Title: Microscopic Examination of the Corroded Hagan Container Used to Store Molten Salt Extraction Residue XBPS333

Technical Report ·
DOI:https://doi.org/10.2172/1418773· OSTI ID:1418773

A microscopic examination was performed on a Hagan container after corrosion and a white powder were found on the outside surface of the lid and filter cover while in storage in the vault. The inside surfaces of the container were covered by a wipeable brown coating. The coating was removed and portions of the container were sectioned and imaged with optical microscopy. General corrosion was found throughout the inside of the container, and pitting corrosion was observed in several locations on the lid and sidewall. This report describes the type and extent of the corrosion observed and its impact on the storage lifetime of the container.

Research Organization:
Los Alamos National Laboratory (LANL), Los Alamos, NM (United States)
Sponsoring Organization:
USDOE National Nuclear Security Administration (NNSA), Office of Defense Programs (DP)
DOE Contract Number:
AC52-06NA25396
OSTI ID:
1418773
Report Number(s):
LA-UR-17-28355
Country of Publication:
United States