Title: Size effect of the active sites in UiO-66-supported nickel catalysts synthesized via atomic layer deposition for ethylene hydrogenation

Abstract

Ni(ii) ions have been deposited on the Zr 6nodes of a metal–organic framework (MOF), UiO-66,viaan ALD-like process (ALD = atomic layer deposition).

Authors:
ORCiD logo [1];  [1]; ORCiD logo [1]; ORCiD logo [1];  [2];  [1];  [3]
  1. Department of Chemistry; Northwestern University; Evanston; USA
  2. Department of Chemical and Biological Engineering; Northwestern University; Evanston; USA
  3. Department of Chemistry; Northwestern University; Evanston; USA; Department of Chemistry
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Energy Frontier Research Center for Inorganometallic Catalyst Design (ICDC)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
OSTI Identifier:
1388267
DOE Contract Number:  
SC0012702
Resource Type:
Journal Article
Journal Name:
Inorganic Chemistry Frontiers (Online)
Additional Journal Information:
Journal Volume: 4; Journal Issue: 5; Related Information: ICDC partners with University of Minnesota(lead); Argonne National Laboratory; Clemson University; Dow Chemical Company; Northwestern University; Pacific Northwest National Laboratory; University of California Davis; University of Washington; Journal ID: ISSN 2052-1553
Publisher:
Royal Society of Chemistry
Country of Publication:
United States
Language:
English
Subject:
catalysis (heterogeneous), materials and chemistry by design, synthesis (novel materials)

Citation Formats

Li, Zhanyong, Peters, Aaron W., Liu, Jian, Zhang, Xuan, Schweitzer, Neil M., Hupp, Joseph T., and Farha, Omar K. Size effect of the active sites in UiO-66-supported nickel catalysts synthesized via atomic layer deposition for ethylene hydrogenation. United States: N. p., 2017. Web. doi:10.1039/c7qi00056a.
Li, Zhanyong, Peters, Aaron W., Liu, Jian, Zhang, Xuan, Schweitzer, Neil M., Hupp, Joseph T., & Farha, Omar K. Size effect of the active sites in UiO-66-supported nickel catalysts synthesized via atomic layer deposition for ethylene hydrogenation. United States. doi:10.1039/c7qi00056a.
Li, Zhanyong, Peters, Aaron W., Liu, Jian, Zhang, Xuan, Schweitzer, Neil M., Hupp, Joseph T., and Farha, Omar K. Sun . "Size effect of the active sites in UiO-66-supported nickel catalysts synthesized via atomic layer deposition for ethylene hydrogenation". United States. doi:10.1039/c7qi00056a.
@article{osti_1388267,
title = {Size effect of the active sites in UiO-66-supported nickel catalysts synthesized via atomic layer deposition for ethylene hydrogenation},
author = {Li, Zhanyong and Peters, Aaron W. and Liu, Jian and Zhang, Xuan and Schweitzer, Neil M. and Hupp, Joseph T. and Farha, Omar K.},
abstractNote = {Ni(ii) ions have been deposited on the Zr6nodes of a metal–organic framework (MOF), UiO-66,viaan ALD-like process (ALD = atomic layer deposition).},
doi = {10.1039/c7qi00056a},
journal = {Inorganic Chemistry Frontiers (Online)},
issn = {2052-1553},
number = 5,
volume = 4,
place = {United States},
year = {2017},
month = {1}
}

Works referenced in this record:

Sintering-Resistant Single-Site Nickel Catalyst Supported by Metal–Organic Framework
journal, February 2016

  • Li, Zhanyong; Schweitzer, Neil M.; League, Aaron B.
  • Journal of the American Chemical Society, Vol. 138, Issue 6
  • DOI: 10.1021/jacs.5b12515

Structural Transitions of the Metal-Oxide Nodes within Metal–Organic Frameworks: On the Local Structures of NU-1000 and UiO-66
journal, March 2016

  • Platero-Prats, Ana E.; Mavrandonakis, Andreas; Gallington, Leighanne C.
  • Journal of the American Chemical Society, Vol. 138, Issue 12
  • DOI: 10.1021/jacs.6b00069

Synthesis, Structure, and Metalation of Two New Highly Porous Zirconium Metal–Organic Frameworks
journal, June 2012

  • Morris, William; Volosskiy, Boris; Demir, Selcuk
  • Inorganic Chemistry, Vol. 51, Issue 12, p. 6443-6445
  • DOI: 10.1021/ic300825s

Toward Inexpensive Photocatalytic Hydrogen Evolution: A Nickel Sulfide Catalyst Supported on a High-Stability Metal–Organic Framework
journal, August 2016

  • Peters, Aaron W.; Li, Zhanyong; Farha, Omar K.
  • ACS Applied Materials & Interfaces, Vol. 8, Issue 32
  • DOI: 10.1021/acsami.6b04729

Metal–Organic Framework Thin Films as Platforms for Atomic Layer Deposition of Cobalt Ions To Enable Electrocatalytic Water Oxidation
journal, December 2015

  • Kung, Chung-Wei; Mondloch, Joseph E.; Wang, Timothy C.
  • ACS Applied Materials & Interfaces, Vol. 7, Issue 51
  • DOI: 10.1021/acsami.5b06901

Metal–Organic Framework Supported Cobalt Catalysts for the Oxidative Dehydrogenation of Propane at Low Temperature
journal, November 2016


Critical Literature Review of the Kinetics for the Oxidative Dehydrogenation of Propane over Well-Defined Supported Vanadium Oxide Catalysts
journal, September 2014

  • Carrero, C. A.; Schloegl, R.; Wachs, I. E.
  • ACS Catalysis, Vol. 4, Issue 10
  • DOI: 10.1021/cs5003417

Metal–Organic Framework Nodes as Nearly Ideal Supports for Molecular Catalysts: NU-1000- and UiO-66-Supported Iridium Complexes
journal, June 2015

  • Yang, Dong; Odoh, Samuel O.; Wang, Timothy C.
  • Journal of the American Chemical Society, Vol. 137, Issue 23, p. 7391-7396
  • DOI: 10.1021/jacs.5b02956

Comparative study of titanium-functionalized UiO-66: support effect on the oxidation of cyclohexene using hydrogen peroxide
journal, January 2015

  • Nguyen, Huong Giang T.; Mao, Lily; Peters, Aaron W.
  • Catalysis Science & Technology, Vol. 5, Issue 9
  • DOI: 10.1039/C5CY00825E

Stable Metal–Organic Framework-Supported Niobium Catalysts
journal, October 2016


Computationally Guided Discovery of a Catalytic Cobalt-Decorated Metal–Organic Framework for Ethylene Dimerization
journal, October 2016

  • Bernales, Varinia; League, Aaron B.; Li, Zhanyong
  • The Journal of Physical Chemistry C, Vol. 120, Issue 41
  • DOI: 10.1021/acs.jpcc.6b07362

Gold Atoms Stabilized on Various Supports Catalyze the Water–Gas Shift Reaction
journal, November 2013

  • Flytzani-Stephanopoulos, Maria
  • Accounts of Chemical Research, Vol. 47, Issue 3
  • DOI: 10.1021/ar4001845

Regioselective Atomic Layer Deposition in Metal–Organic Frameworks Directed by Dispersion Interactions
journal, October 2016

  • Gallington, Leighanne C.; Kim, In Soo; Liu, Wei-Guang
  • Journal of the American Chemical Society, Vol. 138, Issue 41
  • DOI: 10.1021/jacs.6b08711

Unusual and Highly Tunable Missing-Linker Defects in Zirconium Metal–Organic Framework UiO-66 and Their Important Effects on Gas Adsorption
journal, May 2013

  • Wu, Hui; Chua, Yong Shen; Krungleviciute, Vaiva
  • Journal of the American Chemical Society, Vol. 135, Issue 28
  • DOI: 10.1021/ja404514r

Synthesis and Stabilization of Supported Metal Catalysts by Atomic Layer Deposition
journal, March 2013

  • Lu, Junling; Elam, Jeffrey W.; Stair, Peter C.
  • Accounts of Chemical Research, Vol. 46, Issue 8
  • DOI: 10.1021/ar300229c

Defining the Proton Topology of the Zr6-Based Metal–Organic Framework NU-1000
journal, October 2014

  • Planas, Nora; Mondloch, Joseph E.; Tussupbayev, Samat
  • The Journal of Physical Chemistry Letters, Vol. 5, Issue 21, p. 3716-3723
  • DOI: 10.1021/jz501899j

Vanadium-Node-Functionalized UiO-66: A Thermally Stable MOF-Supported Catalyst for the Gas-Phase Oxidative Dehydrogenation of Cyclohexene
journal, June 2014

  • Nguyen, Huong Giang T.; Schweitzer, Neil M.; Chang, Chih-Yi
  • ACS Catalysis, Vol. 4, Issue 8, p. 2496-2500
  • DOI: 10.1021/cs5001448

Effect of Pd Nanoparticle Size on the Catalytic Hydrogenation of Allyl Alcohol
journal, April 2006

  • Wilson, Orla M.; Knecht, Marc R.; Garcia-Martinez, Joaquin C.
  • Journal of the American Chemical Society, Vol. 128, Issue 14, p. 4510-4511
  • DOI: 10.1021/ja058217m

Functionalization of UiO-66 Metal−Organic Framework and Highly Cross-Linked Polystyrene with Cr(CO) 3 : In Situ Formation, Stability, and Photoreactivity
journal, August 2010

  • Chavan, Sachin; Vitillo, Jenny G.; Uddin, Mohammed J.
  • Chemistry of Materials, Vol. 22, Issue 16
  • DOI: 10.1021/cm1005899

Vapor-Phase Metalation by Atomic Layer Deposition in a Metal–Organic Framework
journal, May 2013

  • Mondloch, Joseph E.; Bury, Wojciech; Fairen-Jimenez, David
  • Journal of the American Chemical Society, Vol. 135, Issue 28, p. 10294-10297
  • DOI: 10.1021/ja4050828

Cooperative Cluster Metalation and Ligand Migration in Zirconium Metal-Organic Frameworks
journal, October 2015

  • Yuan, Shuai; Chen, Ying-Pin; Qin, Junsheng
  • Angewandte Chemie International Edition, Vol. 54, Issue 49
  • DOI: 10.1002/anie.201505625

Atomic layer deposition of metal and nitride thin films: Current research efforts and applications for semiconductor device processing
journal, January 2003

  • Kim, H.
  • Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures, Vol. 21, Issue 6
  • DOI: 10.1116/1.1622676

Synthetic Access to Atomically Dispersed Metals in Metal–Organic Frameworks via a Combined Atomic-Layer-Deposition-in-MOF and Metal-Exchange Approach
journal, February 2016


Zr-based metal–organic frameworks: design, synthesis, structure, and applications
journal, January 2016

  • Bai, Yan; Dou, Yibo; Xie, Lin-Hua
  • Chemical Society Reviews, Vol. 45, Issue 8
  • DOI: 10.1039/C5CS00837A

Metals@MOFs - Loading MOFs with Metal Nanoparticles for Hybrid Functions
journal, July 2010

  • Meilikhov, Mikhail; Yusenko, Kirill; Esken, Daniel
  • European Journal of Inorganic Chemistry, Vol. 2010, Issue 24, p. 3701-3714
  • DOI: 10.1002/ejic.201000473

A facile synthesis of UiO-66, UiO-67 and their derivatives
journal, January 2013

  • Katz, Michael J.; Brown, Zachary J.; Colón, Yamil J.
  • Chemical Communications, Vol. 49, Issue 82
  • DOI: 10.1039/c3cc46105j

Catalyst Design with Atomic Layer Deposition
journal, February 2015

  • O’Neill, Brandon J.; Jackson, David H. K.; Lee, Jechan
  • ACS Catalysis, Vol. 5, Issue 3
  • DOI: 10.1021/cs501862h

Atomic Layer Deposition of Nanostructured Materials for Energy and Environmental Applications
journal, January 2012

  • Marichy, Catherine; Bechelany, Mikhael; Pinna, Nicola
  • Advanced Materials, Vol. 24, Issue 8, p. 1017-1032
  • DOI: 10.1002/adma.201104129

Postsynthetic Modification of Zirconium Metal-Organic Frameworks: Postsynthetic Modification of Zirconium Metal-Organic Frameworks
journal, July 2016

  • Marshall, Ross J.; Forgan, Ross S.
  • European Journal of Inorganic Chemistry, Vol. 2016, Issue 27
  • DOI: 10.1002/ejic.201600394

Water Adsorption in Porous Metal–Organic Frameworks and Related Materials
journal, March 2014

  • Furukawa, Hiroyasu; Gándara, Felipe; Zhang, Yue-Biao
  • Journal of the American Chemical Society, Vol. 136, Issue 11, p. 4369-4381
  • DOI: 10.1021/ja500330a

Synthesis, microstructures and UV–vis absorption properties of β-Ni(OH)2 nanoplates and NiO nanostructures
journal, August 2008


Chemical, thermal and mechanical stabilities of metal–organic frameworks
journal, February 2016


Single-Site Cobalt Catalysts at New Zr 82 -O) 82 -OH) 4 Metal-Organic Framework Nodes for Highly Active Hydrogenation of Alkenes, Imines, Carbonyls, and Heterocycles
journal, September 2016

  • Ji, Pengfei; Manna, Kuntal; Lin, Zekai
  • Journal of the American Chemical Society, Vol. 138, Issue 37
  • DOI: 10.1021/jacs.6b06759

An Exceptionally Stable Metal–Organic Framework Supported Molybdenum(VI) Oxide Catalyst for Cyclohexene Epoxidation
journal, October 2016

  • Noh, Hyunho; Cui, Yuexing; Peters, Aaron W.
  • Journal of the American Chemical Society, Vol. 138, Issue 44
  • DOI: 10.1021/jacs.6b08898

A New Zirconium Inorganic Building Brick Forming Metal Organic Frameworks with Exceptional Stability
journal, October 2008

  • Cavka, Jasmina Hafizovic; Jakobsen, Søren; Olsbye, Unni
  • Journal of the American Chemical Society, Vol. 130, Issue 42, p. 13850-13851
  • DOI: 10.1021/ja8057953

Atomic Layer Deposition: An Overview
journal, January 2010

  • George, Steven M.
  • Chemical Reviews, Vol. 110, Issue 1, p. 111-131
  • DOI: 10.1021/cr900056b

Atomic Layer Deposition of Metal Sulfide Materials
journal, January 2015

  • Dasgupta, Neil P.; Meng, Xiangbo; Elam, Jeffrey W.
  • Accounts of Chemical Research, Vol. 48, Issue 2, p. 341-348
  • DOI: 10.1021/ar500360d

Targeted Single-Site MOF Node Modification: Trivalent Metal Loading via Atomic Layer Deposition
journal, June 2015


Hydrogenation of benzene and toluene over size controlled Pt/SBA-15 catalysts: Elucidation of the Pt particle size effect on reaction kinetics
journal, August 2012


Direct Imaging of ALD Deposited Pt Nanoclusters inside the Giant Pores of MIL-101
journal, February 2016

  • Meledina, Maria; Turner, Stuart; Filippousi, Maria
  • Particle & Particle Systems Characterization, Vol. 33, Issue 7
  • DOI: 10.1002/ppsc.201500252

Supported Metal Clusters: Synthesis, Structure, and Catalysis
journal, May 1995


Adsorption and Diffusion of Light Hydrocarbons in UiO-66(Zr): A Combination of Experimental and Modeling Tools
journal, November 2014

  • Ramsahye, N. A.; Gao, J.; Jobic, H.
  • The Journal of Physical Chemistry C, Vol. 118, Issue 47
  • DOI: 10.1021/jp509672c

A brief review of atomic layer deposition: from fundamentals to applications
journal, June 2014


The Chemistry and Applications of Metal-Organic Frameworks
journal, August 2013

  • Furukawa, H.; Cordova, K. E.; O'Keeffe, M.
  • Science, Vol. 341, Issue 6149, p. 1230444-1230444
  • DOI: 10.1126/science.1230444

Single-Site Organozirconium Catalyst Embedded in a Metal–Organic Framework
journal, December 2015

  • Klet, Rachel C.; Tussupbayev, Samat; Borycz, Joshua
  • Journal of the American Chemical Society, Vol. 137, Issue 50
  • DOI: 10.1021/jacs.5b11350

Structure sensitivity: Hydrogenolysis of n-butane and hydrogenation of ethylene on nickel clusters condensed onto amorphous silica
journal, April 1988


Zirconium-Metalloporphyrin PCN-222: Mesoporous Metal-Organic Frameworks with Ultrahigh Stability as Biomimetic Catalysts
journal, August 2012

  • Feng, Dawei; Gu, Zhi-Yuan; Li, Jian-Rong
  • Angewandte Chemie International Edition, Vol. 51, Issue 41
  • DOI: 10.1002/anie.201204475