Title: Synthesis, characterization, and water oxidation by a molecular chromophore-catalyst assembly prepared by atomic layer deposition. The “mummy” strategy

Abstract

A Ru(ii)-polypyridyl chromophore-catalyst assembly for light-assisted water oxidation is constructed using atomic layer deposition with no covalent bonds between molecules required for bilayer formation.

Authors:
 [1];  [1];  [1];  [1];  [1];  [1];  [1]
  1. Department of Chemistry; University of North Carolina at Chapel Hill; Chapel Hill; USA
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Center for Solar Fuels (UNC EFRC)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
OSTI Identifier:
1387088
DOE Contract Number:  
SC0001011
Resource Type:
Journal Article
Journal Name:
Chemical Science
Additional Journal Information:
Journal Volume: 6; Journal Issue: 11; Related Information: UNC partners with University of North Carolina (lead); Duke University; University of Florida; Georgia Institute of Technology; University; North Carolina Central University; Research Triangle Institute; Journal ID: ISSN 2041-6520
Publisher:
Royal Society of Chemistry
Country of Publication:
United States
Language:
English
Subject:
catalysis (homogeneous), catalysis (heterogeneous), solar (photovoltaic), solar (fuels), photosynthesis (natural and artificial), hydrogen and fuel cells, electrodes - solar, charge transport, materials and chemistry by design, synthesis (novel materials), synthesis (self-assembly)

Citation Formats

Lapides, A. M., Sherman, B. D., Brennaman, M. K., Dares, C. J., Skinner, K. R., Templeton, J. L., and Meyer, T. J. Synthesis, characterization, and water oxidation by a molecular chromophore-catalyst assembly prepared by atomic layer deposition. The “mummy” strategy. United States: N. p., 2015. Web. doi:10.1039/C5SC01752A.
Lapides, A. M., Sherman, B. D., Brennaman, M. K., Dares, C. J., Skinner, K. R., Templeton, J. L., & Meyer, T. J. Synthesis, characterization, and water oxidation by a molecular chromophore-catalyst assembly prepared by atomic layer deposition. The “mummy” strategy. United States. doi:10.1039/C5SC01752A.
Lapides, A. M., Sherman, B. D., Brennaman, M. K., Dares, C. J., Skinner, K. R., Templeton, J. L., and Meyer, T. J. Thu . "Synthesis, characterization, and water oxidation by a molecular chromophore-catalyst assembly prepared by atomic layer deposition. The “mummy” strategy". United States. doi:10.1039/C5SC01752A.
@article{osti_1387088,
title = {Synthesis, characterization, and water oxidation by a molecular chromophore-catalyst assembly prepared by atomic layer deposition. The “mummy” strategy},
author = {Lapides, A. M. and Sherman, B. D. and Brennaman, M. K. and Dares, C. J. and Skinner, K. R. and Templeton, J. L. and Meyer, T. J.},
abstractNote = {A Ru(ii)-polypyridyl chromophore-catalyst assembly for light-assisted water oxidation is constructed using atomic layer deposition with no covalent bonds between molecules required for bilayer formation.},
doi = {10.1039/C5SC01752A},
journal = {Chemical Science},
issn = {2041-6520},
number = 11,
volume = 6,
place = {United States},
year = {2015},
month = {1}
}