Amorphous silicon solar cells have been shown to have efficiencies which degrade as a result of long exposure to light. Annealing such cells in air at a temperature of about 200 C for at least 30 minutes restores their efficiency. 2 figs.
- DOE Contract Number:
- EG-77-C-01-4042
- Assignee:
- RCA Corp., New York, NY (United States)
- Patent Number(s):
- US 4371738; A
- Application Number:
- PPN: US 6-260170
- OSTI ID:
- 7258118
- Resource Relation:
- Patent File Date: 4 May 1981
- Country of Publication:
- United States
- Language:
- English
Similar Records
Method of restoring degraded solar cells
Fabricating amorphous silicon solar cells by varying the temperature _of the substrate during deposition of the amorphous silicon layer
Spray solar cell research: CdS/Cu/sub 2/S cells by ion exchange-CSD. Quarterly report No. 1, October 1-December 31, 1979
Patent
·
Sat Jan 01 00:00:00 EST 1983
·
OSTI ID:7258118
Fabricating amorphous silicon solar cells by varying the temperature _of the substrate during deposition of the amorphous silicon layer
Patent
·
Fri Jan 01 00:00:00 EST 1982
·
OSTI ID:7258118
Spray solar cell research: CdS/Cu/sub 2/S cells by ion exchange-CSD. Quarterly report No. 1, October 1-December 31, 1979
Technical Report
·
Mon Jan 01 00:00:00 EST 1979
·
OSTI ID:7258118
Related Subjects
14 SOLAR ENERGY
SILICON SOLAR CELLS
ANNEALING
ENERGY EFFICIENCY
AGE DEPENDENCE
AMORPHOUS STATE
REPAIR
SILICON
DIRECT ENERGY CONVERTERS
EFFICIENCY
ELEMENTS
EQUIPMENT
HEAT TREATMENTS
PHOTOELECTRIC CELLS
PHOTOVOLTAIC CELLS
SEMIMETALS
SOLAR CELLS
SOLAR EQUIPMENT
140501* - Solar Energy Conversion- Photovoltaic Conversion
SILICON SOLAR CELLS
ANNEALING
ENERGY EFFICIENCY
AGE DEPENDENCE
AMORPHOUS STATE
REPAIR
SILICON
DIRECT ENERGY CONVERTERS
EFFICIENCY
ELEMENTS
EQUIPMENT
HEAT TREATMENTS
PHOTOELECTRIC CELLS
PHOTOVOLTAIC CELLS
SEMIMETALS
SOLAR CELLS
SOLAR EQUIPMENT
140501* - Solar Energy Conversion- Photovoltaic Conversion