Work continued on the development of a microkinetic model of Fischer-Tropsch synthesis (FTS) on supported and unsupported Fe catalysts. The following aspects of the FT mechanism on unsupported iron catalysts were investigated on during this third year: (1) the collection of rate data in a Berty CSTR reactor based on sequential design of experiments; (2) CO adsorption and CO-TPD for obtaining the heat of adsorption of CO on polycrystalline iron; and (3) isothermal hydrogenation (IH) after Fischer Tropsch reaction to identify and quantify surface carbonaceous species. Rates of C{sub 2+} formation on unsupported iron catalysts at 220 C and 20 atm correlated well to a Langmuir-Hinshelwood type expression, derived assuming carbon hydrogenation to CH and OH recombination to water to be rate-determining steps. From desorption of molecularly adsorbed CO at different temperatures the heat of adsorption of CO on polycrystalline iron was determined to be 100 kJ/mol. Amounts and types of carbonaceous species formed after FT reaction for 5-10 minutes at 150, 175, 200 and 285 C vary significantly with temperature. Mr. Brian Critchfield completed his M.S. thesis work on a statistically designed study of the kinetics of FTS on 20% Fe/alumina. Preparation of a paper describing this work is in progress. Results of these studies were reported at the Annual Meeting of the Western States Catalysis and at the San Francisco AIChE meeting. In the coming period, studies will focus on quantitative determination of the rates of kinetically-relevant elementary steps on unsupported Fe catalysts with/without K and Pt promoters by SSITKA method. This study will help us to (1) understand effects of promoter and support on elementary kinetic parameters and (2) build a microkinetics model for FTS on iron. Calculations using periodic, self-consistent Density Functional Theory (DFT) methods were performed on models of defected Fe surfaces, most significantly the stepped Fe(211) surface. Binding Energies (BE's), preferred adsorption sites and geometries of all the FTS relevant stable species and intermediates were evaluated. Each elementary step of our reaction model was fully characterized with respect to its thermochemistry and comparisons between the stepped Fe(211) facet and the most-stable Fe(110) facet were established. In most cases the BE's on Fe(211) reflected the trends observed earlier on Fe(110), yet there were significant variations imposed on the underlying trends. Vibrational frequencies were evaluated for the preferred adsorption configurations of each species with the aim of evaluating the entropy-changes and preexponential factors for each elementary step. Kinetic studies were performed for the early steps of FTS (up to CH{sub 4} formation) and CO dissociation. This involved evaluation of the Minimum Energy Pathway (MEP) and activation energy barrier for the steps involved. We concluded that Fe(211) would allow for far more facile CO dissociation in comparison to other Fe catalysts studied so far, but the other FTS steps studied remained mostly unchanged.

Research Organization:
Univ. of Wisconsin, Madison, WI (United States)
Sponsoring Organization:
USDOE
DOE Contract Number:
FC26-03NT41966
OSTI ID:
901151
Country of Publication:
United States
Language:
English