Title: LABORATORY REPORT ON THE REDUCTION AND STABILIZATION (IMMOBILIZATION) OF PERTECHNETATE TO TECHNETIUM DIOXIDE USING TIN(II)APATITE

Abstract

This effort is part of the technetium management initiative and provides data for the handling and disposition of technetium. To that end, the objective of this effort was to challenge tin(II)apatite (Sn(II)apatite) against double-shell tank 241-AN-105 simulant spiked with pertechnetate (TcO{sub 4}{sup -}). The Sn(II)apatite used in this effort was synthesized on site using a recipe developed at and provided by Sandia National Laboratories; the synthesis provides a high quality product while requiring minimal laboratory effort. The Sn(II)apatite reduces pertechnetate from the mobile +7 oxidation state to the non-mobile +4 oxidation state. It also sequesters the technetium and does not allow for re-oxidization to the mo bile +7 state under acidic or oxygenated conditions within the tested period oftime (6 weeks). Previous work (RPP-RPT-39195, Assessment of Technetium Leachability in Cement-Stabilized Basin 43 Groundwater Brine) indicated that the Sn(II)apatite can achieve an ANSI leachability index in Cast Stone of 12.8. The technetium distribution coefficient for Sn(II)apatite exhibits a direct correlation with the pH of the contaminated media. Table A shows Sn(II)apatite distribution coefficients as a function of pH. The asterisked numbers indicate that the lower detection limit of the analytical instrument was used to calculate the distribution coefficient as the concentrationmore » of technetium left in solution was less than the detection limit. The loaded sample (200 mg of Sn(II)apatite loaded with O.311 mg of Tc-99) was subjected to different molarities of nitric acid to determine if the Sn(II)apatite would release the sequestered technetium. The acid was allowed to contact for 1 minute with gentle shaking ('1st wash'); the aqueous solution was then filtered, and the filtrate was analyzed for Tc-99. Table B shows the results ofthe nitric acid exposure. Another portion of acid was added, shaken for a minute, and filtered ('2nd wash'). The technetium-loaded Sn(II)apatite was also subjected to water leach tests. The loaded sample (0.2 g of Sn(II)apatite was loaded with 0.342 mg of Tc-99) was placed in a 200-mL distilled water column and sparged with air. Samples were taken weekly over a 6-week period, and the dissolved oxygen ranged from 8.4 to 8.7 mg/L (average 8.5 mg/L); all samples recorded less than the detection limit of 0.01 mg/L Tc-99. The mechanism by which TcO{sub 2} is sequestered and hence protected from re-oxidation appears to be an exchange with phosphate in the apatite lattice, as the phosphorus that appeared in solution after reaction with technetium was essentially the same moles of technetium that were taken up by the Sn(II)apatite (Table 6). Overall, the reduction of the mobile pertechnetate (+7) to the less mobile technetium dioxide (+4) by Sn(II)apatite and subsequent sequestration of the technetium in the material indicates that Sn(II)apatite is an excellent candidate for long-term immobilization of technetium. The indications are that the Sn(II)apatite will lend itself to sequestering and inhibiting the reoxidation to the mobile pertechnetate species, thus keeping the radionuclide out of the environment.« less

Authors:
; ; ; ; ;
Publication Date:
Research Org.:
Hanford Site (HNF), Richland, WA (United States)
Sponsoring Org.:
USDOE Office of Environmental Management (EM)
OSTI Identifier:
1045370
Report Number(s):
LAB-RPT-12-00001
TRN: US201217%%6
DOE Contract Number:  
DE-AC27-08RV14800
Resource Type:
Technical Report
Country of Publication:
United States
Language:
English
Subject:
58 GEOSCIENCES; APATITES; AQUEOUS SOLUTIONS; BILE; DISSOLVED GASES; DISTRIBUTION; MANAGEMENT; NITRIC ACID; OXYGEN; PERTECHNETATES; PHOSPHATES; PHOSPHORUS; RADIOISOTOPES; SANDIA NATIONAL LABORATORIES; SENSITIVITY; STABILIZATION; SYNTHESIS; TANKS; TECHNETIUM; VALENCE

Citation Formats

JB, DUNCAN, K, HAGERTY, WP, MOORE, RN, RHODES, JM, JOHNSON, and RC, MOORE. LABORATORY REPORT ON THE REDUCTION AND STABILIZATION (IMMOBILIZATION) OF PERTECHNETATE TO TECHNETIUM DIOXIDE USING TIN(II)APATITE. United States: N. p., 2012. Web. doi:10.2172/1045370.
JB, DUNCAN, K, HAGERTY, WP, MOORE, RN, RHODES, JM, JOHNSON, & RC, MOORE. LABORATORY REPORT ON THE REDUCTION AND STABILIZATION (IMMOBILIZATION) OF PERTECHNETATE TO TECHNETIUM DIOXIDE USING TIN(II)APATITE. United States. https://doi.org/10.2172/1045370
JB, DUNCAN, K, HAGERTY, WP, MOORE, RN, RHODES, JM, JOHNSON, and RC, MOORE. Fri . "LABORATORY REPORT ON THE REDUCTION AND STABILIZATION (IMMOBILIZATION) OF PERTECHNETATE TO TECHNETIUM DIOXIDE USING TIN(II)APATITE". United States. https://doi.org/10.2172/1045370. https://www.osti.gov/servlets/purl/1045370.
@article{osti_1045370,
title = {LABORATORY REPORT ON THE REDUCTION AND STABILIZATION (IMMOBILIZATION) OF PERTECHNETATE TO TECHNETIUM DIOXIDE USING TIN(II)APATITE},
author = {JB, DUNCAN and K, HAGERTY and WP, MOORE and RN, RHODES and JM, JOHNSON and RC, MOORE},
abstractNote = {This effort is part of the technetium management initiative and provides data for the handling and disposition of technetium. To that end, the objective of this effort was to challenge tin(II)apatite (Sn(II)apatite) against double-shell tank 241-AN-105 simulant spiked with pertechnetate (TcO{sub 4}{sup -}). The Sn(II)apatite used in this effort was synthesized on site using a recipe developed at and provided by Sandia National Laboratories; the synthesis provides a high quality product while requiring minimal laboratory effort. The Sn(II)apatite reduces pertechnetate from the mobile +7 oxidation state to the non-mobile +4 oxidation state. It also sequesters the technetium and does not allow for re-oxidization to the mo bile +7 state under acidic or oxygenated conditions within the tested period oftime (6 weeks). Previous work (RPP-RPT-39195, Assessment of Technetium Leachability in Cement-Stabilized Basin 43 Groundwater Brine) indicated that the Sn(II)apatite can achieve an ANSI leachability index in Cast Stone of 12.8. The technetium distribution coefficient for Sn(II)apatite exhibits a direct correlation with the pH of the contaminated media. Table A shows Sn(II)apatite distribution coefficients as a function of pH. The asterisked numbers indicate that the lower detection limit of the analytical instrument was used to calculate the distribution coefficient as the concentration of technetium left in solution was less than the detection limit. The loaded sample (200 mg of Sn(II)apatite loaded with O.311 mg of Tc-99) was subjected to different molarities of nitric acid to determine if the Sn(II)apatite would release the sequestered technetium. The acid was allowed to contact for 1 minute with gentle shaking ('1st wash'); the aqueous solution was then filtered, and the filtrate was analyzed for Tc-99. Table B shows the results ofthe nitric acid exposure. Another portion of acid was added, shaken for a minute, and filtered ('2nd wash'). The technetium-loaded Sn(II)apatite was also subjected to water leach tests. The loaded sample (0.2 g of Sn(II)apatite was loaded with 0.342 mg of Tc-99) was placed in a 200-mL distilled water column and sparged with air. Samples were taken weekly over a 6-week period, and the dissolved oxygen ranged from 8.4 to 8.7 mg/L (average 8.5 mg/L); all samples recorded less than the detection limit of 0.01 mg/L Tc-99. The mechanism by which TcO{sub 2} is sequestered and hence protected from re-oxidation appears to be an exchange with phosphate in the apatite lattice, as the phosphorus that appeared in solution after reaction with technetium was essentially the same moles of technetium that were taken up by the Sn(II)apatite (Table 6). Overall, the reduction of the mobile pertechnetate (+7) to the less mobile technetium dioxide (+4) by Sn(II)apatite and subsequent sequestration of the technetium in the material indicates that Sn(II)apatite is an excellent candidate for long-term immobilization of technetium. The indications are that the Sn(II)apatite will lend itself to sequestering and inhibiting the reoxidation to the mobile pertechnetate species, thus keeping the radionuclide out of the environment.},
doi = {10.2172/1045370},
url = {https://www.osti.gov/biblio/1045370}, journal = {},
number = ,
volume = ,
place = {United States},
year = {2012},
month = {6}
}