Abstract

The addition of aluminum oxide (Al 2O 3) as a sintering aid to yttria-stabilized zirconia (YSZ) reduces the required densification temperature. Sintering aids are incorporated using a number of processes which can lead to ambiguity when determining the effect of the sintering aid on the densification mechanism. In this study, a novel method for sintering aid addition, Particle Atomic Layer Deposition (ALD), was used to deposit an amorphous Al 2O 3 thin film on YSZ particles. Transmission electron microscopy confirmed the deposition of conformal Al 2O 3 thin films on the surface of the YSZ particles. The addition of Al 2O 3 to YSZ reduced the temperature at which densification began by ~75 degrees C, and 2.2 wt% Al 2O 3 addition resulted in a minimum activation energy for the intermediate stage of densification. This concentration is well in excess of the solubility limit of Al 2O 3 in YSZ, showing that Al 2O 3 does not enhance the densification of YSZ solely by dissolving into the YSZ lattice and activating volume diffusion. The addition of 0.7 wt% Al 2O 3 with one Particle ALD cycle enhanced the ionic conductivity of YSZ by 23% after sintering at 1350 degrees Cmore » for 2 hours, demonstrating that dense parts with high oxygen ion conductivities can be produced after sintering at reduced temperatures. One Particle ALD cycle is a fast, easily scaled-up process that eliminates the use of solvents and has substantial cost/performance advantages over conventional processing.« less

Authors:
ORCiD logo [1];  [1];  [1];  [1]; ORCiD logo [2];  [2];  [3];  [4]; ORCiD logo [1]
  1. Univ. of Colorado, Boulder, CO (United States)
  2. Colorado School of Mines, Golden, CO (United States)
  3. ALD NanoSolutions, Inc. Broomfield CO (United States)
  4. National Renewable Energy Lab. (NREL), Golden, CO (United States); Univ. of Colorado, Boulder, CO (United States)
Publication Date:
Research Org.:
National Renewable Energy Lab. (NREL), Golden, CO (United States)
Sponsoring Org.:
National Science Foundation (NSF); USDOE
OSTI Identifier:
1480237
Report Number(s):
NREL/JA-5K00-72691
Journal ID: ISSN 0002-7820
Grant/Contract Number:  
AC36-08GO28308
Resource Type:
Journal Article: Accepted Manuscript
Journal Name:
Journal of the American Ceramic Society
Additional Journal Information:
Journal Volume: 102; Journal Issue: 5; Journal ID: ISSN 0002-7820
Publisher:
American Ceramic Society
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; atomic layer deposition; sintering; thin films

Citation Formats

O'Toole, Rebecca J., Bartel, Christopher J., Kodas, Maila U., Horrell, Alexa J., Ricote, Sandrine, Sullivan, Neal P., Gump, Christopher J., Musgrave, Charles B., and Weimer, Alan W. Particle atomic layer deposition of alumina for sintering yttria-stabilized cubic zirconia. United States: N. p., 2018. Web. doi:10.1111/jace.16091.
O'Toole, Rebecca J., Bartel, Christopher J., Kodas, Maila U., Horrell, Alexa J., Ricote, Sandrine, Sullivan, Neal P., Gump, Christopher J., Musgrave, Charles B., & Weimer, Alan W. Particle atomic layer deposition of alumina for sintering yttria-stabilized cubic zirconia. United States. doi:10.1111/jace.16091.
O'Toole, Rebecca J., Bartel, Christopher J., Kodas, Maila U., Horrell, Alexa J., Ricote, Sandrine, Sullivan, Neal P., Gump, Christopher J., Musgrave, Charles B., and Weimer, Alan W. Wed . "Particle atomic layer deposition of alumina for sintering yttria-stabilized cubic zirconia". United States. doi:10.1111/jace.16091. https://www.osti.gov/servlets/purl/1480237.
@article{osti_1480237,
title = {Particle atomic layer deposition of alumina for sintering yttria-stabilized cubic zirconia},
author = {O'Toole, Rebecca J. and Bartel, Christopher J. and Kodas, Maila U. and Horrell, Alexa J. and Ricote, Sandrine and Sullivan, Neal P. and Gump, Christopher J. and Musgrave, Charles B. and Weimer, Alan W.},
abstractNote = {The addition of aluminum oxide (Al2O3) as a sintering aid to yttria-stabilized zirconia (YSZ) reduces the required densification temperature. Sintering aids are incorporated using a number of processes which can lead to ambiguity when determining the effect of the sintering aid on the densification mechanism. In this study, a novel method for sintering aid addition, Particle Atomic Layer Deposition (ALD), was used to deposit an amorphous Al2O3 thin film on YSZ particles. Transmission electron microscopy confirmed the deposition of conformal Al2O3 thin films on the surface of the YSZ particles. The addition of Al2O3 to YSZ reduced the temperature at which densification began by ~75 degrees C, and 2.2 wt% Al2O3 addition resulted in a minimum activation energy for the intermediate stage of densification. This concentration is well in excess of the solubility limit of Al2O3 in YSZ, showing that Al2O3 does not enhance the densification of YSZ solely by dissolving into the YSZ lattice and activating volume diffusion. The addition of 0.7 wt% Al2O3 with one Particle ALD cycle enhanced the ionic conductivity of YSZ by 23% after sintering at 1350 degrees C for 2 hours, demonstrating that dense parts with high oxygen ion conductivities can be produced after sintering at reduced temperatures. One Particle ALD cycle is a fast, easily scaled-up process that eliminates the use of solvents and has substantial cost/performance advantages over conventional processing.},
doi = {10.1111/jace.16091},
journal = {Journal of the American Ceramic Society},
issn = {0002-7820},
number = 5,
volume = 102,
place = {United States},
year = {2018},
month = {9}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record

Citation Metrics:
Cited by: 1 work
Citation information provided by
Web of Science

Figures / Tables:

FIGURE 1 FIGURE 1: (A) Al2O3 concentration for all ALD samples measured using ICP‐OES. (b) HRTEM of 9ALD and (C) EDS of 9ALD

Save / Share:

Works referenced in this record:

A brief review of the ionic conductivity enhancement for selected oxide electrolytes
journal, October 2007


Electrolysis of carbon dioxide in Solid Oxide Electrolysis Cells
journal, August 2009


Microstructural, mechanical and electrical properties of alumina-doped cubic zirconia (c-ZrO2)
journal, March 2008

  • Tekeli, S.; Kayış, A.; Gürü, M.
  • Journal of Solid State Electrochemistry, Vol. 12, Issue 7-8
  • DOI: 10.1007/s10008-008-0530-6

Atomic layer deposition on particles using a fluidized bed reactor with in situ mass spectrometry
journal, September 2007


Mechanical behavior of zirconia/alumina composites
journal, January 2005


Degradation of solid oxide cells during co-electrolysis of steam and carbon dioxide at high current densities
journal, October 2016


Initial Sintering with Constant Rates of Heating
journal, December 1970


Proton conduction in doped LaScO3 perovskites
journal, November 2004


Influence of α-Al2O3 addition on sintering and grain growth behaviour of 8 mol% Y2O3-stabilised cubic zirconia (c-ZrO2)
journal, January 2004


Mechanism of Alumina-Enhanced Sintering of Fine Zirconia Powder: Influence of Alumina Concentration on the Initial Stage Sintering
journal, June 2008


Effect of alumina additions upon electrical properties of 8 mol.% yttria-stabilised zirconia
journal, June 1999


Advances in solid oxide fuel cell technology
journal, November 2000


Catalyst Design with Atomic Layer Deposition
journal, February 2015

  • O’Neill, Brandon J.; Jackson, David H. K.; Lee, Jechan
  • ACS Catalysis, Vol. 5, Issue 3
  • DOI: 10.1021/cs501862h

Effect of alumina-doping on grain boundary segregation-induced phase transformation in yttria-stabilized tetragonal zirconia polycrystal
journal, September 2006

  • Matsui, Koji; Ohmichi, Nobukatsu; Ohgai, Michiharu
  • Journal of Materials Research, Vol. 21, Issue 09
  • DOI: 10.1557/jmr.2006.0274

Sintering densification curve: A practical approach for its construction from dilatometric shrinkage data
journal, January 2008

  • Maca, K.; Pouchly, V.; Boccaccini, A. R.
  • Science of Sintering, Vol. 40, Issue 2
  • DOI: 10.2298/SOS0802117M

Computer Simulation Studies on Sintering and Grain Growth
journal, January 2005

  • Matsubara, Hideaki
  • Journal of the Ceramic Society of Japan, Vol. 113, Issue 1316
  • DOI: 10.2109/jcersj.113.263

Effect of cation doping on lattice and grain boundary diffusion in superplastic yttria-stabilized tetragonal zirconia
journal, February 2010


Cubic-Formation and Grain-Growth Mechanisms in Tetragonal Zirconia Polycrystal
journal, August 2003


Alumina atomic layer deposition nanocoatings on primary diamond particles using a fluidized bed reactor
journal, February 2008


Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process
journal, June 2005

  • Puurunen, Riikka L.
  • Journal of Applied Physics, Vol. 97, Issue 12, Article No. 121301
  • DOI: 10.1063/1.1940727

Solid Solubility and Precipitation in a Single-Crystal Alumina-Zirconia System
journal, December 2002


Functionalization of fine particles using atomic and molecular layer deposition
journal, May 2012


Effects of doping alumina on the electrical and sintering performances of yttrium-stabilized-zirconia
journal, June 2016


Effect of alumina addition on initial sintering of cubic ZrO2 (8YSZ)
journal, April 2010


Colloidal processing, sintering and static grain growth behaviour of alumina-doped cubic zirconia
journal, January 2005


Atomic Layer Deposition: An Overview
journal, January 2010

  • George, Steven M.
  • Chemical Reviews, Vol. 110, Issue 1, p. 111-131
  • DOI: 10.1021/cr900056b

Roles of alumina in zirconia-based solid electrolyte
journal, February 1995

  • Guo, Xin; Yuan, Runzhang
  • Journal of Materials Science, Vol. 30, Issue 4
  • DOI: 10.1007/BF01178426

Effect of Alumina on Sintering Behavior and Electrical Conductivity of High-Purity Yttria-Stabilized Zirconia
journal, August 1994


Microstructural Analysis of Sintered High-Conductivity Zirconia with Al203 Additions
journal, October 1982


Estimate of the Activation Energies for Boundary Diffusion from Rate-Controlled Sintering of Pure Alumina, and Alumina Doped with Zirconia or Titania
journal, May 1990


The role of Al2O3 impurities on the microstructure and properties of Y-TZP
journal, August 1999


Enhanced superplasticity in a alumina-containing zirconia prepared by colloidal processing
journal, September 2000


Sintering mechanism of fine zirconia powders with alumina added by powder mixing and chemical processes
journal, February 2008

  • Matsui, Koji; Yamakawa, Takanori; Uehara, Masato
  • Journal of Materials Science, Vol. 43, Issue 8
  • DOI: 10.1007/s10853-008-2493-5

Effect of Pore Distribution on Microstructure Development: I, Matrix Pores
journal, February 1988


Average Grain Size in Polycrystalline Ceramics
journal, August 1969


Activation Energy for the Sintering of Two-Phase Alumina/Zirconia Ceramics
journal, August 1991


Emerging Applications of Atomic Layer Deposition for Lithium-Ion Battery Studies
journal, June 2012

  • Meng, Xiangbo; Yang, Xiao-Qing; Sun, Xueliang
  • Advanced Materials, Vol. 24, Issue 27
  • DOI: 10.1002/adma.201200397

Coating Fine Nickel Particles with Al 2 O 3 Utilizing an Atomic Layer Deposition-Fluidized Bed Reactor (ALD-FBR)
journal, April 2004


A computational study of yttria-stabilized zirconia: II. Cation diffusion
journal, March 2017


Sintering Kinetics at Constant Rates of Heating: Effect of Alumina on the Initial Sintering Stage of Yttria-Stabilized Cubic Zirconia Powder
journal, January 2006

  • Matsui, Koji; Tanaka, Kenji; Enomoto, Naoya
  • Journal of the Ceramic Society of Japan, Vol. 114, Issue 1333
  • DOI: 10.2109/jcersj.114.763

Improvement of Grain-Boundary Conductivity of 8 mol % Yttria-Stabilized Zirconia by Precursor Scavenging of Siliceous Phase
journal, January 2000

  • Lee, Jong-Heun; Mori, Toshiyuki; Li, Ji-Guang
  • Journal of The Electrochemical Society, Vol. 147, Issue 7
  • DOI: 10.1149/1.1393612

Sensors, Chemical Sensors, Electrochemical Sensors, and ECS
journal, January 2003

  • Stetter, Joseph R.; Penrose, William R.; Yao, Sheng
  • Journal of The Electrochemical Society, Vol. 150, Issue 2
  • DOI: 10.1149/1.1539051

Template-directed synthesis of porous alumina particles with precise wall thickness control via atomic layer deposition
journal, February 2012


    Figures/Tables have been extracted from DOE-funded journal article accepted manuscripts.