The effect of transformation temperature and prior austenite grain size on the pearlite colony size in vanadium treated pearlitic steels
Abstract
The lower the transformation temperature, the smaller the colony size. Over the range of transformation temperatures 660-580/sup 0/C, the ratio of the colony size to the mean true interlamellar spacing was in the range 29 to 35. The prior austenite grain size affected neither the pearlite colony size nor the structure of a colony but influenced the morphology of pearlite.
- Authors:
- Publication Date:
- Research Org.:
- Dept. of Metals and Materials Engineering, Sheffield City Polytechnic, Sheffield S1 1WB
- OSTI Identifier:
- 6481499
- Resource Type:
- Journal Article
- Journal Name:
- Scr. Metall.; (United States)
- Additional Journal Information:
- Journal Volume: 21:3
- Country of Publication:
- United States
- Language:
- English
- Subject:
- 36 MATERIALS SCIENCE; AUSTENITE; GRAIN SIZE; PEARLITE; MORPHOLOGY; TEMPERATURE EFFECTS; HIGH TEMPERATURE; SPACE DEPENDENCE; TRANSITION TEMPERATURE; VANADIUM; ALLOYS; CARBON ADDITIONS; CRYSTAL STRUCTURE; ELEMENTS; IRON ALLOYS; METALS; MICROSTRUCTURE; PHYSICAL PROPERTIES; SIZE; THERMODYNAMIC PROPERTIES; TRANSITION ELEMENTS; 360104* - Metals & Alloys- Physical Properties; 360102 - Metals & Alloys- Structure & Phase Studies
Citation Formats
Pickering, F B, and Garbarz, B. The effect of transformation temperature and prior austenite grain size on the pearlite colony size in vanadium treated pearlitic steels. United States: N. p., 1987.
Web. doi:10.1016/0036-9748(87)90207-9.
Pickering, F B, & Garbarz, B. The effect of transformation temperature and prior austenite grain size on the pearlite colony size in vanadium treated pearlitic steels. United States. https://doi.org/10.1016/0036-9748(87)90207-9
Pickering, F B, and Garbarz, B. 1987.
"The effect of transformation temperature and prior austenite grain size on the pearlite colony size in vanadium treated pearlitic steels". United States. https://doi.org/10.1016/0036-9748(87)90207-9.
@article{osti_6481499,
title = {The effect of transformation temperature and prior austenite grain size on the pearlite colony size in vanadium treated pearlitic steels},
author = {Pickering, F B and Garbarz, B},
abstractNote = {The lower the transformation temperature, the smaller the colony size. Over the range of transformation temperatures 660-580/sup 0/C, the ratio of the colony size to the mean true interlamellar spacing was in the range 29 to 35. The prior austenite grain size affected neither the pearlite colony size nor the structure of a colony but influenced the morphology of pearlite.},
doi = {10.1016/0036-9748(87)90207-9},
url = {https://www.osti.gov/biblio/6481499},
journal = {Scr. Metall.; (United States)},
number = ,
volume = 21:3,
place = {United States},
year = {Sun Mar 01 00:00:00 EST 1987},
month = {Sun Mar 01 00:00:00 EST 1987}
}
Other availability
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.