Title: Gyroidal mesoporous multifunctional nanocomposites via atomic layer deposition

Authors:
; ; ;
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Energy Materials Center at Cornell (EMC2)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
OSTI Identifier:
1370421
DOE Contract Number:  
SC0001086
Resource Type:
Journal Article
Journal Name:
Nanoscale
Additional Journal Information:
Journal Volume: 6; Journal Issue: 15; Related Information: Emc2 partners with Cornell University (lead); Lawrence Berkeley National Laboratory; Journal ID: ISSN 2040-3364
Publisher:
Royal Society of Chemistry
Country of Publication:
United States
Language:
English

Citation Formats

Werner, Jörg G., Scherer, Maik R. J., Steiner, Ullrich, and Wiesner, Ulrich. Gyroidal mesoporous multifunctional nanocomposites via atomic layer deposition. United States: N. p., 2014. Web. doi:10.1039/c4nr01948b.
Werner, Jörg G., Scherer, Maik R. J., Steiner, Ullrich, & Wiesner, Ulrich. Gyroidal mesoporous multifunctional nanocomposites via atomic layer deposition. United States. doi:10.1039/c4nr01948b.
Werner, Jörg G., Scherer, Maik R. J., Steiner, Ullrich, and Wiesner, Ulrich. Wed . "Gyroidal mesoporous multifunctional nanocomposites via atomic layer deposition". United States. doi:10.1039/c4nr01948b.
@article{osti_1370421,
title = {Gyroidal mesoporous multifunctional nanocomposites via atomic layer deposition},
author = {Werner, Jörg G. and Scherer, Maik R. J. and Steiner, Ullrich and Wiesner, Ulrich},
abstractNote = {},
doi = {10.1039/c4nr01948b},
journal = {Nanoscale},
issn = {2040-3364},
number = 15,
volume = 6,
place = {United States},
year = {2014},
month = {1}
}

Works referenced in this record:

Nano-sized transition-metal oxides as negative-electrode materials for lithium-ion batteries
journal, September 2000

  • Poizot, P.; Laruelle, S.; Grugeon, S.
  • Nature, Vol. 407, Issue 6803, p. 496-499
  • DOI: 10.1038/35035045

Building better batteries
journal, February 2008

  • Armand, M.; Tarascon, J.-M.
  • Nature, Vol. 451, Issue 7179, p. 652-657
  • DOI: 10.1038/451652a

Nanostructured materials for advanced energy conversion and storage devices
journal, May 2005

  • Aricò, Antonino Salvatore; Bruce, Peter; Scrosati, Bruno
  • Nature Materials, Vol. 4, Issue 5, p. 366-377
  • DOI: 10.1038/nmat1368

Nanomaterials for Rechargeable Lithium Batteries
journal, April 2008

  • Bruce, Peter G.; Scrosati, Bruno; Tarascon, Jean-Marie
  • Angewandte Chemie International Edition, Vol. 47, Issue 16, p. 2930-2946
  • DOI: 10.1002/anie.200702505

Atomic Layer Deposition: An Overview
journal, January 2010

  • George, Steven M.
  • Chemical Reviews, Vol. 110, Issue 1, p. 111-131
  • DOI: 10.1021/cr900056b

Issues and challenges facing rechargeable lithium batteries
journal, November 2001

  • Tarascon, J.-M.; Armand, M.
  • Nature, Vol. 414, Issue 6861, p. 359-367
  • DOI: 10.1038/35104644

Atomic Layer Deposition of SiO2 and TiO2 in Alumina Tubular Membranes:  Pore Reduction and Effect of Surface Species on Gas Transport
journal, September 2000

  • Cameron, M. A.; Gartland, I. P.; Smith, J. A.
  • Langmuir, Vol. 16, Issue 19, p. 7435-7444
  • DOI: 10.1021/la9916981

Synthesis and Surface Engineering of Complex Nanostructures by Atomic Layer Deposition
journal, November 2007

  • Knez, M.; Nielsch, K.; Niinistö, L.
  • Advanced Materials, Vol. 19, Issue 21, p. 3425-3438
  • DOI: 10.1002/adma.200700079

Superior Electrode Performance of Nanostructured Mesoporous TiO2 (Anatase) through Efficient Hierarchical Mixed Conducting Networks
journal, August 2007

  • Guo, Y.-G.; Hu, Y.-S.; Sigle, W.
  • Advanced Materials, Vol. 19, Issue 16, p. 2087-2091
  • DOI: 10.1002/adma.200602828

Atomic Layer Deposition of Nanostructured Materials for Energy and Environmental Applications
journal, January 2012

  • Marichy, Catherine; Bechelany, Mikhael; Pinna, Nicola
  • Advanced Materials, Vol. 24, Issue 8, p. 1017-1032
  • DOI: 10.1002/adma.201104129

Aerogel Templated ZnO Dye-Sensitized Solar Cells
journal, April 2008

  • Hamann, Thomas W.; Martinson, Alex B. F.; Elam, Jeffrey W.
  • Advanced Materials, Vol. 20, Issue 8, p. 1560-1564
  • DOI: 10.1002/adma.200702781