Title: Selective atomic layer deposition of RuO x catalysts on shape-controlled Pd nanocrystals with significantly enhanced hydrogen evolution activity

Abstract

Octahedral Pd@RuO x/NCNT catalysts are achieved through atomic layer deposition, and exhibit comparable activity with Pt/C for hydrogen evolution reaction.

Authors:
 [1];  [2];  [1];  [2];  [1];  [1];  [3];  [3];  [1];  [1]; ORCiD logo [2]; ORCiD logo [1]
  1. Department of Mechanical and Materials Engineering; The University of Western Ontario; London; Canada
  2. Key Laboratory for Green Chemical Technology of Ministry of Education; School of Chemical Engineering and Technology; Tianjin University; Collaborative Innovation Center of Chemical Science and Engineering (Tianjin); Tianjin 300072
  3. Department of Chemistry; University of Western Ontario; London; Canada
Publication Date:
Research Org.:
Argonne National Lab. (ANL), Argonne, IL (United States). Advanced Photon Source (APS)
Sponsoring Org.:
FOREIGN
OSTI Identifier:
1491869
Resource Type:
Journal Article
Journal Name:
Journal of Materials Chemistry. A
Additional Journal Information:
Journal Volume: 6; Journal Issue: 47; Journal ID: ISSN 2050-7488
Publisher:
Royal Society of Chemistry
Country of Publication:
United States
Language:
ENGLISH

Citation Formats

Zhang, Lei, Zhao, Zhi-Jian, Norouzi Banis, Mohammad, Li, Lulu, Zhao, Yang, Song, Zhongxin, Wang, Zhiqiang, Sham, Tsun-Kong, Li, Ruying, Zheng, Matthew, Gong, Jinlong, and Sun, Xueliang. Selective atomic layer deposition of RuOx catalysts on shape-controlled Pd nanocrystals with significantly enhanced hydrogen evolution activity. United States: N. p., 2018. Web. doi:10.1039/C8TA08931K.
Zhang, Lei, Zhao, Zhi-Jian, Norouzi Banis, Mohammad, Li, Lulu, Zhao, Yang, Song, Zhongxin, Wang, Zhiqiang, Sham, Tsun-Kong, Li, Ruying, Zheng, Matthew, Gong, Jinlong, & Sun, Xueliang. Selective atomic layer deposition of RuOx catalysts on shape-controlled Pd nanocrystals with significantly enhanced hydrogen evolution activity. United States. doi:10.1039/C8TA08931K.
Zhang, Lei, Zhao, Zhi-Jian, Norouzi Banis, Mohammad, Li, Lulu, Zhao, Yang, Song, Zhongxin, Wang, Zhiqiang, Sham, Tsun-Kong, Li, Ruying, Zheng, Matthew, Gong, Jinlong, and Sun, Xueliang. Mon . "Selective atomic layer deposition of RuOx catalysts on shape-controlled Pd nanocrystals with significantly enhanced hydrogen evolution activity". United States. doi:10.1039/C8TA08931K.
@article{osti_1491869,
title = {Selective atomic layer deposition of RuOx catalysts on shape-controlled Pd nanocrystals with significantly enhanced hydrogen evolution activity},
author = {Zhang, Lei and Zhao, Zhi-Jian and Norouzi Banis, Mohammad and Li, Lulu and Zhao, Yang and Song, Zhongxin and Wang, Zhiqiang and Sham, Tsun-Kong and Li, Ruying and Zheng, Matthew and Gong, Jinlong and Sun, Xueliang},
abstractNote = {Octahedral Pd@RuOx/NCNT catalysts are achieved through atomic layer deposition, and exhibit comparable activity with Pt/C for hydrogen evolution reaction.},
doi = {10.1039/C8TA08931K},
journal = {Journal of Materials Chemistry. A},
issn = {2050-7488},
number = 47,
volume = 6,
place = {United States},
year = {2018},
month = {1}
}