Scouting tests to examine potential corrosion of aluminum alloy 2519 during fabrication
Coupons of 2519 aluminum were exposed for three weeks in a variety of environments representative of those expected during fabrication of the advanced amphibious assault vehicle (AAAV). Specimens exposed to tap water developed very minor pitting and staining, while specimens exposed in high humidity air, water chaser, or machine cutting fluid revealed no detectable changes.
- Research Organization:
- Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
- Sponsoring Organization:
- USDOE Office of Energy Research, Washington, DC (United States)
- DOE Contract Number:
- AC05-96OR22464
- OSTI ID:
- 304018
- Report Number(s):
- ORNL/TM-13676; ON: DE99000337; TRN: AHC29904%%92
- Resource Relation:
- Other Information: PBD: Aug 1998
- Country of Publication:
- United States
- Language:
- English
Similar Records
SRNL SHELF LIFE STUDIES - SCC STUDIES AT ROOM TEMPERTURE [stress corrosion cracking ]
Relative Humidity and the Susceptibility of Austenitic Stainless Steel to Stress Corrosion Cracking in an impure Plutonium Oxide Environment
Creep crack growth behavior of aluminum alloy 2519. Part 2: Numerical analysis
Technical Report
·
Wed Nov 12 00:00:00 EST 2014
·
OSTI ID:304018
Relative Humidity and the Susceptibility of Austenitic Stainless Steel to Stress Corrosion Cracking in an impure Plutonium Oxide Environment
Journal Article
·
Wed May 05 00:00:00 EDT 2010
· Journal of Nuclear Materials Management
·
OSTI ID:304018
+1 more
Creep crack growth behavior of aluminum alloy 2519. Part 2: Numerical analysis
Conference
·
Wed Dec 31 00:00:00 EST 1997
·
OSTI ID:304018
+1 more