Fabrication of 3D Core–Shell Multiwalled Carbon Nanotube@RuO 2 Lithium-Ion Battery Electrodes through a RuO 2 Atomic Layer Deposition Process
- Department of Materials Science and Engineering, University of Maryland, College Park, Maryland 20742, United States; Institute for Systems Research, University of Maryland, College Park, Maryland 20742, United States
- Institute for Systems Research, University of Maryland, College Park, Maryland 20742, United States
- Department of Materials Science and Engineering, College of Engineering, Peking University, Beijing 100871, People’s Republic of China
- Department of Materials Science and Engineering, University of Maryland, College Park, Maryland 20742, United States
- Research Organization:
- Energy Frontier Research Centers (EFRC) (United States). Nanostructures for Electrical Energy Storage (NEES)
- Sponsoring Organization:
- USDOE Office of Science (SC), Basic Energy Sciences (BES)
- DOE Contract Number:
- SC0001160
- OSTI ID:
- 1385197
- Journal Information:
- ACS Nano, Vol. 9, Issue 1; Related Information: NEES partners with University of Maryland (lead); University of California, Irvine; University of Florida; Los Alamos National Laboratory; Sandia National Laboratories; Yale University; ISSN 1936-0851
- Publisher:
- American Chemical Society (ACS)
- Country of Publication:
- United States
- Language:
- English
Similar Records
High capacity and good cycling stability of multi-walled carbon nanotube/SnO{sub 2} core-shell structures as anode materials of lithium-ion batteries
SnS{sub 2} nanoflakes decorated multiwalled carbon nanotubes as high performance anode materials for lithium-ion batteries
Engineering the surface of LiCoO2 electrodes using atomic layer deposition for stable high-voltage lithium ion batteries
Journal Article
·
Thu Apr 15 00:00:00 EDT 2010
· Materials Research Bulletin
·
OSTI ID:1385197
+2 more
SnS{sub 2} nanoflakes decorated multiwalled carbon nanotubes as high performance anode materials for lithium-ion batteries
Journal Article
·
Wed Jan 01 00:00:00 EST 2014
· Materials Research Bulletin
·
OSTI ID:1385197
+3 more
Engineering the surface of LiCoO2 electrodes using atomic layer deposition for stable high-voltage lithium ion batteries
Journal Article
·
Tue Jul 25 00:00:00 EDT 2017
· Nano Research
·
OSTI ID:1385197
+7 more