Title: Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys

Abstract

Intergranular stress-corrosion cracking (IGSCC) is a form of environmentally induced crack propagation causing premature failure of elemental metals and alloys. It is believed to require the simultaneous presence of tensile stress and corrosion; however, the exact nature of this synergy has eluded experimental identification. For noble metal alloys such as Ag–Au, IGSCC is a consequence of dealloying corrosion, forming a nanoporous gold layer that is believed to have the ability to transmit cracks into grain boundaries in un-dealloyed parent phase via a pure mechanical process. Here using atomic-scale techniques and statistical characterizations for this alloy system, we show that the separate roles of stress and anodic dissolution can be decoupled and that the apparent synergy exists owing to rapid time-dependent morphology changes at the dealloyed layer/parent phase interface. We discuss the applicability of our findings to the IGSCC of important engineering Fe- and Ni-based alloys in critical applications.

Authors:
 [1];  [1];  [2];  [2];  [2];  [1];  [1];  [2];  [1]
  1. Arizona State Univ., Tempe, AZ (United States)
  2. Pacific Northwest National Lab. (PNNL), Richland, WA (United States)
Publication Date:
Research Org.:
Pacific Northwest National Lab. (PNNL), Richland, WA (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
1507375
Report Number(s):
PNNL-SA-138538
Journal ID: ISSN 1476-1122
Grant/Contract Number:  
AC05-76RL01830
Resource Type:
Journal Article: Accepted Manuscript
Journal Name:
Nature Materials
Additional Journal Information:
Journal Volume: 17; Journal Issue: 10; Journal ID: ISSN 1476-1122
Publisher:
Springer Nature - Nature Publishing Group
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; atom probe tomography (APT); Stress Corrision Cracking; transmission electron microscopy (TEM)

Citation Formats

Badwe, Nilesh, Chen, X., Schreiber, Daniel K., Olszta, Matthew J., Overman, Nicole R., Karasz, E. K., Tse, A. Y., Bruemmer, Stephen M., and Sieradzki, Karl. Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys. United States: N. p., 2018. Web. doi:10.1038/s41563-018-0162-x.
Badwe, Nilesh, Chen, X., Schreiber, Daniel K., Olszta, Matthew J., Overman, Nicole R., Karasz, E. K., Tse, A. Y., Bruemmer, Stephen M., & Sieradzki, Karl. Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys. United States. doi:10.1038/s41563-018-0162-x.
Badwe, Nilesh, Chen, X., Schreiber, Daniel K., Olszta, Matthew J., Overman, Nicole R., Karasz, E. K., Tse, A. Y., Bruemmer, Stephen M., and Sieradzki, Karl. Mon . "Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys". United States. doi:10.1038/s41563-018-0162-x. https://www.osti.gov/servlets/purl/1507375.
@article{osti_1507375,
title = {Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys},
author = {Badwe, Nilesh and Chen, X. and Schreiber, Daniel K. and Olszta, Matthew J. and Overman, Nicole R. and Karasz, E. K. and Tse, A. Y. and Bruemmer, Stephen M. and Sieradzki, Karl},
abstractNote = {Intergranular stress-corrosion cracking (IGSCC) is a form of environmentally induced crack propagation causing premature failure of elemental metals and alloys. It is believed to require the simultaneous presence of tensile stress and corrosion; however, the exact nature of this synergy has eluded experimental identification. For noble metal alloys such as Ag–Au, IGSCC is a consequence of dealloying corrosion, forming a nanoporous gold layer that is believed to have the ability to transmit cracks into grain boundaries in un-dealloyed parent phase via a pure mechanical process. Here using atomic-scale techniques and statistical characterizations for this alloy system, we show that the separate roles of stress and anodic dissolution can be decoupled and that the apparent synergy exists owing to rapid time-dependent morphology changes at the dealloyed layer/parent phase interface. We discuss the applicability of our findings to the IGSCC of important engineering Fe- and Ni-based alloys in critical applications.},
doi = {10.1038/s41563-018-0162-x},
journal = {Nature Materials},
issn = {1476-1122},
number = 10,
volume = 17,
place = {United States},
year = {2018},
month = {9}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record

Citation Metrics:
Cited by: 8 works
Citation information provided by
Web of Science

Save / Share:

Works referenced in this record:

Crack tip chemistry modelling of intergranular stress corrosion cracks in nickel containing segregated phosphorus and sulfur
journal, January 1991


On the relationship between grain boundary connectivity, coincident site lattice boundaries, and intergranular stress corrosion cracking
journal, October 2004


Evolution of nanoporosity in dealloying
journal, March 2001

  • Erlebacher, Jonah; Aziz, Michael J.; Karma, Alain
  • Nature, Vol. 410, Issue 6827, p. 450-453
  • DOI: 10.1038/35068529

Mechanical properties of bulk single crystalline nanoporous gold investigated by millimetre-scale tension and compression testing
journal, January 2014


Stress Corrosion Cracking and Localized Corrosion of Carbon Steel in Nitrate Solutions
journal, July 2016

  • Sridhar, N.; Beavers, J. A.; Rollins, B.
  • Corrosion, Vol. 72, Issue 7
  • DOI: 10.5006/2035

Film-Induced Cleavage of Ag-Au Alloys
journal, November 2008

  • Barnes, Andrew; Senior, Nicholas A.; Newman, Roger C.
  • Metallurgical and Materials Transactions A, Vol. 40, Issue 1
  • DOI: 10.1007/s11661-008-9714-z

Stress-corrosion cracking
journal, January 1987


Progress in the understanding of the long-term corrosion behaviour of copper canisters
journal, July 2013


Mechanical properties of nanoporous gold in tension
journal, May 2017


Modelling of environment assisted cracking
journal, June 1993


Probing the Dealloying Critical Potential
journal, January 2005

  • Dursun, Aziz; Pugh, Dylan V.; Corcoran, Sean G.
  • Journal of The Electrochemical Society, Vol. 152, Issue 2
  • DOI: 10.1149/1.1848351

Scaling laws of nanoporous metals under uniaxial compression
journal, April 2014


Stress corrosion cracking of Cu18%Au in 1N Na2SO4 - 0.01N H2SO4
journal, January 1988


Determination of the fate of the current in the stress corrosion cracking of sensitized type 304SS in high temperature aqueous systems
journal, January 1995


Case reviews on the effect of microstructure on the corrosion behavior of austenitic alloys for processing and storage of nuclear waste
journal, May 2005

  • Kain, V.; Sengupta, P.; De, P. K.
  • Metallurgical and Materials Transactions A, Vol. 36, Issue 5
  • DOI: 10.1007/s11661-005-0201-5

A revised interpretation of ultra-fast stress corrosion cracking experiments by Serebrinsky and Galvele
journal, April 2010


Electrochemical aspects of stress-corrosion cracking of sensitised stainless steels
journal, January 1983


Stress Corrosion Cracking of Candidate Material for Nuclear Waste Containers
journal, December 1990

  • Maiya, P. S.; Shack, W. J.; Kassner, T. F.
  • CORROSION, Vol. 46, Issue 12
  • DOI: 10.5006/1.3585051

Pattern formation during dealloying
journal, November 2003


Length scales in alloy dissolution and measurement of absolute interfacial free energy
journal, November 2006

  • Rugolo, J.; Erlebacher, J.; Sieradzki, K.
  • Nature Materials, Vol. 5, Issue 12
  • DOI: 10.1038/nmat1780

How oxidized grain boundaries fail
journal, August 2013


Observations of Intergranular Stress Corrosion Cracking in a Grain-Mapped Polycrystal
journal, July 2008


Potential-dependent dynamic fracture of nanoporous gold
journal, June 2015

  • Sun, Shaofeng; Chen, Xiying; Badwe, Nilesh
  • Nature Materials, Vol. 14, Issue 9
  • DOI: 10.1038/nmat4335

Applications of a versatile modelling approach to 3D atom probe simulations
journal, December 2015


Film-Induced Brittle Intergranular Cracking of Silver-Gold Alloys
journal, May 1996


Slow strain rate testing for monitoring cracking of mild steels for vessels and pipes for processing using caustic solutions
journal, May 2006

  • Saxena, A.; Raman, R. K. Singh; Muddle, B. C.
  • International Journal of Pressure Vessels and Piping, Vol. 83, Issue 5
  • DOI: 10.1016/j.ijpvp.2006.02.018

Deforming nanoporous metal: Role of lattice coherency
journal, May 2009


Intergranular and transgranular stress corrosion cracking of Cu30Au
journal, December 1993


Ductile-brittle transition in random porous Au
journal, February 1992


Environment-Assisted Intergranular Cracking
journal, July 1999


Mechanistic Aspects of Intergranular Stress Corrosion Cracking of Ferritic Steels
journal, May 1996


Brittle fracture of an Au/Ag alloy induced by a surface film
journal, February 1991

  • Kelly, R. G.; Frost, A. J.; Shahrabi, T.
  • Metallurgical Transactions A, Vol. 22, Issue 2
  • DOI: 10.1007/BF02656821

Effect of the strain rate on stress corrosion crack velocities in face-centred cubic alloys. A mechanistic interpretation
journal, March 2004


Life prediction by mechanistic modeling and system monitoring of environmental cracking of iron and nickel alloys in aqueous systems
journal, August 1988


A mechanistic study of SCC in Alloy 600 through high-resolution characterization
journal, March 2018


Testing the film-induced cleavage model of stress-corrosion cracking
journal, January 1993


The mechanism of intergranular stress corrosion cracking of sensitised austenitic stainless steel in dilute thiosulphate solution
journal, January 1992


High-resolution analytical electron microscopy characterization of corrosion and cracking at buried interfaces
journal, January 2001

  • Bruemmer, S. M.; Thomas, L. E.
  • Surface and Interface Analysis, Vol. 31, Issue 7
  • DOI: 10.1002/sia.1084

Progression markings, striations, and crack-arrest markings on fracture surfaces
journal, November 2007


    Works referencing / citing this record:

    Bi-continuous pattern formation in thin films via solid-state interfacial dealloying studied by multimodal characterization
    journal, January 2019

    • Zhao, Chonghang; Kisslinger, Kim; Huang, Xiaojing
    • Materials Horizons, Vol. 6, Issue 10
    • DOI: 10.1039/c9mh00669a

    Topology evolution during coarsening of nanoscale metal network structures
    journal, July 2019


    Bi-continuous pattern formation in thin films via solid-state interfacial dealloying studied by multimodal characterization
    journal, January 2019

    • Zhao, Chonghang; Kisslinger, Kim; Huang, Xiaojing
    • Materials Horizons, Vol. 6, Issue 10
    • DOI: 10.1039/c9mh00669a

    Topology evolution during coarsening of nanoscale metal network structures
    journal, July 2019