Title: High-Surface Area Ceria-Zirconia Films Prepared by Atomic Layer Deposition

Abstract

Not provided.

Authors:
; ; ; ; ;
Publication Date:
Research Org.:
Univ. of Pennsylvania, Philadelphia, PA (United States)
Sponsoring Org.:
USDOE Office of Science (SC)
OSTI Identifier:
1533327
DOE Contract Number:  
SC0009440
Resource Type:
Journal Article
Journal Name:
Catalysis Letters
Additional Journal Information:
Journal Volume: 147; Journal Issue: 6; Journal ID: ISSN 1011-372X
Publisher:
Springer
Country of Publication:
United States
Language:
English
Subject:
Chemistry

Citation Formats

Onn, Tzia Ming, Dai, Sheng, Chen, Jiayao, Pan, Xiaoqing, Graham, George W., and Gorte, Raymond J. High-Surface Area Ceria-Zirconia Films Prepared by Atomic Layer Deposition. United States: N. p., 2017. Web. doi:10.1007/s10562-017-2053-1.
Onn, Tzia Ming, Dai, Sheng, Chen, Jiayao, Pan, Xiaoqing, Graham, George W., & Gorte, Raymond J. High-Surface Area Ceria-Zirconia Films Prepared by Atomic Layer Deposition. United States. doi:10.1007/s10562-017-2053-1.
Onn, Tzia Ming, Dai, Sheng, Chen, Jiayao, Pan, Xiaoqing, Graham, George W., and Gorte, Raymond J. Mon . "High-Surface Area Ceria-Zirconia Films Prepared by Atomic Layer Deposition". United States. doi:10.1007/s10562-017-2053-1.
@article{osti_1533327,
title = {High-Surface Area Ceria-Zirconia Films Prepared by Atomic Layer Deposition},
author = {Onn, Tzia Ming and Dai, Sheng and Chen, Jiayao and Pan, Xiaoqing and Graham, George W. and Gorte, Raymond J.},
abstractNote = {Not provided.},
doi = {10.1007/s10562-017-2053-1},
journal = {Catalysis Letters},
issn = {1011-372X},
number = 6,
volume = 147,
place = {United States},
year = {2017},
month = {4}
}

Works referenced in this record:

Studies of the water-gas-shift reaction on ceria-supported Pt, Pd, and Rh: Implications for oxygen-storage properties
journal, January 1998


The effect of CeO2 structure on the activity of supported Pd catalysts used for methane steam reforming
journal, April 2002


Automotive exhaust catalysis
journal, May 2003


On the Role of Oxygen Storage in Three-Way Catalysis
journal, April 2004


The effect of ceria content on the properties of Pd/CeO2/Al2O3 catalysts for steam reforming of methane
journal, January 2007


“Redox” vs “associative formate with –OH group regeneration” WGS reaction mechanism on Pt/CeO2: Effect of platinum particle size
journal, April 2011

  • Kalamaras, Christos M.; Americanou, Sofia; Efstathiou, Angelos M.
  • Journal of Catalysis, Vol. 279, Issue 2
  • DOI: 10.1016/j.jcat.2011.01.024

Low-temperature water-gas shift on Pt/Ce1−xLaxO2−δ: Effect of Ce/La ratio
journal, August 2013


Ceria-based palladium zinc catalysts as promising materials for water gas shift reaction
journal, March 2014


Oxidation enthalpies for reduction of ceria surfaces
journal, June 2007


Thermally Induced Deactivation and the Corresponding Strategies for Improving Durability in Automotive Three-Way Catalysts
journal, July 2016

  • He, By Jun-Jun; Wang, Cheng-Xiong; Zheng, Ting-Ting
  • Johnson Matthey Technology Review, Vol. 60, Issue 3
  • DOI: 10.1595/205651316X691960

A new concept in high performance ceria–zirconia oxygen storage capacity material with Al2O3 as a diffusion barrier
journal, February 2008

  • Morikawa, Akira; Suzuki, Tadashi; Kanazawa, Takaaki
  • Applied Catalysis B: Environmental, Vol. 78, Issue 3-4
  • DOI: 10.1016/j.apcatb.2007.09.013

Fundamentals and Catalytic Applications of CeO 2 -Based Materials
journal, April 2016


Evidence for Entropy Effects in the Reduction of Ceria−Zirconia Solutions
journal, October 2006

  • Shah, Parag R.; Kim, Taeyoon; Zhou, Gong
  • Chemistry of Materials, Vol. 18, Issue 22
  • DOI: 10.1021/cm061374f

Thermodynamic Investigation of the Redox Properties of Ceria−Zirconia Solid Solutions
journal, August 2006

  • Kim, Taeyoon; Vohs, John M.; Gorte, Raymond J.
  • Industrial & Engineering Chemistry Research, Vol. 45, Issue 16
  • DOI: 10.1021/ie0511478

Atomic layer deposition of transition metals
journal, October 2003

  • Lim, Booyong S.; Rahtu, Antti; Gordon, Roy G.
  • Nature Materials, Vol. 2, Issue 11
  • DOI: 10.1038/nmat1000

Controlled Growth of Platinum Nanoparticles on Strontium Titanate Nanocubes by Atomic Layer Deposition
journal, March 2009

  • Christensen, Steven T.; Elam, Jeffrey W.; Rabuffetti, Federico A.
  • Small, Vol. 5, Issue 6
  • DOI: 10.1002/smll.200801920

Supported Ru−Pt Bimetallic Nanoparticle Catalysts Prepared by Atomic Layer Deposition
journal, August 2010

  • Christensen, Steven T.; Feng, Hao; Libera, Joseph L.
  • Nano Letters, Vol. 10, Issue 8
  • DOI: 10.1021/nl101567m

A brief review of atomic layer deposition: from fundamentals to applications
journal, June 2014


Catalyst Design with Atomic Layer Deposition
journal, February 2015

  • O’Neill, Brandon J.; Jackson, David H. K.; Lee, Jechan
  • ACS Catalysis, Vol. 5, Issue 3
  • DOI: 10.1021/cs501862h

High-surface-area ceria prepared by ALD on Al2O3 support
journal, February 2017


Low Temperature Epitaxial Oxide Ultrathin Films and Nanostructures by Atomic Layer Deposition
journal, September 2012

  • Coll, Mariona; Gazquez, Jaume; Palau, Anna
  • Chemistry of Materials, Vol. 24, Issue 19
  • DOI: 10.1021/cm301864c

Characterisation of ceria–zirconia solid solutions after hydrothermal ageing
journal, October 2001


CO oxidation for the characterization of reducibility in oxygen storage components of three-way automotive catalysts
journal, December 1997


Control of Metal Nanocrystal Size Reveals Metal-Support Interface Role for Ceria Catalysts
journal, July 2013


Improved Thermal Stability and Methane-Oxidation Activity of Pd/Al 2 O 3 Catalysts by Atomic Layer Deposition of ZrO 2
journal, August 2015


Modification of Pd/CeO2 catalyst by Atomic Layer Deposition of ZrO2
journal, November 2016


High-surface-area, iron-oxide films prepared by atomic layer deposition on γ-Al2O3
journal, March 2017