Title: Corrosion Of Superalloys In 200 Bar, 750 C Supercritical Carbon Dioxide

Authors:
 [1];  [1];  [2]
  1. ORNL
  2. Gas Technology Institute, Des Plaines, IL
Publication Date:
Research Org.:
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Sponsoring Org.:
FE USDOE - Office of Fossil Energy (FE)
OSTI Identifier:
1360059
DOE Contract Number:  
AC05-00OR22725
Resource Type:
Conference
Resource Relation:
Conference: Corrosion 2017 Conference & Exposition, New Orleans, LA, USA, 20170326, 20170330
Country of Publication:
United States
Language:
English

Citation Formats

Keiser, James R, Leonard, Donovan N, and McDowell, Michael. Corrosion Of Superalloys In 200 Bar, 750 C Supercritical Carbon Dioxide. United States: N. p., 2017. Web.
Keiser, James R, Leonard, Donovan N, & McDowell, Michael. Corrosion Of Superalloys In 200 Bar, 750 C Supercritical Carbon Dioxide. United States.
Keiser, James R, Leonard, Donovan N, and McDowell, Michael. Sun . "Corrosion Of Superalloys In 200 Bar, 750 C Supercritical Carbon Dioxide". United States. doi:.
@article{osti_1360059,
title = {Corrosion Of Superalloys In 200 Bar, 750 C Supercritical Carbon Dioxide},
author = {Keiser, James R and Leonard, Donovan N and McDowell, Michael},
abstractNote = {},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {Sun Jan 01 00:00:00 EST 2017},
month = {Sun Jan 01 00:00:00 EST 2017}
}

Conference:
Other availability
Please see Document Availability for additional information on obtaining the full-text document. Library patrons may search WorldCat to identify libraries that hold this conference proceeding.

Save / Share: