Helium Release Behavior of Aged Titanium Tritides
One sample of bulk Ti has been loaded with a 50 per cent / 50 per cent deuterium/tritium mixture and statically aged for 6.5 years. Thermal desorption of the sample shows an initial release of hydrogen isotopes followed by 3He release. Subsequent D2 loading/desorption was used to quantify the trapped tritium heel. The sample shows an excess hydrogen capacity as a second thermal desorption peak that partially disappears and shifts with annealing at 923-973K. The main hydrogen desorption peak also shifts to higher temperature, indicating a partial reversal of the tritium-decay induced damage by annealing.
- Research Organization:
- Savannah River Site (SRS), Aiken, SC (United States)
- Sponsoring Organization:
- US Department of Energy (US)
- DOE Contract Number:
- AC09-96SR18500
- OSTI ID:
- 829869
- Report Number(s):
- WSRC-MS-2003-00129; TRN: US0404794
- Resource Relation:
- Journal Volume: 404-406; Conference: Int'l Symp on Metal-Hydrogen Systems 2004, Cracow (PL), 09/05/2004--09/09/2004; Other Information: PBD: 27 Jul 2004
- Country of Publication:
- United States
- Language:
- English
Similar Records
DEUTERIUM, TRITIUM, AND HELIUM DESORPTION FROM AGED TITANIUM TRITIDES. PART I.
DEUTERIUM, TRITIUM, AND HELIUM DESORPTION FROM AGED TITANIUM TRITIDES. PART II.
DISPLACEMENT AND HELIUM-INDUCED ENHANCEMENT OF HYDROGEN AND DEUTERIUM RETENTION IN ION-IRRADIATED 18Cr10NiTi STAINLESS STEEL
Journal Article
·
Mon Jul 10 00:00:00 EDT 2006
· Journal of Alloys and Compounds
·
OSTI ID:829869
DEUTERIUM, TRITIUM, AND HELIUM DESORPTION FROM AGED TITANIUM TRITIDES. PART II.
Journal Article
·
Thu Aug 17 00:00:00 EDT 2006
·
OSTI ID:829869
DISPLACEMENT AND HELIUM-INDUCED ENHANCEMENT OF HYDROGEN AND DEUTERIUM RETENTION IN ION-IRRADIATED 18Cr10NiTi STAINLESS STEEL
Journal Article
·
Fri Sep 15 00:00:00 EDT 2006
· Journal of Nuclear Materials, 356(1-3):136-147
·
OSTI ID:829869
+4 more