Title: Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition

Abstract

Atomic layer deposition (ALD) was used to deposit Ni and Pt on alumina supports to form monometallic and bimetallic catalysts with initial particle sizes of 1–2.4 nm. The ALD catalysts were more active (per mass of metal) than catalysts prepared by incipient wetness (IW) for dry reforming of methane (DRM), and they did not form carbon whiskers during reaction due to their sufficiently small size. Catalysts modified by Pt ALD had higher rates of reaction per mass of metal and inhibited coking, whereas NiPt catalysts synthesized by IW still formed carbon whiskers. Temperature-programmed reduction of Ni catalysts modified by Pt ALD indicated the presence of bimetallic interaction. Density functional theory calculations suggested that under reaction conditions, the NiPt surfaces form Ni-terminated surfaces that are associated with higher DRM rates (due to their C and O adsorption energies, as well as the CO formation and CH4 dissociation energies).

Authors:
; ; ; ; ; ;
Publication Date:
Research Org.:
Pacific Northwest National Laboratory (PNNL), Richland, WA (US), Environmental Molecular Sciences Laboratory (EMSL)
Sponsoring Org.:
USDOE
OSTI Identifier:
1222068
DOE Contract Number:  
AC05-76RL01830
Resource Type:
Journal Article
Resource Relation:
Journal Name: Applied Catalysis. A, General, 492:107–116
Country of Publication:
United States
Language:
English
Subject:
Environmental Molecular Sciences Laboratory

Citation Formats

Gould, Troy D., Montemore, Matthew M., Lubers, Alia M., Ellis, Lucas D., Weimer, Alan, Falconer, John L., and Medlin, James W. Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition. United States: N. p., 2015. Web. doi:10.1016/j.apcata.2014.11.037.
Gould, Troy D., Montemore, Matthew M., Lubers, Alia M., Ellis, Lucas D., Weimer, Alan, Falconer, John L., & Medlin, James W. Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition. United States. doi:10.1016/j.apcata.2014.11.037.
Gould, Troy D., Montemore, Matthew M., Lubers, Alia M., Ellis, Lucas D., Weimer, Alan, Falconer, John L., and Medlin, James W. Wed . "Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition". United States. doi:10.1016/j.apcata.2014.11.037.
@article{osti_1222068,
title = {Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition},
author = {Gould, Troy D. and Montemore, Matthew M. and Lubers, Alia M. and Ellis, Lucas D. and Weimer, Alan and Falconer, John L. and Medlin, James W.},
abstractNote = {Atomic layer deposition (ALD) was used to deposit Ni and Pt on alumina supports to form monometallic and bimetallic catalysts with initial particle sizes of 1–2.4 nm. The ALD catalysts were more active (per mass of metal) than catalysts prepared by incipient wetness (IW) for dry reforming of methane (DRM), and they did not form carbon whiskers during reaction due to their sufficiently small size. Catalysts modified by Pt ALD had higher rates of reaction per mass of metal and inhibited coking, whereas NiPt catalysts synthesized by IW still formed carbon whiskers. Temperature-programmed reduction of Ni catalysts modified by Pt ALD indicated the presence of bimetallic interaction. Density functional theory calculations suggested that under reaction conditions, the NiPt surfaces form Ni-terminated surfaces that are associated with higher DRM rates (due to their C and O adsorption energies, as well as the CO formation and CH4 dissociation energies).},
doi = {10.1016/j.apcata.2014.11.037},
journal = {Applied Catalysis. A, General, 492:107–116},
number = ,
volume = ,
place = {United States},
year = {Wed Feb 25 00:00:00 EST 2015},
month = {Wed Feb 25 00:00:00 EST 2015}
}