Temperature effects on hydrogen-induced cracking in an iron-based superalloy
Conference
·
OSTI ID:10194547
- Research Organization:
- Sandia National Labs., Livermore, CA (United States)
- DOE Contract Number:
- AC04-94AL85000
- OSTI ID:
- 10194547
- Report Number(s):
- SAND-95-8435C; CONF-940945-3; ON: DE95003037; BR: GB0103012
- Resource Relation:
- Conference: 5. international conference on hydrogen effects on material behavior,Moran, WY (United States),11-15 Sep 1994
- Country of Publication:
- United States
- Language:
- English
Similar Records
Microstructure Effects on Hydrogen Induced Crack Growth Susceptibility of a High Strength Iron Based Superalloy.
Effects of Internal and External Hydrogen Environments on Crack Growth Susceptibility of an Iron Based Superalloy.
Effects of Hydrogen Pressure on Crack Growth Rates in an Iron Based Superalloy.
Conference
·
Tue Oct 01 00:00:00 EDT 2019
·
OSTI ID:10194547
+2 more
Effects of Internal and External Hydrogen Environments on Crack Growth Susceptibility of an Iron Based Superalloy.
Conference
·
Mon Aug 01 00:00:00 EDT 2011
·
OSTI ID:10194547
+1 more
Effects of Hydrogen Pressure on Crack Growth Rates in an Iron Based Superalloy.
Conference
·
Sun Jan 01 00:00:00 EST 2017
·
OSTI ID:10194547
+2 more