li x Si to Crystalline Li 15 Si 4
journal, June 2013

  • Gu, Meng; Wang, Zhiguo; Connell, Justin G.
  • ACS Nano, Vol. 7, Issue 7
  • DOI: 10.1021/nn402349j

Toward Efficient Binders for Li-Ion Battery Si-Based Anodes: Polyacrylic Acid
journal, October 2010

  • Magasinski, Alexandre; Zdyrko, Bogdan; Kovalenko, Igor
  • ACS Applied Materials & Interfaces, Vol. 2, Issue 11
  • DOI: 10.1021/am100871y

Preparation of Poly(vinylidene fluoride) Lithium-Ion Battery Separators and Their Compatibilization with Ionic Liquid - A Green Solvent Approach
journal, July 2017

  • Costa, Carlos M.; Rodrigues, Henrique M.; Gören, Attila
  • ChemistrySelect, Vol. 2, Issue 19
  • DOI: 10.1002/slct.201701028

In Situ Quantification of the Swelling of Graphite Composite Electrodes by Scanning Electrochemical Microscopy
journal, October 2015

  • Bülter, Heinz; Peters, Fabian; Schwenzel, Julian
  • Journal of The Electrochemical Society, Vol. 163, Issue 2
  • DOI: 10.1149/2.1061514jes

Enhanced Cycle Life of Si Anode for Li-Ion Batteries by Using Modified Elastomeric Binder
journal, January 2005

  • Liu, Wei-Ren; Yang, Mo-Hua; Wu, Hung-Chun
  • Electrochemical and Solid-State Letters, Vol. 8, Issue 2
  • DOI: 10.1149/1.1847685

Mechanical Degradation of Graphite/PVDF Composite Electrodes: A Model-Experimental Study
journal, December 2015

  • Takahashi, Kenji; Higa, Kenneth; Mair, Sunil
  • Journal of The Electrochemical Society, Vol. 163, Issue 3
  • DOI: 10.1149/2.0271603jes

A nanoindentation study of the viscoplastic behavior of pure lithium
journal, March 2017


Molecular Layer Deposition for Surface Modification of Lithium-Ion Battery Electrodes
journal, October 2016


A Robust Ion-Conductive Biopolymer as a Binder for Si Anodes of Lithium-Ion Batteries
journal, May 2015

  • Liu, Jie; Zhang, Qian; Zhang, Tao
  • Advanced Functional Materials, Vol. 25, Issue 23
  • DOI: 10.1002/adfm.201500589

Water Soluble Binder, an Electrochemical Performance Booster for Electrode Materials with High Energy Density
journal, July 2017

  • Li, Jun-Tao; Wu, Zhan-Yu; Lu, Yan-Qiu
  • Advanced Energy Materials, Vol. 7, Issue 24
  • DOI: 10.1002/aenm.201701185

Systematic Investigation of the Alucone-Coating Enhancement on Silicon Anodes
journal, November 2017

  • Son, Seoung-Bum; Wang, Yikai; Xu, Jiagang
  • ACS Applied Materials & Interfaces, Vol. 9, Issue 46
  • DOI: 10.1021/acsami.7b08960

An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments
journal, June 1992

  • Oliver, W. C.; Pharr, G. M.
  • Journal of Materials Research, Vol. 7, Issue 06, p. 1564-1583
  • DOI: 10.1557/JMR.1992.1564

Spherical indentation of porous ceramics: Elasticity and hardness
journal, May 2016


The nanogranular nature of C–S–H
journal, January 2007

  • Constantinides, Georgios; Ulm, Franz-Josef
  • Journal of the Mechanics and Physics of Solids, Vol. 55, Issue 1
  • DOI: 10.1016/j.jmps.2006.06.003

Mesoscale texture of cement hydrates
journal, February 2016

  • Ioannidou, Katerina; Krakowiak, Konrad J.; Bauchy, Mathieu
  • Proceedings of the National Academy of Sciences, Vol. 113, Issue 8
  • DOI: 10.1073/pnas.1520487113

Statistical Indentation Techniques for Hydrated Nanocomposites: Concrete, Bone, and Shale
journal, September 2007


High Capacity Silicon Electrodes with Nafion as Binders for Lithium-Ion Batteries
journal, December 2015

  • Xu, Jiagang; Zhang, Qinglin; Cheng, Yang-Tse
  • Journal of The Electrochemical Society, Vol. 163, Issue 3
  • DOI: 10.1149/2.0261603jes

An In Situ X-Ray Diffraction Study of the Reaction of Li with Crystalline Si
journal, January 2007

  • Li, Jing; Dahn, J. R.
  • Journal of The Electrochemical Society, Vol. 154, Issue 3
  • DOI: 10.1149/1.2409862

In Situ XRD and Electrochemical Study of the Reaction of Lithium with Amorphous Silicon
journal, January 2004

  • Hatchard, T. D.; Dahn, J. R.
  • Journal of The Electrochemical Society, Vol. 151, Issue 6
  • DOI: 10.1149/1.1739217

In Situ X-ray Diffraction Studies of (De)lithiation Mechanism in Silicon Nanowire Anodes
journal, May 2012

  • Misra, Sumohan; Liu, Nian; Nelson, Johanna
  • ACS Nano, Vol. 6, Issue 6
  • DOI: 10.1021/nn301339g

Wet Nanoindentation of the Solid Electrolyte Interphase on Thin Film Si Electrodes
journal, October 2015

  • Kuznetsov, Volodymyr; Zinn, Arndt-Hendrik; Zampardi, Giorgia
  • ACS Applied Materials & Interfaces, Vol. 7, Issue 42
  • DOI: 10.1021/acsami.5b06700

Direct Observation of Inhomogeneous Solid Electrolyte Interphase on MnO Anode with Atomic Force Microscopy and Spectroscopy
journal, January 2012

  • Zhang, Jie; Wang, Rui; Yang, Xiaocheng
  • Nano Letters, Vol. 12, Issue 4
  • DOI: 10.1021/nl300570d

A Major Constituent of Brown Algae for Use in High-Capacity Li-Ion Batteries
journal, September 2011


The Effects of Cross-Linking in a Supramolecular Binder on Cycle Life in Silicon Microparticle Anodes
journal, January 2016

  • Lopez, Jeffrey; Chen, Zheng; Wang, Chao
  • ACS Applied Materials & Interfaces, Vol. 8, Issue 3
  • DOI: 10.1021/acsami.5b11363

Highly elastic binders integrating polyrotaxanes for silicon microparticle anodes in lithium ion batteries
journal, July 2017


Chemically stable artificial SEI for Li-ion battery electrodes
journal, March 2017

  • Zhang, Qinglin; Han, Lei; Pan, Jie
  • Applied Physics Letters, Vol. 110, Issue 13
  • DOI: 10.1063/1.4979108

Enhanced Lithiation Cycle Stability of ALD-Coated Confined a-Si Microstructures Determined Using In Situ AFM
journal, January 2016

  • Becker, Collin R.; Prokes, S. M.; Love, Corey T.
  • ACS Applied Materials & Interfaces, Vol. 8, Issue 1
  • DOI: 10.1021/acsami.5b09544

Surface Fluorination of Reactive Battery Anode Materials for Enhanced Stability
journal, August 2017

  • Zhao, Jie; Liao, Lei; Shi, Feifei
  • Journal of the American Chemical Society, Vol. 139, Issue 33
  • DOI: 10.1021/jacs.7b05251

A Stretchable Graphitic Carbon/Si Anode Enabled by Conformal Coating of a Self-Healing Elastic Polymer
journal, January 2016

  • Sun, Yongming; Lopez, Jeffrey; Lee, Hyun-Wook
  • Advanced Materials, Vol. 28, Issue 12
  • DOI: 10.1002/adma.201504723