Low temperature process for obtaining thin glass films
Patent
·
OSTI ID:5447304
A method for coating a substrate with a glass-like film comprises, applying to the substrate an aqueous alcoholic solution containing a polymeric network of partially hydrolyzed metal alkoxide into which network there is incorporated finely powdered glass, whereby there is achieved on the substrate a coherent and adherent initial film; and heating said film to a temperature sufficient to melt said powdered glass component, thereby converting said initial film to a final densified film.
- DOE Contract Number:
- AC04-76DP00789
- Assignee:
- SNL; EDB-84-030206
- Application Number:
- ON: DE84005961
- OSTI ID:
- 5447304
- Country of Publication:
- United States
- Language:
- English
Similar Records
Low temperature process for obtaining thin glass films
Low temperature process for obtaining thin glass films
Inorganic-polymer-derived dielectric films
Patent
·
Sun Jan 01 00:00:00 EST 1984
·
OSTI ID:5447304
Low temperature process for obtaining thin glass films
Patent
·
Tue Oct 09 00:00:00 EDT 1984
·
OSTI ID:5447304
Inorganic-polymer-derived dielectric films
Patent
·
Tue Mar 24 00:00:00 EST 1987
·
OSTI ID:5447304