Title: Next-Generation Lithium Metal Anode Engineering via Atomic Layer Deposition

Journal Article · · ACS Nano

Research Organization:
Energy Frontier Research Centers (EFRC) (United States). Nanostructures for Electrical Energy Storage (NEES)
Sponsoring Organization:
USDOE Office of Science (SC), Basic Energy Sciences (BES)
DOE Contract Number:
SC0001160
OSTI ID:
1210782
Journal Information:
ACS Nano, Vol. In Press; Related Information: NEES partners with University of Maryland (lead); University of California, Irvine; University of Florida; Los Alamos National Laboratory; Sandia National Laboratories; Yale University
Country of Publication:
United States
Language:
English

References (37)

Quantifying the promise of lithium–air batteries for electric vehicles journal January 2014
Performances and safety behaviour of rechargeable AA-size Li/LixMnO2 cell journal March 1995
Fluorinated Carbonyl and Olefinic Compounds:  Basic Character and Asymmetric Catalytic Reactions journal January 2004
Capacity Fade Mechanisms and Side Reactions in Lithium-Ion Batteries journal January 1998
Fingerprinting Lithium-Sulfur Battery Reaction Products by X-ray Absorption Spectroscopy journal January 2014
Protection of Lithium Metal Surfaces Using Chlorosilanes journal November 2007
Cycling characteristics of lithium metal batteries assembled with a surface modified lithium electrode journal December 2013
An Effective Approach To Protect Lithium Anode and Improve Cycle Performance for Li–S Batteries journal August 2014
Lithium phosphorous oxynitride as a passive layer for anodes in lithium secondary batteries journal May 2004
Addition of a thin-film inorganic solid electrolyte (Lipon) as a protective film in lithium batteries with a liquid electrolyte journal August 2000
Interconnected hollow carbon nanospheres for stable lithium metal anodes journal July 2014
Effective enhancement of lithium-ion battery performance using SLMP journal July 2011
Examining the role of hydrogen in the electrical performance of in situ fabricated metal-insulator-metal trilayers using an atomic layer deposited Al 2 O 3 dielectric journal April 2013
Lithium Sulfur Battery: Oxidation/Reduction Mechanisms of Polysulfides in THF Solutions journal January 1988
Atomic Layer Deposition: An Overview journal January 2010
Al 2 O 3 and TiO 2 Atomic Layer Deposition on Copper for Water Corrosion Resistance journal November 2011
A study of atomic layer deposited LiAlxOy films on Mg–Li alloys journal October 2010
Multilayer Al2O3/TiO2 Atomic Layer Deposition coatings for the corrosion protection of stainless steel journal November 2012
Gas diffusion barrier characteristics of Al2O3/alucone films formed using trimethylaluminum, water and ethylene glycol for organic light emitting diode encapsulation journal November 2013
Evaluating Al 2 O 3 gas diffusion barriers grown directly on Ca films using atomic layer deposition techniques journal January 2013
Surface-modified silicon nanowire anodes for lithium-ion batteries journal October 2011
ALD TiO2 coated silicon nanowires for lithium ion battery anodes with enhanced cycling stability and coulombic efficiency journal January 2013
Improved Mechanical Integrity of ALD-Coated Composite Electrodes for Li-Ion Batteries journal January 2011
Conformal Surface Coatings to Enable High Volume Expansion Li-Ion Anode Materials journal May 2010
Low-temperature atomic layer deposited Al2O3 thin film on layer structure cathode for enhanced cycleability in lithium-ion batteries journal April 2010
Electrochemical effects of ALD surface modification on combustion synthesized LiNi1/3Mn1/3Co1/3O2 as a layered-cathode material journal March 2011
Plasma-Enhanced Atomic Layer Deposition of Ultrathin Oxide Coatings for Stabilized Lithium-Sulfur Batteries journal June 2013
How Do Li Atoms Pass through the Al 2 O 3 Coating Layer during Lithiation in Li-ion Batteries? journal July 2013
Design of electrolyte solutions for Li and Li-ion batteries: a review journal November 2004
A Reversible and Higher-Rate Li-O2 Battery journal July 2012
Oxygen, hydrogen, ethylene and CO2 development in lithium-ion batteries journal December 2007
Dual-Confined Flexible Sulfur Cathodes Encapsulated in Nitrogen-Doped Double-Shelled Hollow Carbon Spheres and Wrapped with Graphene for Li-S Batteries journal February 2015
Sulfur-Impregnated Activated Carbon Fiber Cloth as a Binder-Free Cathode for Rechargeable Li-S Batteries journal November 2011
Self-discharge of lithium–sulfur cells using stainless-steel current-collectors journal February 2005
Electronic Structure Modeling of Electrochemical Reactions at Electrode/Electrolyte Interfaces in Lithium Ion Batteries journal December 2012
Using Atomic Layer Deposition to Hinder Solvent Decomposition in Lithium Ion Batteries: First-Principles Modeling and Experimental Studies journal September 2011
Advanced process technologies: Plasma, direct-write, atmospheric pressure, and roll-to-roll ALD journal November 2011

Cited By (157)

Pseudocapacitance Induced Uniform Plating/Stripping of Li Metal Anode in Vertical Graphene Nanowalls journal October 2018
Anode Improvement in Rechargeable Lithium-Sulfur Batteries journal June 2017
Anode Interface Engineering and Architecture Design for High‐Performance Lithium–Sulfur Batteries journal January 2019
ALD Protection of Li-Metal Anode Surfaces - Quantifying and Preventing Chemical and Electrochemical Corrosion in Organic Solvent journal August 2016
Dendrite‐Free Lithium Plating Induced by In Situ Transferring Protection Layer from Separator journal November 2019
Soft, Highly Elastic, and Discharge-Current-Controllable Eutectic Gallium-Indium Liquid Metal-Air Battery Operated at Room Temperature journal March 2018
Review on High-Loading and High-Energy Lithium-Sulfur Batteries journal May 2017
Rational design of spontaneous reactions for protecting porous lithium electrodes in lithium–sulfur batteries journal July 2019
Recent Progress in Metal-Organic Frameworks and Their Derived Nanostructures for Energy and Environmental Applications journal March 2017
Solid-state polymer electrolytes for high-performance lithium metal batteries journal September 2019
Electrolytes for electrochemical energy storage journal January 2017
A 3D Cu current collector with a biporous structure derived by a phase inversion tape casting method for stable Li metal anodes journal January 2019
Lithium–Magnesium Alloy as a Stable Anode for Lithium–Sulfur Battery journal February 2019
Building Organic/Inorganic Hybrid Interphases for Fast Interfacial Transport in Rechargeable Metal Batteries journal December 2017
A hybrid electrolyte for long-life semi-solid-state lithium sulfur batteries journal January 2017
Bisalt ether electrolytes: a pathway towards lithium metal batteries with Ni-rich cathodes journal January 2019
Current Status and Future Prospects of Metal–Sulfur Batteries journal May 2019
Environmental Screening of Electrode Materials for a Rechargeable Aluminum Battery with an AlCl3/EMIMCl Electrolyte journal June 2018
Facile Generation of Polymer–Alloy Hybrid Layers for Dendrite‐Free Lithium‐Metal Anodes with Improved Moisture Stability journal July 2019
High Dielectric, Robust Composite Protective Layer for Dendrite‐Free and LiPF 6 Degradation‐Free Lithium Metal Anode journal September 2019
An Armored Mixed Conductor Interphase on a Dendrite-Free Lithium-Metal Anode journal September 2018
Three‐Dimensional Graphene/Ag Aerogel for Durable and Stable Li Metal Anodes in Carbonate‐Based Electrolytes journal March 2019
A Li 2 S-Based Sacrificial Layer for Stable Operation of Lithium-Sulfur Batteries journal October 2018
An Artificial Solid Electrolyte Interphase with High Li-Ion Conductivity, Mechanical Strength, and Flexibility for Stable Lithium Metal Anodes journal December 2016
Self-supported TiN nanorod array/carbon textile as a lithium host that induces dendrite-free lithium plating with high rates and long cycle life journal January 2020
Advances in Interfaces between Li Metal Anode and Electrolyte journal December 2017
Ultrafine Silver Nanoparticles for Seeded Lithium Deposition toward Stable Lithium Metal Anode journal August 2017
Two-dimensional molecular brush-functionalized porous bilayer composite separators toward ultrastable high-current density lithium metal anodes journal March 2019
SiO 2 Hollow Nanosphere-Based Composite Solid Electrolyte for Lithium Metal Batteries to Suppress Lithium Dendrite Growth and Enhance Cycle Life journal January 2016
Lithium Silicide Surface Enrichment: A Solution to Lithium Metal Battery journal July 2018
Air‐Stable and Dendrite‐Free Lithium Metal Anodes Enabled by a Hybrid Interphase of C 60 and Mg journal December 2019
Advances in Artificial Layers for Stable Lithium Metal Anodes journal April 2020
Sulfide Solid Electrolytes for Lithium Battery Applications journal August 2018
Review—Solid Electrolytes for Safe and High Energy Density Lithium-Sulfur Batteries: Promises and Challenges journal June 2017
Self‐Stabilized and Strongly Adhesive Supramolecular Polymer Protective Layer Enables Ultrahigh‐Rate and Large‐Capacity Lithium‐Metal Anode journal December 2019
Fast galvanic lithium corrosion involving a Kirkendall-type mechanism journal January 2019
2D MoS2 as an efficient protective layer for lithium metal anodes in high-performance Li–S batteries journal February 2018
High-Energy-Density Metal-Oxygen Batteries: Lithium-Oxygen Batteries vs Sodium-Oxygen Batteries journal September 2017
Synthesis and characterization of a hierarchically structured three-dimensional conducting scaffold for highly stable Li metal anodes journal January 2019
In Situ Li 3 PS 4 Solid-State Electrolyte Protection Layers for Superior Long-Life and High-Rate Lithium-Metal Anodes journal October 2018
Catalysts in metal–air batteries journal April 2018
Tin Intercalated Ultrathin MoO 3 Nanoribbons for Advanced Lithium-Sulfur Batteries journal December 2018
Bending impact on the performance of a flexible Li 4 Ti 5 O 12 -based all-solid-state thin-film battery journal May 2018
An Interconnected Channel-Like Framework as Host for Lithium Metal Composite Anodes journal January 2019
Soybean-derived hierarchical porous carbon with large sulfur loading and sulfur content for high-performance lithium–sulfur batteries journal January 2016
A Rechargeable Al/S Battery with an Ionic-Liquid Electrolyte journal July 2016
Facile Generation of Polymer-Alloy Hybrid Layers for Dendrite-Free Lithium-Metal Anodes with Improved Moisture Stability journal July 2019
Dendrite-Free Lithium Anode via a Homogenous Li-Ion Distribution Enabled by a Kimwipe Paper journal January 2017
Compact 3D Copper with Uniform Porous Structure Derived by Electrochemical Dealloying as Dendrite-Free Lithium Metal Anode Current Collector journal March 2018
Recent developments and insights into the understanding of Na metal anodes for Na-metal batteries journal January 2018
Stable cycling of Li–S batteries by simultaneously suppressing Li-dendrite growth and polysulfide shuttling enabled by a bioinspired separator journal January 2020
Understanding undesirable anode lithium plating issues in lithium-ion batteries journal January 2016
Promise and reality of post-lithium-ion batteries with high energy densities journal March 2016
Facile and scalable engineering of a heterogeneous microstructure for uniform, stable and fast lithium plating/stripping journal January 2019
Revisiting the Role of Polysulfides in Lithium-Sulfur Batteries journal March 2018
Turning bulk materials into 0D, 1D and 2D metallic nanomaterials by selective aqueous corrosion journal January 2019
Suppressing Li Metal Dendrites Through a Solid Li‐Ion Backup Layer journal August 2018
Blocking Polysulfides in Graphene–Sulfur Cathodes of Lithium–Sulfur Batteries through Atomic Layer Deposition of Alumina journal May 2019
Conversion cathodes for rechargeable lithium and lithium-ion batteries journal January 2017
Solid/Solid Interfacial Architecturing of Solid Polymer Electrolyte–Based All‐Solid‐State Lithium–Sulfur Batteries by Atomic Layer Deposition journal September 2019
Self‐Stabilized and Strongly Adhesive Supramolecular Polymer Protective Layer Enables Ultrahigh‐Rate and Large‐Capacity Lithium‐Metal Anode journal January 2020
Lithium Metal Anode Materials Design: Interphase and Host journal October 2019
Recent research trends in Li–S batteries journal January 2018
A Li–Al–O Solid‐State Electrolyte with High Ionic Conductivity and Good Capability to Protect Li Anode journal December 2019
Conformality in atomic layer deposition: Current status overview of analysis and modelling journal June 2019
Pre-treatments of Lithium Foil Surface for Improving the Cycling Life of Li Metal Batteries journal November 2019
Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries journal March 2018
A high-performance lithium anode based on N-doped composite graphene journal April 2019
Anode interfacial layer formation via reductive ethyl detaching of organic iodide in lithium–oxygen batteries journal August 2019
Lithium-coated polymeric matrix as a minimum volume-change and dendrite-free lithium metal anode journal March 2016
Suppression of dendritic lithium growth in lithium metal-based batteries journal January 2018
Structural Design of Lithium–Sulfur Batteries: From Fundamental Research to Practical Application journal June 2018
Designable ultra-smooth ultra-thin solid-electrolyte interphases of three alkali metal anodes journal April 2018
A facile surface chemistry route to a stabilized lithium metal anode journal July 2017
Tailoring Lithium Deposition via an SEI‐Functionalized Membrane Derived from LiF Decorated Layered Carbon Structure journal January 2019
Effective Stabilization of a High-Loading Sulfur Cathode and a Lithium-Metal Anode in Li-S Batteries Utilizing SWCNT-Modulated Separators journal November 2015
Lithium metal protected by atomic layer deposition metal oxide for high performance anodes journal January 2017
Recent advances in understanding Li–CO 2 electrochemistry journal January 2019
ZnO nanoconfined 3D porous carbon composite microspheres to stabilize lithium nucleation/growth for high-performance lithium metal anodes journal January 2019
Antimony‐Doped Lithium Phosphate Artificial Solid Electrolyte Interphase for Dendrite‐Free Lithium‐Metal Batteries journal January 2019
Lithium anode stable in air for low-cost fabrication of a dendrite-free lithium battery journal February 2019
Continuous plating/stripping behavior of solid-state lithium metal anode in a 3D ion-conductive framework journal March 2018
Reviving Lithium-Metal Anodes for Next-Generation High-Energy Batteries journal June 2017
Guiding Uniform Li Plating/Stripping through Lithium–Aluminum Alloying Medium for Long‐Life Li Metal Batteries journal December 2018
Air-stable and freestanding lithium alloy/graphene foil as an alternative to lithium metal anodes journal July 2017
Atomic and Molecular Layer Deposition for Superior Lithium-Sulfur Batteries: Strategies, Performance, and Mechanisms journal May 2018
Electroless Formation of Hybrid Lithium Anodes for Fast Interfacial Ion Transport journal September 2017
Protected Lithium-Metal Anodes in Batteries: From Liquid to Solid journal July 2017
Straw-Brick-Like Carbon Fiber Cloth/Lithium Composite Electrode as an Advanced Lithium Metal Anode journal April 2018
Toward High Performance Lithium-Sulfur Batteries Based on Li 2 S Cathodes and Beyond: Status, Challenges, and Perspectives journal March 2018
Bottom-top channeling Li nucleation and growth by a gradient lithiophilic 3D conductive host for highly stable Li-metal anodes journal January 2020
Nanostructured Silicon Anodes for High-Performance Lithium-Ion Batteries journal December 2015
Oxygenated Nitrogen‐Doped Microporous Nanocarbon as a Permselective Interlayer for Ultrastable Lithium‐Sulfur Batteries journal January 2019
An Artificial Lithium Protective Layer that Enables the Use of Acetonitrile-Based Electrolytes in Lithium Metal Batteries journal March 2018
Ultrathin Al2O3-coated reduced graphene oxide membrane for stable lithium metal anode journal May 2018
Promises and challenges of nanomaterials for lithium-based rechargeable batteries journal June 2016
Implanting CNT Forest onto Carbon Nanosheets as Multifunctional Hosts for High-Performance Lithium Metal Batteries journal February 2019
Improving Lithium‐Metal Battery Performance under the Conditions of Lean Electrolyte through MoS 2 Coating journal January 2020
Directing lateral growth of lithium dendrites in micro-compartmented anode arrays for safe lithium metal batteries journal January 2018
Ferromagnetic Nanoparticle-Assisted Polysulfide Trapping for Enhanced Lithium-Sulfur Batteries journal April 2018
Intercalated Electrolyte with High Transference Number for Dendrite‐Free Solid‐State Lithium Batteries journal April 2019
Chemical Dealloying Derived 3D Porous Current Collector for Li Metal Anodes journal May 2016
Nanostructured Metal Oxides and Sulfides for Lithium-Sulfur Batteries journal February 2017
Superior Stable and Long Life Sodium Metal Anodes Achieved by Atomic Layer Deposition journal March 2017
Recent Developments of the Lithium Metal Anode for Rechargeable Non-Aqueous Batteries journal July 2016
Theoretical Investigation of 2D Layered Materials as Protective Films for Lithium and Sodium Metal Anodes journal February 2017
High Performance Lithium Metal Batteries Enabled by Surface Tailoring of Polypropylene Separator with a Polydopamine/Graphene Layer journal November 2018
Efficient Li‐Ion‐Conductive Layer for the Realization of Highly Stable High‐Voltage and High‐Capacity Lithium Metal Batteries journal February 2019
An Air‐Stable and Dendrite‐Free Li Anode for Highly Stable All‐Solid‐State Sulfide‐Based Li Batteries journal August 2019
The Failure of Solid Electrolyte Interphase on Li Metal Anode: Structural Uniformity or Mechanical Strength? journal March 2020
Guiding Uniform Li Plating/Stripping through Lithium-Aluminum Alloying Medium for Long-Life Li Metal Batteries journal December 2018
Atomic Layer Deposition of Li x Al y S Solid-State Electrolytes for Stabilizing Lithium-Metal Anodes journal April 2016
Reduced Shuttle Effect of Lithium−sulfur Batteries by using a Simple Graphite-Modified Separator with a Preformed SEI Film journal November 2017
Low-Weight 3D Al 2 O 3 Network as an Artificial Layer to Stabilize Lithium Deposition journal August 2018
Design Principles of Functional Polymer Separators for High-Energy, Metal-Based Batteries journal December 2017
Key Aspects of Lithium Metal Anodes for Lithium Metal Batteries journal March 2019
Anode‐Free Sodium Metal Batteries Based on Nanohybrid Core–Shell Templates journal June 2019
The Challenge of Lithium Metal Anodes for Practical Applications journal April 2019
Dendrite-free all-solid-state lithium batteries with lithium phosphorous oxynitride-modified lithium metal anode and composite solid electrolytes journal September 2018
High-Performance Anode Materials for Rechargeable Lithium-Ion Batteries journal March 2018
Recent Progress in Liquid Electrolyte-Based Li–S Batteries: Shuttle Problem and Solutions journal November 2018
Design principles for electrolytes and interfaces for stable lithium-metal batteries journal September 2016
Reviving the lithium metal anode for high-energy batteries journal March 2017
Organosulfide-plasticized solid-electrolyte interphase layer enables stable lithium metal anodes for long-cycle lithium-sulfur batteries journal October 2017
An artificial TiO 2 /lithium n -butoxide hybrid SEI layer with facilitated lithium-ion transportation ability for stable lithium anodes journal January 2019
Inhibiting the growth of lithium dendrites at high current densities with oriented graphene foam journal January 2018
Lithium phosphide/lithium chloride coating on lithium for advanced lithium metal anode journal January 2018
Multi-functional nanowall arrays with unrestricted Li + transport channels and an integrated conductive network for high-areal-capacity Li–S batteries journal January 2018
A fast and stable Li metal anode incorporating an Mo 6 S 8 artificial interphase with super Li-ion conductivity journal January 2019
Probing the dynamic evolution of lithium dendrites: a review of in situ / operando characterization for lithium metallic batteries journal January 2019
Protection of lithium anodes by fibrous silica nanospheres journal January 2020
Engineering stable interfaces for three-dimensional lithium metal anodes journal July 2018
Electrochemically Stable Coating Materials for Li, Na, and Mg Metal Anodes in Durable High Energy Batteries journal January 2017
Self-Supporting Dendritic Copper Porous Film Inducing the Lateral Growth of Metallic Lithium for Highly Stable Li Metal Battery journal January 2019
Rechargeable Magnesium–Sulfur Battery Technology: State of the Art and Key Challenges journal September 2019
Dendrite-Suppressed Lithium Plating from a Liquid Electrolyte via Wetting of Li 3 N journal July 2017
Synergistic Effect of 3D Current Collectors and ALD Surface Modification for High Coulombic Efficiency Lithium Metal Anodes journal December 2018
A Rechargeable Al/S Battery with an Ionic-Liquid Electrolyte journal July 2016
Electroless Formation of Hybrid Lithium Anodes for Fast Interfacial Ion Transport journal September 2017
Ultrahigh-Capacity and Long-Life Lithium-Metal Batteries Enabled by Engineering Carbon Nanofiber-Stabilized Graphene Aerogel Film Host journal September 2018
Understanding the molecular mechanism of pulse current charging for stable lithium-metal batteries journal July 2017
Ultrahigh–current density anodes with interconnected Li metal reservoir through overlithiation of mesoporous AlF 3 framework journal September 2017
Transforming from planar to three-dimensional lithium with flowable interphase for solid lithium metal batteries journal October 2017
Advanced Porous Carbon Materials for High-Efficient Lithium Metal Anodes journal July 2017
A Material Perspective of Rechargeable Metallic Lithium Anodes journal February 2018
Why Do Lithium-Oxygen Batteries Fail: Parasitic Chemical Reactions and Their Synergistic Effect journal July 2016
Atomic and Molecular Layer Deposition for Superior Lithium-Sulfur Batteries: Strategies, Performance, and Mechanisms journal June 2018
Cover Feature: Improving Lithium‐Metal Battery Performance under the Conditions of Lean Electrolyte through MoS 2 Coating (ChemElectroChem 4/2020) journal January 2020
Synergetic effect on catalytic activity and charge transfer in Pt-Pd bimetallic model catalysts prepared by atomic layer deposition journal January 2020
Cycle stability of lithium/garnet/lithium cells with different intermediate layers journal May 2018
A dual-phase Li–Ca alloy with a patternable and lithiophilic 3D framework for improving lithium anode performance journal January 2019
An Artificial Lithium Protective Layer that Enables the Use of Acetonitrile-Based Electrolytes in Lithium Metal Batteries journal March 2018
Review : Solid Electrolytes for Safe and High Energy Density Lithium-Sulfur Batteries : Promises and Challenges text January 2018
Robust Pinhole-free Li 3 N Solid Electrolyte Grown from Molten Lithium journal December 2017
Toward High-Performance Li Metal Anode via Difunctional Protecting Layer journal August 2019
Graphene-Modified 3D Copper Foam Current Collector for Dendrite-Free Lithium Deposition journal November 2019
Recent Progresses and Development of Advanced Atomic Layer Deposition towards High-Performance Li-Ion Batteries journal October 2017