skip to main content
OSTI.GOV title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Improved Functionality of Lithium-Ion Batteries Enabled by Atomic Layer Deposition on the Porous Microstructure of Polymer Separators and Coating Electrodes

Authors:
; ; ; ; ; ; ; ;
Publication Date:
Research Org.:
National Renewable Energy Lab. (NREL), Golden, CO (United States)
Sponsoring Org.:
USDOE Office of Energy Efficiency and Renewable Energy (EERE), Vehicle Technologies Office (EE-3V)
OSTI Identifier:
1051941
Report Number(s):
NREL/JA-5400-52797
DOE Contract Number:  
AC36-08GO28308
Resource Type:
Journal Article
Journal Name:
Advanced Energy Materials
Additional Journal Information:
Journal Volume: 2; Journal Issue: 8
Country of Publication:
United States
Language:
English
Subject:
25 ENERGY STORAGE; 33 ADVANCED PROPULSION SYSTEMS; 36 MATERIALS SCIENCE; lithium ion batteries; atomic layer depostion; polymer separators; coating electrodes; fuel cells

Citation Formats

Jung, Yoon Seok, Cavanagh, Andrew S., Gedvilas, Lynn, Widjonarko, Nicodemus E., Scott, Isaac D., Lee, Se Hee, Kim, Gi Heon, George, Steven M., and Dillon, Anne C. Improved Functionality of Lithium-Ion Batteries Enabled by Atomic Layer Deposition on the Porous Microstructure of Polymer Separators and Coating Electrodes. United States: N. p., 2012. Web. doi:10.1002/aenm.201100750.
Jung, Yoon Seok, Cavanagh, Andrew S., Gedvilas, Lynn, Widjonarko, Nicodemus E., Scott, Isaac D., Lee, Se Hee, Kim, Gi Heon, George, Steven M., & Dillon, Anne C. Improved Functionality of Lithium-Ion Batteries Enabled by Atomic Layer Deposition on the Porous Microstructure of Polymer Separators and Coating Electrodes. United States. doi:10.1002/aenm.201100750.
Jung, Yoon Seok, Cavanagh, Andrew S., Gedvilas, Lynn, Widjonarko, Nicodemus E., Scott, Isaac D., Lee, Se Hee, Kim, Gi Heon, George, Steven M., and Dillon, Anne C. Wed . "Improved Functionality of Lithium-Ion Batteries Enabled by Atomic Layer Deposition on the Porous Microstructure of Polymer Separators and Coating Electrodes". United States. doi:10.1002/aenm.201100750.
@article{osti_1051941,
title = {Improved Functionality of Lithium-Ion Batteries Enabled by Atomic Layer Deposition on the Porous Microstructure of Polymer Separators and Coating Electrodes},
author = {Jung, Yoon Seok and Cavanagh, Andrew S. and Gedvilas, Lynn and Widjonarko, Nicodemus E. and Scott, Isaac D. and Lee, Se Hee and Kim, Gi Heon and George, Steven M. and Dillon, Anne C.},
abstractNote = {},
doi = {10.1002/aenm.201100750},
journal = {Advanced Energy Materials},
number = 8,
volume = 2,
place = {United States},
year = {2012},
month = {8}
}

Works referenced in this record:

Building better batteries
journal, February 2008

  • Armand, M.; Tarascon, J.-M.
  • Nature, Vol. 451, Issue 7179, p. 652-657
  • DOI: 10.1038/451652a

Challenges for Rechargeable Li Batteries
journal, February 2010

  • Goodenough, John B.; Kim, Youngsik
  • Chemistry of Materials, Vol. 22, Issue 3, p. 587-603
  • DOI: 10.1021/cm901452z

Carbon Nanotubes for Photoconversion and Electrical Energy Storage
journal, November 2010


Battery Separators
journal, October 2004

  • Arora, Pankaj; Zhang, Zhengming (John)
  • Chemical Reviews, Vol. 104, Issue 10
  • DOI: 10.1021/cr020738u

A consideration of lithium cell safety
journal, September 1999


Electrochemical performances of lithium-ion cells prepared with polyethylene oxide-coated separators
journal, October 2001


Thin-film type Li-ion battery, using a polyethylene separator grafted with glycidyl methacrylate
journal, November 2004


Effect of thickness of coating layer on polymer-coated separator on cycling performance of lithium-ion polymer cells
journal, April 2004


Mussel-Inspired Polydopamine-Treated Polyethylene Separators for High-Power Li-Ion Batteries
journal, May 2011

  • Ryou, Myung-Hyun; Lee, Yong Min; Park, Jung-Ki
  • Advanced Materials, Vol. 23, Issue 27
  • DOI: 10.1002/adma.201100303

An inorganic composite membrane as the separator of Li-ion batteries
journal, February 2005


A powder particle size effect on ceramic powder based separator for lithium rechargeable battery
journal, August 2005


Preparation of micro-porous gel polymer for lithium ion polymer battery
journal, November 2004


Enhancement of thermal stability and cycling performance in lithium-ion cells through the use of ceramic-coated separators
journal, September 2010


Preparation of a trilayer separator and its application to lithium-ion batteries
journal, December 2010


Enhanced Stability of LiCoO2 Cathodes in Lithium-Ion Batteries Using Surface Modification by Atomic Layer Deposition
journal, January 2010

  • Jung, Yoon Seok; Cavanagh, Andrew S.; Dillon, Anne C.
  • Journal of The Electrochemical Society, Vol. 157, Issue 1, p. A75-A81
  • DOI: 10.1149/1.3258274

Ultrathin Coatings on Nano-LiCoO2 for Li-Ion Vehicular Applications
journal, February 2011

  • Scott, Isaac D.; Jung, Yoon Seok; Cavanagh, Andrew S.
  • Nano Letters, Vol. 11, Issue 2, p. 414-418
  • DOI: 10.1021/nl1030198

Electrochemical effects of ALD surface modification on combustion synthesized LiNi1/3Mn1/3Co1/3O2 as a layered-cathode material
journal, March 2011


Ultrathin Direct Atomic Layer Deposition on Composite Electrodes for Highly Durable and Safe Li-Ion Batteries
journal, April 2010

  • Jung, Yoon Seok; Cavanagh, Andrew S.; Riley, Leah A.
  • Advanced Materials, Vol. 22, Issue 19
  • DOI: 10.1002/adma.200903951

Conformal Surface Coatings to Enable High Volume Expansion Li-Ion Anode Materials
journal, May 2010

  • Riley, Leah A.; Cavanagh, Andrew S.; George, Steven M.
  • ChemPhysChem, Vol. 11, Issue 10
  • DOI: 10.1002/cphc.201000158

Fe3O4 Nanoparticles Confined in Mesocellular Carbon Foam for High Performance Anode Materials for Lithium-Ion Batteries
journal, April 2011

  • Kang, Eunae; Jung, Yoon Seok; Cavanagh, Andrew S.
  • Advanced Functional Materials, Vol. 21, Issue 13
  • DOI: 10.1002/adfm.201002576

Atomic Layer Deposition: An Overview
journal, January 2010

  • George, Steven M.
  • Chemical Reviews, Vol. 110, Issue 1, p. 111-131
  • DOI: 10.1021/cr900056b

Surface chemistry of Al2O3 deposition using Al(CH3)3 and H2O in a binary reaction sequence
journal, January 1995


Atomic Layer Deposition of Al 2 O 3 Films on Polyethylene Particles
journal, December 2004

  • Ferguson, J. D.; Weimer, A. W.; George, S. M.
  • Chemistry of Materials, Vol. 16, Issue 26
  • DOI: 10.1021/cm040008y

Nucleation and Growth during Al 2 O 3 Atomic Layer Deposition on Polymers
journal, November 2005

  • Wilson, C. A.; Grubbs, R. K.; George, S. M.
  • Chemistry of Materials, Vol. 17, Issue 23
  • DOI: 10.1021/cm050704d

Three dimensional structure of celgard® microporous membranes
journal, August 1983


Greatly Increased Toughness of Infiltrated Spider Silk
journal, April 2009


FT-IR Study of Water Adsorption on Aluminum Oxide Surfaces
journal, January 2003

  • Al-Abadleh, Hind A.; Grassian, V. H.
  • Langmuir, Vol. 19, Issue 2
  • DOI: 10.1021/la026208a