Title: Atomic Layer Deposition of Metastable β-Fe 2 O 3 via Isomorphic Epitaxy for Photoassisted Water Oxidation

Journal Article · · ACS Applied Materials and Interfaces
DOI:https://doi.org/10.1021/am507065y· OSTI ID:1386535
; ;  [1]; ;  [1];
  1. Department of Materials Science and Engineering, Northwestern University, 2220 Campus Drive, Evanston, Illinois 60208, United States

Research Organization:
Energy Frontier Research Centers (EFRC) (United States). Argonne-Northwestern Solar Energy Research Center (ANSER)
Sponsoring Organization:
USDOE Office of Science (SC), Basic Energy Sciences (BES)
DOE Contract Number:
SC0001059
OSTI ID:
1386535
Journal Information:
ACS Applied Materials and Interfaces, Vol. 6, Issue 24; Related Information: ANSER partners with Northwestern University (lead); Argonne National Laboratory; University of Chicago; University of Illinois, Urbana-Champaign; Yale University; ISSN 1944-8244
Publisher:
American Chemical Society (ACS)
Country of Publication:
United States
Language:
English

References (51)

The stabilization of metastable phases by epitaxy journal January 1983
Epitaxial Stabilization of Oxides in Thin Films journal October 2002
A Thin Film Approach to Engineering Functionality into Oxides journal August 2008
Epitaxial stabilization and structural properties of REMnO3 (RE=Dy,Gd,Sm) compounds in a layered, hexagonal ABO3 structure journal December 2007
Preparation of crystalline beta barium borate (β‐BaB 2 O 4 ) thin films by pulsed laser deposition journal July 1995
Epitaxial growth and properties of metastable BiMnO3 thin films journal January 2004
Atomic layer deposition (ALD): from precursors to thin film structures journal April 2002
Atomic Layer Deposition: An Overview journal January 2010
Crystallinity of inorganic films grown by atomic layer deposition: Overview and general trends journal January 2013
Powering the planet: Chemical challenges in solar energy utilization journal October 2006
Inorganic Materials as Catalysts for Photochemical Splitting of Water journal January 2008
Solar Water Splitting Cells journal November 2010
Research Update: Strategies for efficient photoelectrochemical water splitting using metal oxide photoanodes journal January 2014
Solar Water Splitting: Progress Using Hematite (α-Fe2O3) Photoelectrodes journal March 2011
Toward solar fuels: Water splitting with sunlight and “rust”? journal November 2012
Structural disorder and anomalous diffusion in random packing of spheres journal September 2013
Beta-Fe2O3?eine neue Eisen(III)oxyd-Struktur journal January 1958
Crystal Structure of β-Fe 2 O 3 and Topotactic Phase Transformation to α-Fe 2 O 3 journal January 2013
First Observation of Phase Transformation of All Four Fe 2 O 3 Phases (γ → ε → β → α-Phase) journal December 2009
β   Fe2 O 3: Preparation of Thin Films by Chemical Vapor Deposition from Organometallic Chelates and Their Characterization journal March 1977
β-Fe 2 O 3 nanomaterials from an iron( ii ) diketonate-diamine complex: a study from molecular precursor to growth process journal January 2012
Effect of the substrate on the growth of spinel iron oxide thin films by metal-organic chemical vapor deposition journal February 1997
Electrochromic Properties of Iron Oxide Thin Films Prepared by Chemical Vapor Deposition journal May 1996
Thermally Induced Solid-State Syntheses of γ-Fe2O3 Nanoparticles and Their Transformation to α-Fe2O3 via ε-Fe2O3 journal March 2002
Characterization and applications of as-grown β-Fe2O3 nanoparticles prepared by hydrothermal method journal March 2011
Controlled synthesis and properties of β-Fe2O3 nanosystems functionalized with Ag or Pt nanoparticles journal January 2012
Enhanced Hydrogen Production by Photoreforming of Renewable Oxygenates Through Nanostructured Fe 2 O 3 Polymorphs journal September 2013
Iron(III) Oxides from Thermal ProcessesSynthesis, Structural and Magnetic Properties, Mössbauer Spectroscopy Characterization, and Applications journal March 2002
An analysis of the optimal band gaps of light absorbers in integrated tandem photoelectrochemical water-splitting systems journal January 2013
2-Photon tandem device for water splitting: comparing photocathode first versus photoanode first designs journal January 2014
Influence of Si dopant and SnO2 interfacial layer on the structure of the spray-deposited Fe2O3 films journal September 2009
Photoelectrochemical cells for solar hydrogen production: current state of promising photoelectrodes, methods to improve their properties, and outlook journal January 2013
Photoelectrochemical Characterization of Sprayed α - Fe 2 O 3 Thin Films: Influence of Si Doping and SnO 2 Interfacial Layer journal January 2008
Controlling Photoactivity in Ultrathin Hematite Films for Solar Water-Splitting journal March 2010
A Ga 2 O 3 underlayer as an isomorphic template for ultrathin hematite films toward efficient photoelectrochemical water splitting journal January 2012
Enhancement in the Performance of Ultrathin Hematite Photoanode for Water Splitting by an Oxide Underlayer journal April 2012
Substrate Dependent Water Splitting with Ultrathin α-Fe 2 O 3 Electrodes journal May 2014
Atomic Layer Deposition of Indium Tin Oxide Thin Films Using Nonhalogenated Precursors journal February 2008
Atomic Layer Deposition of Fe2O3 Using Ferrocene and Ozone
  • Martinson, Alex B. F.; DeVries, Michael J.; Libera, Joseph A.
  • The Journal of Physical Chemistry C, Vol. 115, Issue 10, p. 4333-4339 https://doi.org/10.1021/jp110203x
journal February 2011
Three dimensional reciprocal space measurement by x-ray diffraction using linear and area detectors: Applications to texture and defects determination in oriented thin films and nanoprecipitates
  • Gaudet, Simon; De Keyser, Koen; Lambert-Milot, Samuel
  • Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Vol. 31, Issue 2 https://doi.org/10.1116/1.4789984
journal March 2013
Fast pole figure acquisition using area detectors at the DiffAbs beamline – Synchrotron SOLEIL journal November 2013
Impact of structural features on pigment properties of α-Fe2O3 haematite journal October 2008
Photoelectrochemical Investigation of Ultrathin Film Iron Oxide Solar Cells Prepared by Atomic Layer Deposition journal January 2011
Identifying champion nanostructures for solar water-splitting journal July 2013
The Photoelectrochemical Behavior of Ferric Oxide in the Presence of Redox Reagents journal January 1981
Probing the photoelectrochemical properties of hematite (α-Fe 2 O 3 ) electrodes using hydrogen peroxide as a hole scavenger journal January 2011
Enhanced photoanode properties of epitaxial Ti doped α-Fe 2 O 3 (0001) thin films journal September 2012
Single Crystalline Hematite Films for Solar Water Splitting: Ti-Doping and Thickness Effects journal January 2014
Carrier dynamics in α‐Fe2O3 (0001) thin films and single crystals probed by femtosecond transient absorption and reflectivity journal March 2006
Nanonet-Based Hematite Heteronanostructures for Efficient Solar Water Splitting journal March 2011
Atomic Layer Deposition of Ga 2 O 3 Films from a Dialkylamido-Based Precursor journal January 2006

Cited By (2)