Title: Reduced defect density at the CZTSSe/CdS interface by atomic layer deposition of Al2O3

Authors:
 [1] ;  [2] ;  [3]
  1. Department of Electrical and Computer Engineering, University of Utah, Salt Lake City, Utah 84112, USA
  2. AQT Solar, Inc., Sunnyvale, California 94086, USA
  3. Department of Electrical and Computer Engineering, University of Utah, Salt Lake City, Utah 84112, USA, Department of Materials Science and Engineering, University of Utah, Salt Lake City, Utah 84112, USA
Publication Date:
OSTI Identifier:
1253658
Grant/Contract Number:
SC0001630
Type:
Publisher's Accepted Manuscript
Journal Name:
Journal of Applied Physics
Additional Journal Information:
Journal Volume: 119; Journal Issue: 19; Related Information: CHORUS Timestamp: 2016-05-18 13:11:42; Journal ID: ISSN 0021-8979
Publisher:
American Institute of Physics
Sponsoring Org:
USDOE
Country of Publication:
United States
Language:
English