Title: Catalytic hydrotreating of solvent refined coal (SRC-II): the effect of metal combinations, impregnation technique and water addition on catalyst activity

Thesis/Dissertation ·
OSTI ID:6491922

Solvent refined coal (SRC-II) must be catalytically hydrotreated at elevated temperatures and pressures to improve its stability and meet the feedstock requirements of conventional petroleum refineries and boilers. Once the operating conditions are set, the development of catalysts is the primary problem. Four transition metals, cobalt (Co), nickel (Ni), molybdenum (Mo) and tungsten (W), were selected as the catalytic magnets and impregnated on a 8-alumina support having large surface area and pore size. In the first stage, seven different combinations of the metals were impregnated by stepwise impregnation technique to test their hydrotreating activity. In the second stage, the most active metal combinations, Ni-Mo and Co-Mo, were subjected to three different impregnation techniques to test the effect of impregnation method on catalytic activity. The effect of the presence of 2% water in the feed on the catalytic activity was tested for every catalyst. The most active metal combinations among the seven were Ni-Mo for hydrodenitrogenation (HDN) and hydrogenation (HYD), and Co-Mo for hydrocracking (HYC). Water enhanced the activity of the catalysts containing Ni-Mo and Co-Mo combinations, but inhibited activity of the catalysts containing Ni-Mo and Ni-W combinations. In general, HYC activities of the catalysts prepared by stepwise impregnation were improved by water addition.

OSTI ID:
6491922
Resource Relation:
Other Information: Thesis (Ph. D.)
Country of Publication:
United States
Language:
English