Title: Characterizing the Effects of Thermal Processing on Microstructure in Paliney-7 Using Nanoindentation and Electron Microscopy.

Abstract

Abstract not provided.

Authors:
Publication Date:
Research Org.:
Sandia National Lab. (SNL-NM), Albuquerque, NM (United States)
Sponsoring Org.:
USDOE National Nuclear Security Administration (NNSA)
OSTI Identifier:
1399199
Report Number(s):
SAND2016-9955C
648012
DOE Contract Number:
AC04-94AL85000
Resource Type:
Conference
Resource Relation:
Conference: Proposed for presentation at the Rio Grande Symposium on Advanced Materials held October 3, 2016 in Albuquerque, NM, United States of America.
Country of Publication:
United States
Language:
English

Citation Formats

Finfrock, Christopher. Characterizing the Effects of Thermal Processing on Microstructure in Paliney-7 Using Nanoindentation and Electron Microscopy.. United States: N. p., 2016. Web.
Finfrock, Christopher. Characterizing the Effects of Thermal Processing on Microstructure in Paliney-7 Using Nanoindentation and Electron Microscopy.. United States.
Finfrock, Christopher. 2016. "Characterizing the Effects of Thermal Processing on Microstructure in Paliney-7 Using Nanoindentation and Electron Microscopy.". United States. doi:. https://www.osti.gov/servlets/purl/1399199.
@article{osti_1399199,
title = {Characterizing the Effects of Thermal Processing on Microstructure in Paliney-7 Using Nanoindentation and Electron Microscopy.},
author = {Finfrock, Christopher},
abstractNote = {Abstract not provided.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = 2016,
month =
}

Conference:
Other availability
Please see Document Availability for additional information on obtaining the full-text document. Library patrons may search WorldCat to identify libraries that hold this conference proceeding.

Save / Share: