Title: Uncertainty quantification methodologies development for stress corrosion cracking of canister welds

Abstract

This letter report presents a probabilistic performance assessment model to evaluate the probability of canister failure (through-wall penetration) by SCC. The model first assesses whether environmental conditions for SCC – the presence of an aqueous film – are present at canister weld locations (where tensile stresses are likely to occur) on the canister surface. Geometry-specific storage system thermal models and weather data sets representative of U.S. spent nuclear fuel (SNF) storage sites are implemented to evaluate location-specific canister surface temperature and relative humidity (RH). As the canister cools and aqueous conditions become possible, the occurrence of corrosion is evaluated. Corrosion is modeled as a two-step process: first, pitting is initiated, and the extent and depth of pitting is a function of the chloride surface load and the environmental conditions (temperature and RH). Second, as corrosion penetration increases, the pit eventually transitions to a SCC crack, with crack initiation becoming more likely with increasing pit depth. Once pits convert to cracks, a crack growth model is implemented. The SCC growth model includes rate dependencies on both temperature and crack tip stress intensity factor, and crack growth only occurs in time steps when aqueous conditions are predicted. The model suggests that SCCmore » is likely to occur over potential SNF interim storage intervals; however, this result is based on many modeling assumptions. Sensitivity analyses provide information on the model assumptions and parameter values that have the greatest impact on predicted storage canister performance, and provide guidance for further research to reduce uncertainties.« less

Authors:
 [1];  [1]
  1. Sandia National Lab. (SNL-NM), Albuquerque, NM (United States)
Publication Date:
Research Org.:
Sandia National Lab. (SNL-NM), Albuquerque, NM (United States)
Sponsoring Org.:
USDOE Office of Nuclear Energy (NE), Fuel Cycle Technologies (NE-5). Used Fuel Disposition Campaign (UFDC)
OSTI Identifier:
1333707
Report Number(s):
SAND2016-9487R
647678; TRN: US1700774
DOE Contract Number:  
AC04-94AL85000
Resource Type:
Technical Report
Country of Publication:
United States
Language:
English
Subject:
42 ENGINEERING; 11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS; STRESS CORROSION; WELDED JOINTS; CONTAINERS; CRACKS; SENSITIVITY ANALYSIS; SPENT FUEL STORAGE; STRESSES; CRACK PROPAGATION; CHLORIDES; SURFACES; PROBABILISTIC ESTIMATION; HUMIDITY; PERFORMANCE; STRESS INTENSITY FACTORS; FAILURES; PROBABILITY; SIMULATION; WALLS; TEMPERATURE DEPENDENCE

Citation Formats

Dingreville, Remi Philippe Michel, and Bryan, Charles R. Uncertainty quantification methodologies development for stress corrosion cracking of canister welds. United States: N. p., 2016. Web. doi:10.2172/1333707.
Dingreville, Remi Philippe Michel, & Bryan, Charles R. Uncertainty quantification methodologies development for stress corrosion cracking of canister welds. United States. doi:10.2172/1333707.
Dingreville, Remi Philippe Michel, and Bryan, Charles R. Fri . "Uncertainty quantification methodologies development for stress corrosion cracking of canister welds". United States. doi:10.2172/1333707. https://www.osti.gov/servlets/purl/1333707.
@article{osti_1333707,
title = {Uncertainty quantification methodologies development for stress corrosion cracking of canister welds},
author = {Dingreville, Remi Philippe Michel and Bryan, Charles R.},
abstractNote = {This letter report presents a probabilistic performance assessment model to evaluate the probability of canister failure (through-wall penetration) by SCC. The model first assesses whether environmental conditions for SCC – the presence of an aqueous film – are present at canister weld locations (where tensile stresses are likely to occur) on the canister surface. Geometry-specific storage system thermal models and weather data sets representative of U.S. spent nuclear fuel (SNF) storage sites are implemented to evaluate location-specific canister surface temperature and relative humidity (RH). As the canister cools and aqueous conditions become possible, the occurrence of corrosion is evaluated. Corrosion is modeled as a two-step process: first, pitting is initiated, and the extent and depth of pitting is a function of the chloride surface load and the environmental conditions (temperature and RH). Second, as corrosion penetration increases, the pit eventually transitions to a SCC crack, with crack initiation becoming more likely with increasing pit depth. Once pits convert to cracks, a crack growth model is implemented. The SCC growth model includes rate dependencies on both temperature and crack tip stress intensity factor, and crack growth only occurs in time steps when aqueous conditions are predicted. The model suggests that SCC is likely to occur over potential SNF interim storage intervals; however, this result is based on many modeling assumptions. Sensitivity analyses provide information on the model assumptions and parameter values that have the greatest impact on predicted storage canister performance, and provide guidance for further research to reduce uncertainties.},
doi = {10.2172/1333707},
journal = {},
number = ,
volume = ,
place = {United States},
year = {Fri Sep 30 00:00:00 EDT 2016},
month = {Fri Sep 30 00:00:00 EDT 2016}
}

Technical Report:

Save / Share: