Title: SCC Initiation Behavior of Alloy 182 in PWR Primary Water

Abstract

SCC initiation behavior of 15% cold forged specimens cut from four different alloy 182 weldments was investigated in 360°C simulated PWR primary water under constant load at the yield stress using direct current potential drop to perform in-situ monitoring of SCC initiation time. Within each weldment, one or more specimens underwent SCC initiation within 24 hours of reaching full load while some specimens had much longer initiation times, in a few cases exceeding 2500 hours. Detailed examinations were conducted on these specimens with a focus on different microstructural features such as preexisting defects, grain orientation and second phases, highlighting an important role of microstructure in crack initiation of alloy 182.

Authors:
; ;
Publication Date:
Research Org.:
Pacific Northwest National Lab. (PNNL), Richland, WA (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
1440627
Report Number(s):
PNNL-SA-128211
453060031
DOE Contract Number:  
AC05-76RL01830
Resource Type:
Conference
Resource Relation:
Conference: Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors (EDM 2017), 1:137-160
Country of Publication:
United States
Language:
English
Subject:
SCC initiation; Alloy 182; PWR

Citation Formats

Toloczko, Mychailo B., Zhai, Ziqing, and Bruemmer, Stephen M. SCC Initiation Behavior of Alloy 182 in PWR Primary Water. United States: N. p., 2018. Web. doi:10.1007/978-3-319-67244-1_9.
Toloczko, Mychailo B., Zhai, Ziqing, & Bruemmer, Stephen M. SCC Initiation Behavior of Alloy 182 in PWR Primary Water. United States. doi:10.1007/978-3-319-67244-1_9.
Toloczko, Mychailo B., Zhai, Ziqing, and Bruemmer, Stephen M. Sun . "SCC Initiation Behavior of Alloy 182 in PWR Primary Water". United States. doi:10.1007/978-3-319-67244-1_9.
@article{osti_1440627,
title = {SCC Initiation Behavior of Alloy 182 in PWR Primary Water},
author = {Toloczko, Mychailo B. and Zhai, Ziqing and Bruemmer, Stephen M.},
abstractNote = {SCC initiation behavior of 15% cold forged specimens cut from four different alloy 182 weldments was investigated in 360°C simulated PWR primary water under constant load at the yield stress using direct current potential drop to perform in-situ monitoring of SCC initiation time. Within each weldment, one or more specimens underwent SCC initiation within 24 hours of reaching full load while some specimens had much longer initiation times, in a few cases exceeding 2500 hours. Detailed examinations were conducted on these specimens with a focus on different microstructural features such as preexisting defects, grain orientation and second phases, highlighting an important role of microstructure in crack initiation of alloy 182.},
doi = {10.1007/978-3-319-67244-1_9},
journal = {},
number = ,
volume = ,
place = {United States},
year = {2018},
month = {10}
}

Conference:
Other availability
Please see Document Availability for additional information on obtaining the full-text document. Library patrons may search WorldCat to identify libraries that hold this conference proceeding.

Save / Share: