Amorphous Metal Fluoride Passivation Coatings Prepared by Atomic Layer Deposition on LiCoO2 for Li-Ion Batteries
- Research Organization:
- Energy Frontier Research Centers (EFRC) (United States). Center for Electrical Energy Storage (CEES)
- Sponsoring Organization:
- USDOE Office of Science (SC), Basic Energy Sciences (BES)
- DOE Contract Number:
- AC02-06CH11357
- OSTI ID:
- 1210439
- Journal Information:
- Chem. Mater., Related Information: CEES partners with Argonne National Laboratory (lead); University of Illinois, Urbana-Champaign; Northwest University
- Country of Publication:
- United States
- Language:
- English
Similar Records
Amorphous Metal Fluoride Passivation Coatings Prepared by Atomic Layer Deposition on LiCoO 2 for Li-Ion Batteries
Metal fluoride passivation coatings prepared by atomic layer deposition for Li-ion batteries
Metal fluoride passivation coatings prepared by atomic layer deposition for Li-ion batteries
Journal Article
·
Tue Mar 24 00:00:00 EDT 2015
· Chemistry of Materials
·
OSTI ID:1210439
+1 more
Metal fluoride passivation coatings prepared by atomic layer deposition for Li-ion batteries
Patent
·
Tue Jan 08 00:00:00 EST 2019
·
OSTI ID:1210439
+1 more
Metal fluoride passivation coatings prepared by atomic layer deposition for Li-ion batteries
Patent
·
Tue Sep 14 00:00:00 EDT 2021
·
OSTI ID:1210439
+1 more