Title: Fabrication of 3D Core–Shell Multiwalled Carbon Nanotube@RuO2 Lithium-Ion Battery Electrodes through a RuO2 Atomic Layer Deposition Process

Authors:
; ; ; ; ; ; ;
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC); Nanostructures for Electrical Energy Storage (NEES)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
OSTI Identifier:
1210601
DOE Contract Number:  
SC0001160
Resource Type:
Journal Article
Resource Relation:
Journal Name: ACS Nano; Journal Volume: 9(1); Related Information: NEES partners with University of Maryland (lead); University of California, Irvine; University of Florida; Los Alamos National Laboratory; Sandia National Laboratories; Yale University
Country of Publication:
United States
Language:
English
Subject:
bio-inspired, energy storage (including batteries and capacitors), defects, charge transport, synthesis (novel materials), synthesis (self-assembly), synthesis (scalable processing)

Citation Formats

Gregorczyk, Keith, Kozen, Alexander C, Chen, Xin, Schroeder, Marshall A, Noked, Malachi, Cao, A. Y., Hu, Liangbing, and Rubloff, Gary W. Fabrication of 3D Core–Shell Multiwalled Carbon Nanotube@RuO2 Lithium-Ion Battery Electrodes through a RuO2 Atomic Layer Deposition Process. United States: N. p., 2015. Web. doi:10.1021/nn505644q.
Gregorczyk, Keith, Kozen, Alexander C, Chen, Xin, Schroeder, Marshall A, Noked, Malachi, Cao, A. Y., Hu, Liangbing, & Rubloff, Gary W. Fabrication of 3D Core–Shell Multiwalled Carbon Nanotube@RuO2 Lithium-Ion Battery Electrodes through a RuO2 Atomic Layer Deposition Process. United States. doi:10.1021/nn505644q.
Gregorczyk, Keith, Kozen, Alexander C, Chen, Xin, Schroeder, Marshall A, Noked, Malachi, Cao, A. Y., Hu, Liangbing, and Rubloff, Gary W. Tue . "Fabrication of 3D Core–Shell Multiwalled Carbon Nanotube@RuO2 Lithium-Ion Battery Electrodes through a RuO2 Atomic Layer Deposition Process". United States. doi:10.1021/nn505644q.
@article{osti_1210601,
title = {Fabrication of 3D Core–Shell Multiwalled Carbon Nanotube@RuO2 Lithium-Ion Battery Electrodes through a RuO2 Atomic Layer Deposition Process},
author = {Gregorczyk, Keith and Kozen, Alexander C and Chen, Xin and Schroeder, Marshall A and Noked, Malachi and Cao, A. Y. and Hu, Liangbing and Rubloff, Gary W},
abstractNote = {},
doi = {10.1021/nn505644q},
journal = {ACS Nano},
number = ,
volume = 9(1),
place = {United States},
year = {Tue Jan 27 00:00:00 EST 2015},
month = {Tue Jan 27 00:00:00 EST 2015}
}