FINE GRAIN NUCLEAR EMULSION
Patent
·
OSTI ID:4785924
A method of preparing nuclear track emulsions having mean grain sizes less than 0.1 microns is described. The method comprises adding silver nitrate to potassium bromide at a rate at which there is always a constant, critical excess of silver ions. For minimum size grains, the silver ion concentration is maintained at the critical level of about pAg 2.0 to 5.0 during prectpitation, pAg being defined as the negative logarithm of the silver ion concentration. It is preferred to eliminate the excess silver at the conclusion of the precipitation steps. The emulsion is processed by methods in all other respects generally similar to the methods of the prior art. (AEC)
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-16-013838
- Assignee:
- U.S. Atomic Energy Commission
- Patent Number(s):
- US 3031304
- OSTI ID:
- 4785924
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-62
- Country of Publication:
- United States
- Language:
- English
Similar Records
LABORATORY PRODUCTION OF FINE GRAIN NUCLEAR EMULSION
THE EFFECT OF CADMIUM IONS ON THE PROPERTIES OF NUCLEAR EMULSIONS
GRAIN SIZE AND GRAIN DENSITY IN ILFORD K-5 AND L-4 EMULSIONS
Technical Report
·
Thu Jul 10 00:00:00 EDT 1958
·
OSTI ID:4785924
THE EFFECT OF CADMIUM IONS ON THE PROPERTIES OF NUCLEAR EMULSIONS
Journal Article
·
Wed Jan 01 00:00:00 EST 1958
· Czechoslov. J. Phys.
·
OSTI ID:4785924
GRAIN SIZE AND GRAIN DENSITY IN ILFORD K-5 AND L-4 EMULSIONS
Journal Article
·
Thu Jan 01 00:00:00 EST 1959
· Nuovo Cimento (Italy) Divided into Nuovo Cimento A and Nuovo Cimento B
·
OSTI ID:4785924