A low-temperature synthesis of electrochemical active Pt nanoparticles and thin films by atomic layer deposition on Si(111) and glassy carbon surfaces
- Authors:
- Publication Date:
- Sponsoring Org.:
- USDOE
- OSTI Identifier:
- 1245645
- Grant/Contract Number:
- SC0004993
- Resource Type:
- Journal Article: Publisher's Accepted Manuscript
- Journal Name:
- Thin Solid Films
- Additional Journal Information:
- Journal Name: Thin Solid Films Journal Volume: 586 Journal Issue: C; Journal ID: ISSN 0040-6090
- Publisher:
- Elsevier
- Country of Publication:
- Netherlands
- Language:
- English
Citation Formats
Liu, Rui, Han, Lihao, Huang, Zhuangqun, Ferrer, Ivonne M., Smets, Arno H. M., Zeman, Miro, Brunschwig, Bruce S., and Lewis, Nathan S. A low-temperature synthesis of electrochemical active Pt nanoparticles and thin films by atomic layer deposition on Si(111) and glassy carbon surfaces. Netherlands: N. p., 2015.
Web. doi:10.1016/j.tsf.2015.04.018.
Liu, Rui, Han, Lihao, Huang, Zhuangqun, Ferrer, Ivonne M., Smets, Arno H. M., Zeman, Miro, Brunschwig, Bruce S., & Lewis, Nathan S. A low-temperature synthesis of electrochemical active Pt nanoparticles and thin films by atomic layer deposition on Si(111) and glassy carbon surfaces. Netherlands. https://doi.org/10.1016/j.tsf.2015.04.018
Liu, Rui, Han, Lihao, Huang, Zhuangqun, Ferrer, Ivonne M., Smets, Arno H. M., Zeman, Miro, Brunschwig, Bruce S., and Lewis, Nathan S. 2015.
"A low-temperature synthesis of electrochemical active Pt nanoparticles and thin films by atomic layer deposition on Si(111) and glassy carbon surfaces". Netherlands. https://doi.org/10.1016/j.tsf.2015.04.018.
@article{osti_1245645,
title = {A low-temperature synthesis of electrochemical active Pt nanoparticles and thin films by atomic layer deposition on Si(111) and glassy carbon surfaces},
author = {Liu, Rui and Han, Lihao and Huang, Zhuangqun and Ferrer, Ivonne M. and Smets, Arno H. M. and Zeman, Miro and Brunschwig, Bruce S. and Lewis, Nathan S.},
abstractNote = {},
doi = {10.1016/j.tsf.2015.04.018},
url = {https://www.osti.gov/biblio/1245645},
journal = {Thin Solid Films},
issn = {0040-6090},
number = C,
volume = 586,
place = {Netherlands},
year = {Wed Jul 01 00:00:00 EDT 2015},
month = {Wed Jul 01 00:00:00 EDT 2015}
}
Free Publicly Available Full Text
Publisher's Version of Record at https://doi.org/10.1016/j.tsf.2015.04.018
Other availability
Cited by: 8 works
Citation information provided by
Web of Science
Web of Science
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.