PREPARATION OF SPHERICAL URANIUM DIOXIDE PARTICLES
Patent
·
OSTI ID:4710374
This patent relates to the preparation of high-density, spherical UO/sub 2/ particles 80 to 150 microns in diameter. Sinterable UO/sub 2/ powder is wetted with 3 to 5 weight per cent water and tumbled for at least 48 hours. The resulting spherical particles are then sintered. The sintered particles are useful in dispersion-type fuel elements for nuclear reactors. (AEC)
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-17-018694
- Assignee:
- U.S. Atomic Energy Commission
- Patent Number(s):
- US 3087781
- OSTI ID:
- 4710374
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-63
- Country of Publication:
- United States
- Language:
- English
Similar Records
METHOD FOR PREPARATION OF SPHERICAL UO$sub 4$
METHOD FOR THE DIRECT PREPARATION OF GRANULAR MATERIAL CONTAINING URANIUM WITH A DETERMINATE PARTICLE SIZE AND A CLEARLY SPHERICAL SHAPE
METHOD FOR THE DIRECT PREPARATION OF GRANULAR MATERIAL CONTAINING URANIUM WITH A DETERMINATE PARTICLE SIZE AND A CLEARLY SPHERICAL SHAPE
Patent
·
Fri Jun 01 00:00:00 EDT 1962
·
OSTI ID:4710374
METHOD FOR THE DIRECT PREPARATION OF GRANULAR MATERIAL CONTAINING URANIUM WITH A DETERMINATE PARTICLE SIZE AND A CLEARLY SPHERICAL SHAPE
Patent
·
Tue Aug 01 00:00:00 EDT 1961
·
OSTI ID:4710374
METHOD FOR THE DIRECT PREPARATION OF GRANULAR MATERIAL CONTAINING URANIUM WITH A DETERMINATE PARTICLE SIZE AND A CLEARLY SPHERICAL SHAPE
Patent
·
Tue Aug 01 00:00:00 EDT 1961
·
OSTI ID:4710374