Title: Design and synthesis of model and practical palladium catalysts using atomic layer deposition

Authors:
; ; ; ; ; ; ;
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Institute for Atom-efficient Chemical Transformations (IACT)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
OSTI Identifier:
1370183
DOE Contract Number:  
AC02-06CH11357
Resource Type:
Journal Article
Journal Name:
Catalysis Science and Technology
Additional Journal Information:
Journal Volume: 6; Journal Issue: 18; Related Information: IACT partners with Argonne National Laboratory (lead); Brookhaven National Laboratory; Northwestern University; Purdue University; University of Wisconsin at Madison; Journal ID: ISSN 2044-4753
Publisher:
Royal Society of Chemistry
Country of Publication:
United States
Language:
English

Citation Formats

Lu, Zheng, Kizilkaya, Orhan, Kropf, A. Jeremy, Piernavieja-Hermida, Mar, Miller, Jeffrey T., Kurtz, Richard L., Elam, Jeffrey W., and Lei, Yu. Design and synthesis of model and practical palladium catalysts using atomic layer deposition. United States: N. p., 2016. Web. doi:10.1039/c6cy00682e.
Lu, Zheng, Kizilkaya, Orhan, Kropf, A. Jeremy, Piernavieja-Hermida, Mar, Miller, Jeffrey T., Kurtz, Richard L., Elam, Jeffrey W., & Lei, Yu. Design and synthesis of model and practical palladium catalysts using atomic layer deposition. United States. doi:10.1039/c6cy00682e.
Lu, Zheng, Kizilkaya, Orhan, Kropf, A. Jeremy, Piernavieja-Hermida, Mar, Miller, Jeffrey T., Kurtz, Richard L., Elam, Jeffrey W., and Lei, Yu. Fri . "Design and synthesis of model and practical palladium catalysts using atomic layer deposition". United States. doi:10.1039/c6cy00682e.
@article{osti_1370183,
title = {Design and synthesis of model and practical palladium catalysts using atomic layer deposition},
author = {Lu, Zheng and Kizilkaya, Orhan and Kropf, A. Jeremy and Piernavieja-Hermida, Mar and Miller, Jeffrey T. and Kurtz, Richard L. and Elam, Jeffrey W. and Lei, Yu},
abstractNote = {},
doi = {10.1039/c6cy00682e},
journal = {Catalysis Science and Technology},
issn = {2044-4753},
number = 18,
volume = 6,
place = {United States},
year = {2016},
month = {1}
}

Works referenced in this record:

Increased Silver Activity for Direct Propylene Epoxidation via Subnanometer Size Effects
journal, April 2010


Atomic layer deposition of palladium films on Al2O3 surfaces
journal, December 2006


Atomic Layer Deposition: An Overview
journal, January 2010

  • George, Steven M.
  • Chemical Reviews, Vol. 110, Issue 1, p. 111-131
  • DOI: 10.1021/cr900056b

Viscous flow reactor with quartz crystal microbalance for thin film growth by atomic layer deposition
journal, August 2002

  • Elam, J. W.; Groner, M. D.; George, S. M.
  • Review of Scientific Instruments, Vol. 73, Issue 8, p. 2981-2987
  • DOI: 10.1063/1.1490410

Review of Pt-Based Bimetallic Catalysis: From Model Surfaces to Supported Catalysts
journal, August 2012

  • Yu, Weiting; Porosoff, Marc D.; Chen, Jingguang G.
  • Chemical Reviews, Vol. 112, Issue 11, p. 5780-5817
  • DOI: 10.1021/cr300096b