A method of improving electrical contact to a thin film of a p-type tellurium-containing II-VI semiconductor comprising: depositing a first undoped layer of ZnTe on a thin film of p-type tellurium containing II-VI semiconductor with material properties selected to limit the formation of potential barriers at the interface between the p-CdTe and the undoped layer, to a thickness sufficient to control diffusion of the metallic-doped ZnTe into the p-type tellurim-containing II-VI semiconductor, but thin enough to minimize affects of series resistance; depositing a second heavy doped p-type ZnTe layer to the first layer using an appropriate dopant; and depositing an appropriate metal onto the outer-most surface of the doped ZnTe layer for connecting an external electrical conductor to an ohmic contact.
Use of separate ZnTe interface layers to form OHMIC contacts to p-CdTe films
Gessert, Timothy A. 01/01/1999 US 5909632
View USPTO link (Link will open in a new window)
A method of making a low-resistance electrical contact between a p-CdTe layer and outer contact layers by ion beam processing comprising: a) placing a CdS/CdTe device into a chamber and evacuating the chamber; b) orienting the p-CdTe side of the CdS/CdTe layer so that it faces apparatus capable of generating Ar atoms and ions of preferred energy and directionality; c) introducing Ar and igniting the area of apparatus capable of generating Ar atoms and ions of preferred energy and directionality in a manner so that during ion exposure, the source-to-substrate distance is maintained such that it is less than the mean-free path or diffusion length of the Ar atoms and ions at the vacuum pressure; d) allowing exposure of the p-CdTe side of the device to said ion beam for a period less than about 5 minutes; and e) imparting movement to the substrate to control the real uniformity of the ion-beam exposure on the p-CdTe side of the device.
Ion-beam treatment to prepare surfaces of p-CdTe films
Gessert, Timothy A. 01/01/2001 US 6281035
View USPTO link (Link will open in a new window)
A method of making a low-resistance electrical contact between a metal and a layer of p-type CdTe surface by plasma etching and reactive ion etching comprising: a) placing a CdS/CdTe layer into a chamber and evacuating said chamber; b) backfilling the chamber with Argon or a reactive gas to a pressure sufficient for plasma ignition; and c) generating plasma ignition by energizing a cathode which is connected to a power supply to enable the plasma to interact argon ions alone or in the presence of a radio-frequency DC self-bias voltage with the p-CdTe surface.
Plasma & reactive ion etching to prepare ohmic contacts
Gessert, Timothy A. 01/01/2002 US 6458254
View USPTO link (Link will open in a new window)
A transparent conducting oxide (TCO) film comprising: a TCO layer, and dopants selected from the elements consisting of Vanadium, Molybdenum, Tantalum, Niobium, Antimony, Titanium, Zirconium, and Hafnium, wherein the elements are n-type dopants; and wherein the transparent conducting oxide is characterized by an improved electron mobility of about 42 cm.sup.2/V-sec while simultaneously maintaining a high carrier density of .about.4.4e.times.10.sup.20 cm.sup.-3.
High quality transparent conducting oxide thin films
Gessert, Timothy A. , Duenow, Joel N. , Barnes, Teresa , Coutts, Timothy J. 08/28/2012 8,253,012
View USPTO link (Link will open in a new window)
A method for producing transparent p-type conducting oxide films without co-doping plasma enhancement or high temperature comprising: a) introducing a dialkyl metal at ambient temperature and a saturated pressure in a carrier gas into a low pressure deposition chamber, and b) introducing NO alone or with an oxidizer into the chamber under an environment sufficient to produce a metal-rich condition to enable NO decomposition and atomic nitrogen incorporation into the formed transparent metal conducting oxide.
Method for producing high carrier concentration p-Type transparent conducting oxides
Li, Xiaonan , Yan, Yanfa , Coutts, Timothy J. , Gessert, Timothy A. , Dehart, Clay M. 04/14/2009 7,517,784