Title: Unexpected high power performance of atomic layer deposition coated Li(Ni1/3Mn1/3C01/3)O2 cathodes

Journal Article · · Journal of Power Sources

Research Organization:
Brookhaven National Lab. (BNL), Upton, NY (United States). National Synchrotron Light Source
Sponsoring Organization:
USDOE EE OFFICE OF ENERGY EFFICIENCY & RENEWABLE ENERGY (EERE)
DOE Contract Number:
DE-AC02-98CH10886
OSTI ID:
1124555
Report Number(s):
BNL-103621-2014-JA; R&D Project: EST-451
Journal Information:
Journal of Power Sources, Vol. 254
Country of Publication:
United States
Language:
English

Similar Records

Unexpected High Power Performance of Atomic Layer Deposition Coated Li[Ni1/3Mn1/3Co1/3]O2 Cathodes
Journal Article · Thu May 15 00:00:00 EDT 2014 · Journal of Power Sources · OSTI ID:1124555

Three-dimensional morphological measurements of LiCoO2 and LiCoO2/Li (Ni1/3Mn1/3Co1/3)O2 lithium-ion battery cathodes
Journal Article · Thu Nov 15 00:00:00 EST 2012 · Journal of Power Sources · OSTI ID:1124555

3D analysis of a LiCoO2–Li(Ni1/3Mn1/3Co1/3)O2 Li-ion battery positive electrode using x-ray nano-tomography
Journal Article · Fri Dec 28 00:00:00 EST 2012 · Electrochemistry Communications · OSTI ID:1124555