Title: Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment

Authors:
; ;
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Center for Lignocellulose Structure and Formation (CLSF)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
OSTI Identifier:
1385105
DOE Contract Number:  
SC0001090
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Applied Physics; Journal Volume: 117; Journal Issue: 2; Related Information: CLSF partners with Pennsylvania State University (lead); North Carolina State University; University of Rhode Island; Virginia Tech University
Country of Publication:
United States
Language:
English
Subject:
biofuels (including algae and biomass), bio-inspired, membrane, carbon sequestration, materials and chemistry by design, synthesis (self-assembly)

Citation Formats

Xi, Xiaoning, Kim, Seong H., and Tittmann, Bernhard. Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment. United States: N. p., 2015. Web. doi:10.1063/1.4906094.
Xi, Xiaoning, Kim, Seong H., & Tittmann, Bernhard. Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment. United States. doi:10.1063/1.4906094.
Xi, Xiaoning, Kim, Seong H., and Tittmann, Bernhard. Wed . "Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment". United States. doi:10.1063/1.4906094.
@article{osti_1385105,
title = {Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment},
author = {Xi, Xiaoning and Kim, Seong H. and Tittmann, Bernhard},
abstractNote = {},
doi = {10.1063/1.4906094},
journal = {Journal of Applied Physics},
number = 2,
volume = 117,
place = {United States},
year = {Wed Jan 14 00:00:00 EST 2015},
month = {Wed Jan 14 00:00:00 EST 2015}
}