Title: Atomic Layer Deposition of MnS: Phase Control and Electrochemical Applications

Authors:
 [1];  [1];  [2];  [3];  [2];  [3];  [2];  [3]
  1. Department of Chemistry, University of Wisconsin−Stevens Point, Stevens Point, Wisconsin 54481, United States
  2. Energy Systems Division, Argonne National Laboratory, Argonne, Illinois 60439, United States
  3. Materials Science Division, Argonne National Laboratory, Argonne, Illinois 60439, United States
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Center for Electrical Energy Storage (CEES)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22); USDOE Office of Science (SC), Workforce Development for Teachers and Scientists (WDTS) (SC-27)
OSTI Identifier:
1387806
DOE Contract Number:  
AC02-06CH11357
Resource Type:
Journal Article
Journal Name:
ACS Applied Materials and Interfaces
Additional Journal Information:
Journal Volume: 8; Journal Issue: 4; Related Information: CEES partners with Argonne National Laboratory (lead); University of Illinois, Urbana-Champaign; Northwest University; Journal ID: ISSN 1944-8244
Publisher:
American Chemical Society (ACS)
Country of Publication:
United States
Language:
English
Subject:
energy storage (including batteries and capacitors), charge transport, materials and chemistry by design, synthesis (novel materials)

Citation Formats

Riha, Shannon C., Koegel, Alexandra A., Meng, Xiangbo, Kim, In Soo, Cao, Yanqiang, Pellin, Michael J., Elam, Jeffrey W., and Martinson, Alex B. F. Atomic Layer Deposition of MnS: Phase Control and Electrochemical Applications. United States: N. p., 2016. Web. doi:10.1021/acsami.5b11075.
Riha, Shannon C., Koegel, Alexandra A., Meng, Xiangbo, Kim, In Soo, Cao, Yanqiang, Pellin, Michael J., Elam, Jeffrey W., & Martinson, Alex B. F. Atomic Layer Deposition of MnS: Phase Control and Electrochemical Applications. United States. doi:10.1021/acsami.5b11075.
Riha, Shannon C., Koegel, Alexandra A., Meng, Xiangbo, Kim, In Soo, Cao, Yanqiang, Pellin, Michael J., Elam, Jeffrey W., and Martinson, Alex B. F. Tue . "Atomic Layer Deposition of MnS: Phase Control and Electrochemical Applications". United States. doi:10.1021/acsami.5b11075.
@article{osti_1387806,
title = {Atomic Layer Deposition of MnS: Phase Control and Electrochemical Applications},
author = {Riha, Shannon C. and Koegel, Alexandra A. and Meng, Xiangbo and Kim, In Soo and Cao, Yanqiang and Pellin, Michael J. and Elam, Jeffrey W. and Martinson, Alex B. F.},
abstractNote = {},
doi = {10.1021/acsami.5b11075},
journal = {ACS Applied Materials and Interfaces},
issn = {1944-8244},
number = 4,
volume = 8,
place = {United States},
year = {2016},
month = {1}
}

Works referencing / citing this record:

An aminopyridinato Mn( ii ) compound as a novel CVD precursor for manganese-containing films
journal, January 2018

  • Du, Liyong; Yu, Shaoshan; Liu, Xinfang
  • New Journal of Chemistry, Vol. 42, Issue 6
  • DOI: 10.1039/c8nj00062j